... in brazing of the lower melting brazeable aluminum alloys, such as wrought alloy 6151 (UNS A96151) and cast alloys 443.0 (UNS A04430) and 356.0 (UNS A03560), because the melting range of these filler metals approaches closely or overlaps the melting range of the work metal. Copper-Phosphorus Alloys...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006568
EISBN: 978-1-62708-210-5
... and/or the heat treatment used (see also the datasheet for 357 type alloys in this Volume). Alloy 356.0 and A356.0 composition limits Table 1 Alloy 356.0 and A356.0 composition limits Element (a) Alloy (UNS) 356.0 (A03560) A356.0 (A13560) Si 6.5–7.5 6.5–7.5 Fe 0.6 max 0.20 max Cu...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004139
EISBN: 978-1-62708-184-9
...-saturated, oxygen-depleted wood. A combination of corrosion resistance and mechanical strength is needed that exceeds most mild steel and common brass. Most of the copper alloy seavalves, seacocks, or through-hulls and other underwater fittings are made of cast phosphor bronze (UNS C94300) or a cast...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006543
EISBN: 978-1-62708-183-2
... 2.70 0.098 7075 A97075 2.80 0.101 7079 A97079 2.74 0.099 7178 A97178 2.82 0.102 Casting alloys 242.0 A02420 2.81 0.102 295.0 A02950 2.81 0.102 356.0 A03560 2.68 0.097 380.0 A03800 2.76 0.099 413.0 A04130 2.66 0.096 443.0 A04430 2.69 0.097...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001062
EISBN: 978-1-62708-162-7
... KO-1 Specifications Former ASTM CQ 51A SAE 382 UNS Number A02010 AMS 4228 and 4229 Chemical Composition Composition Limits 4.0 to 5.2 Cu, 0.15 to 0.55 Mg, 0.20 to 0.50 Mn, 0.10 Si max, 0.15 Fe max, 0.15 to 0.35 Ti, 0.40 to 1.0 Ag, 0.05 other (each) max, 0.10...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006482
EISBN: 978-1-62708-207-5
... Association is the registrar under ANSI H35.1 with respect to the designation and composition of aluminum alloys and tempers registered in the United States. Another rather widely known alloy classification system is the Unified Numbering System (UNS), which is a system that covers all metallic alloy systems...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003123
EISBN: 978-1-62708-199-3
..., and designations and composition limits for aluminum alloys in the form of castings and ingot. It provides helpful information on the Unified Numbering System (UNS) numbers and its corresponding AA numbers for aluminum and aluminum alloys, and the international alloy designations cross-referenced to its equivalent...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006251
EISBN: 978-1-62708-169-6
... rather widely known alloy classification system is the Unified Numbering System (UNS), which is a system that covers all metallic alloy systems ( Ref 2 ). For aluminum alloys, the UNS system is essentially an adaptation of the Aluminum Association alloy designation system, whereby the UNS format involves...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001058
EISBN: 978-1-62708-162-7
... 0.40–0.6 … … 0.10 … 0.20 0.05 0.15 rem C355.1 A33351 … Ingot 4.5–5.5 0.15 1.0–1.5 0.10 0.45–0.6 … … 0.10 … 0.20 0.05 0.15 rem C355.2 A33352 … Ingot 4.5–5.5 0.13 1.0–1.5 0.05 0.50–0.6 … … 0.05 … 0.20 0.05 0.15 rem 356.0 A03560 3522 AlSi7Mg R2147 AlSi7Mg...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006548
EISBN: 978-1-62708-210-5
... 333 … A03330 333 … … … … … 336.0 A332 … A03360 A132 SN122A 321 … Al-Si12Cu 48000 354.0 354 … A03540 … … … C354 … … 355.0 355 … A03550 355 SC51A 322 4210 Al-Si5Cu1Mg 45300 C355.0 C355 … A33550 C355 SC51B 355 C355 … … 356.0 356 … A03560 356...