Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005255
EISBN: 978-1-62708-187-0
... materials. It presents recommendations that which serve as a useful guide to the design of investment castings. The article tabulates the applications of the process and illustrates the Shellvest system for investment casting of small parts. It explains the manufacturing process of ceramic shell molds and...