Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006717
EISBN: 978-1-62708-210-5
... and colored. While alloy 6063 is essentially a ternary Al-Mg-Si alloy, minor elements, such as Fe, Cu, Mn, and Cr can be important at less than 0.10% levels. Equivalent specifications of 6063 are: UNS: A96063 ISO: AlMgSi Austria: Önorm AlMgSi0,5 Canada: CSA GS10 France: NF A-GS...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004139
EISBN: 978-1-62708-184-9
...-saturated, oxygen-depleted wood. A combination of corrosion resistance and mechanical strength is needed that exceeds most mild steel and common brass. Most of the copper alloy seavalves, seacocks, or through-hulls and other underwater fittings are made of cast phosphor bronze (UNS C94300) or a cast...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006543
EISBN: 978-1-62708-183-2
... 5052 A95052 2.68 0.097 5056 A95056 2.64 0.095 5083 A95083 2.66 0.096 5086 A95086 2.65 0.096 5154 A95154 2.66 0.096 5357 A95357 2.70 0.098 5456 A95456 2.66 0.096 6061, 6063 A96061, A96063 2.70 0.098 6070 A96070 2.71 0.098 6101, 6151 A96101, A96151...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001060
EISBN: 978-1-62708-162-7
... aluminum 1050<break />99.5 Al min Specifications ASTM B 491 UNS Number A91050 Foreign Canada: CSA 9950. France: NF A5. United Kingdom: BS 1B. West Germany: DIN A 199.5 Chemical Composition Composition Limits 99.50 Al min, 0.25 Si max, 0.40 Fe max, 0.05 Cu max, 0.05 Mn...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003123
EISBN: 978-1-62708-199-3
..., and designations and composition limits for aluminum alloys in the form of castings and ingot. It provides helpful information on the Unified Numbering System (UNS) numbers and its corresponding AA numbers for aluminum and aluminum alloys, and the international alloy designations cross-referenced to its equivalent...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006251
EISBN: 978-1-62708-169-6
... 0.8–1.2 0.25 0.04–0.35Cr bal 6063 A96063 0.20–0.6 0.35 0.10 0.10 0.45–0.9 0.10 … bal 6066 A96066 0.9–1.8 0.50 0.7–1.2 0.6–1.1 0.8–1.4 0.25 … bal 6070 A96070 1.0–1.7 0.50 0.15–0.40 0.40–1.0 0.50–1.2 0.25 … bal 6101 A96101 0.30–0.7 0.50 0.10 0.03 0.35–0.8...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006482
EISBN: 978-1-62708-207-5
... 0.6-1.1 0.2-0.8 0.8-1.2 bal 6053 A96053 (b) 0.35 0.10 … 1.1–1.4 0.10 0.15–0.35Cr bal 6060 A96060 0.30–0.6 0.10–0.30 0.10 0.10 0.35–0.6 0.15 … bal 6061 A96061 0.40–0.8 0.7 0.15–0.40 0.15 0.8–1.2 0.25 0.04–0.35Cr bal 6063 A96063 0.20–0.6 0.35 0.10 0.10...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006624
EISBN: 978-1-62708-210-5
... 0.15 bal … 6063 A96063 Nominal 0.4 … … … 0.7 … … … … … … … … Limits 0.20–0.6 0.35 0.1 0.1 0.45–0.9 0.1 … 0.1 0.1 0.05 0.15 bal … 6064 A96064 Nominal … … … … … … … … … … … … (oo) Limits 0.4–0.8 0.7 0.15–0.40 0.15 0.8–1.2 0.05–0.14 … 0.25...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006543
EISBN: 978-1-62708-210-5
... … … … … bal … 6061 A96061 0.6 … 0.28 … 1 0.2 … … … bal … Alclad 6061 Alc A96061 0.6 … 0.28 … 1.0 0.2 … … … bal (x) 6062 A96062 0.6 0.35 0.28 … 1.0 0.7 … … … bal … 6063 A96063 0.4 … … … 0.7 … … … … bal … 6064 A96064...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001058
EISBN: 978-1-62708-162-7
... 6262 A96262 AlMg1SiPb 0.40–0.8 0.7 0.15–0.40 0.15 0.8–1.2 0..04–0.14 … 0.25 … … (s) 0.15 0.05 0.15 rem 6063 A96063 AlMg0.5Si 0.20–0.6 0.35 0.10 0.10 0.45–0.9 0.10 … 0.10 … … … 0.10 0.05 0.15 rem 6463 A96463 AlMg0.7Si 0.20–0.6 0.15 0.20 0.05 0.45–0.9...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006626
EISBN: 978-1-62708-210-5
... (a) 6063 A96063 O 2.685 23.4 616–652 218 34 111 0.03 900 … T1, T4 2.685 23.4 616–652 193 29 96 0.035 900 … T5 2.685 23.4 616–652 209 32 105 0.032 900 … T6 2.685 23.4 616–652 200 31 102 0.033 900 … T83 2.685 23.4 616–652 200 31 102 0.033 900...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.9781627081627
EISBN: 978-1-62708-162-7
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006546
EISBN: 978-1-62708-210-5