Published: 01 December 2008
Fig. 10 Sequence of operations used in the Shaw all-ceramic mold process More
Image
Published: 01 December 2008
Fig. 11 Diagram of Shaw composite mold process More
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005249
EISBN: 978-1-62708-187-0
..., high-alumina mullite slurries for molding. The Shaw process and the proprietary Unicast processes are also discussed. ceramic molding foamed plaster process match plate pattern molding plaster molding conventional plaster mold casting slurry molding Antioch process Shaw process Unicast...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001239
EISBN: 978-1-62708-170-2
.... , Peters J. , and Tonshoff H.K. , Residual Stresses—Measurement and Causes in Machining Processes , Annals of CIRP , Vol 31 ( No. 2 ), 1982 , p 491 – 510 10.1016/S0007-8506(07)60172-3 6. Chandrasekar S. , Shaw M.C. , and Bhushan B. , A Comparison of the Grinding...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003172
EISBN: 978-1-62708-199-3
...) Phenolic ester No-bake resin binder processes Furan (acid catalyzed) Oil urethane Phenolic urethane Polyol urethane Silicate and phosphate bonds Sodium silicate/CO 2 Shaw process (ceramic molding) Unicast process (ceramic molding) Alumina phosphate Plaster bonds...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004107
EISBN: 978-1-62708-184-9
... on Steel,” STP 947, DiBari G.A. and Harding W.B. , Ed., American Society for Testing and Materials , 1987 , p 211 – 234 10.1520/STP20039S 2. “Corrosion Tests of Flame-Sprayed Coated Steel 19-Year Report,” American Welding Society , Miami, FL , 1974 3. Shaw B.A...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006297
EISBN: 978-1-62708-179-5
... Abstract Aggregate molding, or sand casting, is the gravity pouring of liquid metal into a mold that is made of a mixture molded against a permanent pattern. This article summarizes the most important materials in the process of sand casting of cast iron, including different types of molding...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001238
EISBN: 978-1-62708-170-2
.... , Leskovar P. , Peters J. , and Tonshoff H.K. , Residual Stresses—Measurement and Causes in Machining Processes , Ann. CIRP , Vol 31 ( No. 2 ), 1982 , p 491 – 510 10.1016/S0007-8506(07)60172-3 31. Snoeys R. , Thermal Damage in Grinding , Proc. Milton C. Shaw Grinding Symp...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005503
EISBN: 978-1-62708-197-9
..., the Reynolds number (a dimensionless number characterizing a ratio of inertia force to viscous force) is low, and the flow is modeled as a creeping flow with lubrication, as treated with the Hele-Shaw formulation. With the Hele-Shaw model, the continuity and momentum equations for the melt flow...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003186
EISBN: 978-1-62708-199-3
... , Ellis Horwood , 1989 • Oxley P.L.B. , The Mechanics of Machining , Ellis Horwood , 1989 • Shaw M.C. , Metal Cutting Principles , 4th ed. , Oxford University Press , 1984 • Stephenson D.A. and Agapiov J.S. , Metal Cutting Theory and Practice , Dekker...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005519
EISBN: 978-1-62708-197-9
... ( Ref 8 ) developed a slip line field assuming multiple shear planes, which also fell short in terms of accuracy but provided further insight into the mechanics of chip formation. Semiatin and Rao ( Ref 9 ) extended Merchant's theory and the temperature predictions of Loewen and Shaw to develop...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001114
EISBN: 978-1-62708-162-7
.... , Proceedings of Conference on Superconducting Materials and Applications , 1989 14. Shaw D.T. et al. , Plasma-Assisted Laser Deposition of Superconducting Films Without Post-Annealing , to be published in Superconductivity: Theory and Applications 15. Beasley M.R. and Kircher...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004123
EISBN: 978-1-62708-184-9
... CPCR-2 Project 1L1612105AH84, U.S. Army Armament Research, Development and Engineering Center • Shaw G. , Optimizing Paint Durability, Part I , Prod. Finish. , Nov 2004 , p 42 – 46 • Uhlig H.H. and Revie R.W. , Corrosion and Corrosion Control, An Introduction...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005286
EISBN: 978-1-62708-187-0
... Explosions , Light Metals 1991 , TMS , 1991 • Faunce J.P. , Wagstaff F.E. , and Shaw H. , New Casting Method for Improving Billet Quality (Air-Slip) , Light Metals 1984 , TMS , 1984 • Fjaer H.G. and Jensen E.K. , Mathematical Modeling of Butt Curl Deformation...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006485
EISBN: 978-1-62708-207-5
... Aluminum Extrusion Technology Seminar , 1988 • Epstein S.G. , Causes and Prevention of Molten Aluminum-Water Explosions , Light Metals 1991 , TMS , 1991 • Faunce J.P. , Wagstaff F.E. , and Shaw H. , New Casting Method for Improving Billet Quality (Air-Slip) , Light...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004132
EISBN: 978-1-62708-184-9
.... “Supercritical Water Oxidation—Achievements and Challenges in Commercial Applications,” a workshop sponsored by the Office of Naval Research (ONR) , Arlington, VA , Aug 2001 2. Shaw R.W. , Supercritical Water Oxidation of Toxic Military Materials: Current Status , Proc. of The International...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006045
EISBN: 978-1-62708-175-7
... Titanium Powders , Science and Technology of Powder Materials: Synthesis, Consolidation and Properties , Shaw L. et al. , Ed., TMS , 2005 , p 151 – 158 15. Duz V.A. , Ivasishin O. , Lavender C. , Moxson V.S. , and Telin V.V. , Innovative Powder Metallurgy...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006550
EISBN: 978-1-62708-290-7
... Process and System , U.S. Patent 4,665,492 , 1987 , https://patentimages.storage.googleapis.com/b9/08/3e/a4364a808e722a/US4665492.pdf 10.1016/0736-5845(87)90060-3 5. Blazdell P.F. , Evans J.R.G. , Edirisinghe M.J. , Shaw P. , and Binstead M.J. , The Computer Aided...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001232
EISBN: 978-1-62708-170-2
... products and materials, abrasive finishing processes, and the mechanisms of delivering the abrasives to the grinding or machining zone. Abrasive finishing processes, such as grinding, honing, superfinishing, microgrinding, polishing, buffing, and lapping, are discussed. The article presents a brief...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006942
EISBN: 978-1-62708-395-9
... Abstract Failure analysis is the process used to determine the cause of a failure. There is no definitive method for performing a failure analysis, and the method chosen is dependent upon the type of failure, the availability of background information, the tools available to perform...