1-20 of 20 Search Results for

UNS C22000

Sort by
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006280
EISBN: 978-1-62708-169-6
... or minimum. Wrought copper-zinc brasses C21000 Gilding, 95% 94.0–96.0 0.03 0.05 bal … C22000 Commercial bronze, 90% 89.0–91.0 0.05 0.05 bal … C22600 Jewelry bronze, 87.5% 86.0–89.0 0.05 0.05 bal … C23000 Red brass, 85% 84.0–86.0 0.05 0.05 bal … C23030 … 83.5...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002454
EISBN: 978-1-62708-194-8
... Properties A 1020 steel (ASTM A 611, grade B) B 304 stainless steel (ASTM A 666, grade D) C 5052-H34 aluminum (ASTM B 209) D C11000-H04 ETP copper (ASTM B 152) E C22000-H01 commercial bronze (ASTM B 36) Thickness ( t ), in. 0.107 0.107 0.407 0.205 0.205 Thermal conductivity, Btu · ft/h · °F...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003132
EISBN: 978-1-62708-199-3
... for various alloys are given in the following table: UNS number Piercing temperature °C °F C11000 815–870 1500–1600 C12200 815–870 1500–1600 C22000 815–870 1500–1600 C23000 815–870 1500–1600 C26000 760–790 1400–1450 C28000 705–760 1300–1400 C46400 730–790 1350...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005143
EISBN: 978-1-62708-186-3
..., 2.35 Fe, 0.125 Zn, 0.05 P C19500 Iron-cobalt-bearing copper 97 (min) Cu, l.5 Fe, 0.18 P, 0.8 Co, 0.6 Sn C19700 … 99 (min) Cu, 0.6 Fe, 0.2 P, 0.05 Mg Wrought brass alloys C21000 Gilding metal, 95% bal Cu, 5 Zn C22000 Commercial bronze, 90% bal Cu, 10 Zn C23000 Red brass, 85...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006543
EISBN: 978-1-62708-183-2
... … 8.94 0.323  1.0% Pb … 8.94 0.323 Wrought alloys Gilding, 95% … 8.86 0.320 Commercial bronze, 90% C22000 8.80 0.318 Jewelry bronze, 87.5% C22600 8.78 0.317 Red brass, 85% C23000 8.75 0.316 Low brass, 80% C24000 8.67 0.313 Cartridge brass, 70% C26000 8.52...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006276
EISBN: 978-1-62708-169-6
... … 375–600 750–1100 C21000 Gilding metal 425–800 800–1450 C22000 Commercial bronze 425–800 800–1450 C22600 Jewelry bronze 425–750 800–1400 C23000 Red brass 425–725 800–1350 C24000 Low brass 425–700 800–1300 C26000 Cartridge brass 425–750 800–1400 C26800, C27000...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003131
EISBN: 978-1-62708-199-3
...) 0.03 0.05 bal … C22000 Commercial bronze, 90% 89.0–91.0 (t) 0.05 0.05 bal … C22600 Jewelry bronze, 87 1 2 % 86.0–89.0 (t) 0.05 0.05 bal … C23000 Red brass, 85% 84.0–86.0 (t) 0.05 0.05 bal … C23030 … 83.5–85.5 (t) 0.05 0.05 bal 0.20–0.40Si C23400...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003137
EISBN: 978-1-62708-199-3
... C22000 205 400 1 Cartridge brass C26000 260 500 1 Muntz metal C28000 190 375 1 2 Admiralty metal C44300, C44400, C44500 300 575 1 Phosphor bronze, 5 or 10% C51000, C52400 190 375 1 Silicon bronze C65500 370 700 1 Aluminum bronze C61300, C61400 400...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003181
EISBN: 978-1-62708-199-3
...% 95 5 … … … 100 E C22000 Commercial bronze, 90% 90 10 … … … 90 E C22600 Jewelry bronze, 87.5% 87.5 12.5 … … … 90 E C23000 Red brass, 85% 85 15 … … … 70 E C24000 Low brass, 80% 80 20 … … … 70 E C26000 Cartridge brass, 70% 70 30 … … … 60 E...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001065
EISBN: 978-1-62708-162-7
... 165–503 24–73 32–2 20 C21000 (gilding, 95%) 95.0 Cu, 5.0 Zn F, W 234–441 34–64 69–400 10–58 45–4 20 C22000 (commercial bronze, 90%) 90.0 Cu, 10.0 Zn F, R, W, T 255–496 37–72 69–427 10–62 50–3 20 C22600 (jewelry bronze, 87.5%) 87.5 Cu, 12.5 Zn F, W 269–669 39–97 76–427...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004004
EISBN: 978-1-62708-185-6
... alloys Table 4 Cold formability of copper and copper alloys Best Good Fair C10200 (OFHC) C15000 C14500 C11000 (ETP) C16200 C14700 C11400 C17200 C28000 (Muntz metal) C12200 C18200 C35000 C22000 C18700 C35300 C23000 (red brass) C27400 (yellow brass) C35600...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.9781627081627
EISBN: 978-1-62708-162-7
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001438
EISBN: 978-1-62708-173-3
... 53–66 (c) F F F Low-zinc brasses C21000 Gilding 95 Cu, 5 Zn 1065 1950 60 G G NR C22000 Commercial bronze 90 Cu, 10 Zn 1043 1910 48 G G NR C23000 Red brass 85 Cu, 15 Zn 1026 1880 41 G G NR C24000 Low brass 80 Cu, 20 Zn 999 1830 36 G G NR High...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003206
EISBN: 978-1-62708-199-3
... electrodes (AWS A5.17-89) Electrode Composition (a) (b) , wt% AWS classification UNS No. C Mn Si S P Cu (c) Ti Low-manganese electrodes EL8 K01008 0.10 0.25–0.60 0.07 0.030 0.030 0.35 … EL8K K01009 0.10 0.25–0.60 0.10–0.25 0.030 0.030 0.35 … EL12 K01012...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003816
EISBN: 978-1-62708-183-2
... Composition Copper alloys are traditionally classified under the groupings listed in Table 1 . The Unified Numbering System (UNS) numbers are administered by the Copper Development Association. Similar compositionally based designation systems are used internationally. Classification of copper alloys...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003204
EISBN: 978-1-62708-199-3
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001066
EISBN: 978-1-62708-162-7
... Copper tube alloys and typical applications UNS number Alloy type ASTM specifications Typical uses C10200 Oxygen-free copper B 68, B 75, B 88, B 111, B 188, B 280, B 359, B 372, B 395, B 447 Bus tube, conductors, wave guides C12200 Phosphorus deoxidized copper B 68, B 75, B 88, B 111...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006579
EISBN: 978-1-62708-290-7
... as an efficient deoxidizer in casting, where 2P + 4Cu + 7O → 2Cu 2 O · P 2 O 5 (UNS grades C12000 to C12510) ( Ref 106 ). In AM, the inadvertent use of phosphorus-deoxidized copper has been reported in a number of papers ( Ref 22 , 23 ). This is problematic for two reasons. First, even small quantities...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001067
EISBN: 978-1-62708-162-7
... capacity increases with increasing cold work; for example, the damping capacity of 70-30 brass has been reported to increase for reductions up to 60%. When subjected to the same conditions, coppers have about three times the damping capacity of C21000 or C22000. A specific damping capacity of 5 × 10 −5...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.9781627081993
EISBN: 978-1-62708-199-3