1-10 of 10 Search Results for

UNS A92017

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006597
EISBN: 978-1-62708-210-5
... use in aircraft structures. Equivalent alloy designations or specifications include: UNS: A92017 ISO or European: AlCuMgS France: A-U46 Germany: AlCuMg1 and 3.1325 Great Britain: L18 and 150A Canada: CM41 Austria: AlCuMg1 Alloy 2017, A2017, and 2117...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001060
EISBN: 978-1-62708-162-7
.... Sheet, plate, wire, rod, bar, shapes, and tube: 160 °C (320 °F) for 18 h at temperature. Forgings: 171 °C (340 °F) for 10 h at temperature 2017<break />4.0Cu-0.6Mg-0.7Mn-0.5Si Specifications ASTM B 211 and B 316 SAE J454 ANSI H38.4 and H38.12 UNS Number A92017...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003123
EISBN: 978-1-62708-199-3
..., and designations and composition limits for aluminum alloys in the form of castings and ingot. It provides helpful information on the Unified Numbering System (UNS) numbers and its corresponding AA numbers for aluminum and aluminum alloys, and the international alloy designations cross-referenced to its equivalent...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006251
EISBN: 978-1-62708-169-6
... … … 0.30 0.20–0.6% Bi; 0.20–0.6% Pb bal 2014 A92014 0.50–1.2 0.7 3.9–5.0 0.40–1.2 0.20–0.8 0.25 … bal 2017 A92017 0.20–0.8 0.7 3.5–4.5 0.40–1.0 0.40–0.8 0.25 … bal 2018 A92018 0.9 1.0 3.5–4.5 0.20 0.45–0.9 0.25 1.7–2.3Ni bal 2024 A92024 0.50 0.50 3.8–4.9 0.30...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006482
EISBN: 978-1-62708-207-5
... 0.50–1.2 0.7 3.9–5.0 0.40–1.2 0.20–0.8 0.25 … bal 2017 A92017 0.20–0.8 0.7 3.5–4.5 0.40–1.0 0.40–0.8 0.25 … bal 2018 A92018 0.9 1.0 3.5–4.5 0.20 0.45–0.9 0.25 1.7–2.3Ni bal 2024 A92024 0.50 0.50 3.8–4.9 0.30–0.9 1.2–1.8 0.25 … bal 2025 A92025 0.50–1.2...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006624
EISBN: 978-1-62708-210-5
... 0.1 … 0.25 0.15 0.05 0.15 bal (i) 2017 A92017 Nominal 0.5 … 4 0.7 0.6 … … … … … … … … Limits 0.20–0.8 0.7 3.5–4.5 0.40–1.0 0.40–0.8 0.1 … 0.25 0.15 0.05 0.15 bal … 2018 A92018 Nominal … … 4 … 0.7 … 2 … … … … … … Limits 0.9 1 3.5–4.5 0.2...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001058
EISBN: 978-1-62708-162-7
... 0.40–1.2 0.20–0.8 0.10 … 0.25 … … (k) 0.15 0.05 0.15 rem 2017 A92017 AlCu4MgSi 0.20–0.8 0.7 3.5–4.5 0.40–1.0 0.40–0.8 0.10 … 0.25 … … (k) 0.15 0.05 0.15 rem 2117 A92117 AlCu2.5Mg 0.20–0.8 0.7 3.5–4.5 0.40–1.0 0.40–1.0 0.10 … 0.25 … … 0.25 Zr + Ti...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006543
EISBN: 978-1-62708-210-5
... … Alclad 2014 Alc A92014 0.8 … 4.4 0.8 0.5 … … … … bal (e) 2017 A92017 0.5 … 4 0.7 0.6 … … … … bal … 2018 A92018 … … 4 … 0.7 … 2 … … bal … 2020 A92020 … … 4.5 0.5 … … … … … bal (f) 2021 A92021 … … 6.3 0.30 … … … … 0.06 bal (g...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006626
EISBN: 978-1-62708-210-5
... 2.713 23 507–638 154 23 74 0.043 900 (a) 2014 A92014 O 2.796 23 507–638 193 29 92 0.035 900 … T4, T451 2.796 23 507–638 134 20 63 0.052 900 … T6, T651 2.796 23 507–638 154 23 74 0.043 900 … 2017 A92017 O 2.796 23.6 513–641 193 29 92 0.035 900...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.9781627081627
EISBN: 978-1-62708-162-7