1-12 of 12

Search Results for UNS A92014

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006596
EISBN: 978-1-62708-210-5
... strength forgings. Equivalent alloy designations or specifications include: UNS: A92014 ISO or European: AlCu4SiMg, AECMA 2387, A-U4SG Canada: CSA CS41N France: NF A-U4SG Germany: DIN AlCuSiMn United Kingdom: BS H15 Alloy 2014 and 2014A composition limits Table 1...
Book Chapter

By Peter Elliott
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003702
EISBN: 978-1-62708-182-5
... about corrosion, sometimes the direct result of poor communication and/or a lack of appreciation of the true service conditions ( Ref 5 ). As an example, a type 316 stainless steel (Unified Numbering System, or UNS, S31600) pipe was considered a suitable choice for admitting steam and subsequently air...
Book Chapter

Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006543
EISBN: 978-1-62708-183-2
... 2.70 0.098 2011 A92011 2.82 0.102 2014 A92014 2.80 0.101 2024 A92024 2.77 0.100 2218 A92218 2.81 0.101 2219 A2219 2.84 0.103 3003 A93003 2.73 0.099 3004 A93004 2.72 0.098 4032 A94032 2.69 0.097 5005 A95005 2.70 0.098 5050 A95050 2.69 0.097...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006624
EISBN: 978-1-62708-210-5
... … 2014 A92014 Nominal 0.8 … 4.4 0.8 0.5 … … … … … … … … Limits 0.50–1.2 0.7 3.9–5.0 0.40–1.2 0.20–0.8 0.1 … 0.25 0.15 0.05 0.15 bal … Alclad 2014 Alc A92014 Nominal 0.8 … 4.4 0.8 0.5 … … … … … … … (i) Limits 0.50–1.2 0.7 3.9–5.0 0.40–1.2 0.20–0.8...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006543
EISBN: 978-1-62708-210-5
... … … … … … … … … … 99.50 (c) 2008 A92008 0.65 … 0.9 … 0.38 … … … … bal … 2010 A92010 … … 1 0.25 0.7 … … … … bal … 2011 A92011 … … 5.5 … … … … … … bal (d) 2013 A92013 0.8 … … … 1 0.2 … … … bal … 2014 A92014 0.8 … 4.4 0.8 0.5 … … … … bal...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003123
EISBN: 978-1-62708-199-3
..., and designations and composition limits for aluminum alloys in the form of castings and ingot. It provides helpful information on the Unified Numbering System (UNS) numbers and its corresponding AA numbers for aluminum and aluminum alloys, and the international alloy designations cross-referenced to its equivalent...
Book Chapter

Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001060
EISBN: 978-1-62708-162-7
... A92014 Government See Table 16 . Foreign Canada: CSA CS41N. France: NF A-U4SG. Germany: DIN AlCuSiMn. ISO: AlCu4SiMg. United Kingdom: BS H15 Chemical Composition Composition Limits of 2014 3.9 to 5.0 Cu, 0.50 to 1.2 Si, 0.7 Fe max, 0.40 to 1.2 Mn, 0.20 to 0.8 Mg, 0.25 Zn max...
Book Chapter

Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006251
EISBN: 978-1-62708-169-6
... … … 0.30 0.20–0.6% Bi; 0.20–0.6% Pb bal 2014 A92014 0.50–1.2 0.7 3.9–5.0 0.40–1.2 0.20–0.8 0.25 … bal 2017 A92017 0.20–0.8 0.7 3.5–4.5 0.40–1.0 0.40–0.8 0.25 … bal 2018 A92018 0.9 1.0 3.5–4.5 0.20 0.45–0.9 0.25 1.7–2.3Ni bal 2024 A92024 0.50 0.50 3.8–4.9 0.30...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006482
EISBN: 978-1-62708-207-5
... 0.05 0.10 … 99.30 1235 A91235 0.65 Si + Fe 0.05 0.05 0.05 0.10 … 99.35 1345 A91345 0.30 0.40 0.10 0.05 0.05 0.05 … 99.45 1350 A91350 0.10 0.40 0.05 0.01 … … … 99.50 2011 A92011 0.40 0.7 5.0–6.0 … … 0.30 0.20–0.6% Bi; 0.20–0.6% Pb bal 2014 A92014...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001058
EISBN: 978-1-62708-162-7
... … 0.05 … 0.10 0.05 0.15 rem 2011 A92011 AlCu6Bi Pb 0.40 0.7 5.0–6.0 … … … … 0.30 … … (j) … 0.05 0.15 rem 2014 A92014 AlCu4SiMg 0.50–1.2 0.7 3.9–5.0 0.40–1.2 0.20–0.8 0.10 … 0.25 … … (k) 0.15 0.05 0.15 rem 2214 A92214 AlCu4SiMg 0.50–1.2 0.30 3.9–5.0...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006626
EISBN: 978-1-62708-210-5
... 2.713 23 507–638 154 23 74 0.043 900 (a) 2014 A92014 O 2.796 23 507–638 193 29 92 0.035 900 … T4, T451 2.796 23 507–638 134 20 63 0.052 900 … T6, T651 2.796 23 507–638 154 23 74 0.043 900 … 2017 A92017 O 2.796 23.6 513–641 193 29 92 0.035 900...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.9781627081627
EISBN: 978-1-62708-162-7