DOI: 10.31399/asm.hb.v02b.a0006590
EISBN: 978-1-62708-210-5
... A08500) and alloy 851.0 (UNS A08510) have similar mechanical properties, but 851.0 is easier to cast and better adapted to the production of complicated parts. With less nickel and a great deal more silicon, 851.0 has better castability and less hot shortness than does 850.0. Alloy 852.0 has fair to poor...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003167
EISBN: 978-1-62708-199-3
... Wrought strip, bonded to steel back Bimetal surface layer Low-tin alloys 9 … … AlSn6CuNi … 91.5 … 1 1 … 6.5 … Cast tubes Solid aluminum alloy bearings 10 A08500 … … … 90.5 … 1 1 1 6.5 … Cast tubes Solid aluminum alloy bearings 11 A08510 … … … 89.5 2.5 1 0.5...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001062
EISBN: 978-1-62708-162-7
... KO-1 Specifications Former ASTM CQ 51A SAE 382 UNS Number A02010 AMS 4228 and 4229 Chemical Composition Composition Limits 4.0 to 5.2 Cu, 0.15 to 0.55 Mg, 0.20 to 0.50 Mn, 0.10 Si max, 0.15 Fe max, 0.15 to 0.35 Ti, 0.40 to 1.0 Ag, 0.05 other (each) max, 0.10...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003123
EISBN: 978-1-62708-199-3
..., and designations and composition limits for aluminum alloys in the form of castings and ingot. It provides helpful information on the Unified Numbering System (UNS) numbers and its corresponding AA numbers for aluminum and aluminum alloys, and the international alloy designations cross-referenced to its equivalent...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006412
EISBN: 978-1-62708-192-4
... Designations and nominal composition of tin-base bearing alloys Designation (a) Composition, % Product form Applications UNS SAE ISO ASTM (B23) Sa Sb Cu Other L13910 … … Alloy 1 91 4.5 4.5 … Cast on steel or bronze back Bimetal surface layer L13870 … … Alloy 11 87 7 6...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006251
EISBN: 978-1-62708-169-6
... rather widely known alloy classification system is the Unified Numbering System (UNS), which is a system that covers all metallic alloy systems ( Ref 2 ). For aluminum alloys, the UNS system is essentially an adaptation of the Aluminum Association alloy designation system, whereby the UNS format involves...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006482
EISBN: 978-1-62708-207-5
... Association is the registrar under ANSI H35.1 with respect to the designation and composition of aluminum alloys and tempers registered in the United States. Another rather widely known alloy classification system is the Unified Numbering System (UNS), which is a system that covers all metallic alloy systems...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001058
EISBN: 978-1-62708-162-7
... designations. It also tabulates the grade designations and compositions of wrought and cast aluminum and aluminum alloys. The article provides information on cross-referencing of aluminum wrought and ingot/cast products according to composition, per the Aluminum Association, Unified Numbering System (UNS...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.9781627081627
EISBN: 978-1-62708-162-7
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006548
EISBN: 978-1-62708-210-5
... … … … … … … … … 713.0 613 Tenzaloy A07130 Tenzaloy ZC81A 315 … … … 771.0 … Precedent 71A A07710 Precedent 71A … … … … … 772.0 B771 Precedent 71B A07720 Precedent 71B … … … … … 850.0 750 … A08500 750 … … … … … 851.0 A850 … A08510 A750 … … … … … 852.0 B850...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006551
EISBN: 978-1-62708-210-5
... … 91.5 … 1 1 … 6.5 … Cast tubes Solid aluminum alloy bearings 10 A08500 … … … 90.5 … 1 1 1 6.5 … Cast tubes Solid aluminum alloy bearings 11 A08510 … … … 89.5 2.5 1 0.5 … 6.5 … Cast tubes Solid aluminum alloy bearings 12 A08520 … … … 89.5 … 2 1.2 1 6.5...