Skip Nav Destination
Close Modal
Search Results for
Pumping plants
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 399 Search Results for
Pumping plants
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006059
EISBN: 978-1-62708-172-6
... later in this article. When the conveyed wastewater reaches pump stations, it collects in wet wells from which suction inlets to pumps are positioned. The pumps convey the wastewater to another pump station or storage facility or onward to a treatment plant. The headspace surfaces, typically cast...
Abstract
This article provides information on the municipal wastewater system components such as piping, pump stations, headworks, clarifiers, aeration structures, digesters, biosolids dewatering equipment, and sludge stabilization. It explains the major corrosion damage mechanisms to which those component parts of the system are exposed. It presents useful guidelines for selecting and using protective coatings in municipal sewerage collection systems and water reclamation facilities in wastewater treatment plants. The article includes annotated flow diagrams of a wastewater collection system, wastewater treatment plants, and spreadsheets listing the most widely used generic coating systems by structure and substrate material. It concludes with a section on quality watchouts when selecting or using protective coatings in municipal wastewater systems.
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005851
EISBN: 978-1-62708-167-2
...-loop nonferrous recirculating system to cool the power supply, heat station, coils, bus, and water-cooled leads/cables. All use some sort of water-to-water heat exchanger in conjunction with plant water (dirty water) supplied by a cooling tower, radiator/fan, refrigeration-type chillers, city water...
Abstract
Cooling towers are designed to remove heat from water in an induction system and dissipate it into the atmosphere. This article provides information on closed-loop recirculating water systems of an induction system to cool the power supply. It focuses on various types of cooling towers, namely, air-cooled heat exchangers, air-cooled heat exchangers with trim cooler, closed-circuit evaporative cooling towers, and open evaporative cooling towers. The article discusses the importance of their placement or positioning to reduce the chances of air recirculation, and concludes with a discussion on refrigerant chillers.
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006040
EISBN: 978-1-62708-172-6
... vertical-shaft lift pumps or centrifugal pumps that convey raw water from reservoirs or holding tanks to a treatment plant through either aqueducts or large-diameter water transmission piping. The pumps are commonly coated externally but not internally. If they are coated internally, fusion-bonded epoxy...
Abstract
This article presents information regarding the use of protective coatings in municipal potable water systems, including raw water collection and transmission, water treatment plants, and treated water distribution. It provides useful guidance for the selection and use of protective coatings in these municipal water systems. The most commonplace corrosion-damage mechanisms are highlighted. The article describes the most common materials of construction found in municipal water systems, namely, cast iron, ductile iron, carbon steel, precast concrete cylinder pipe and reinforced concrete pipe, prestressed concrete tanks, and stainless steel. It provides information on the most common generic coating systems used for new steel tanks and water storage tanks. It concludes with a discussion of quality watch-outs when selecting or using protective coatings in municipal water systems.
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006035
EISBN: 978-1-62708-172-6
... and the PWR include emergency core cooling systems. The article describes a DBA test and other coating performance parameters necessary for safety-related coating systems. It provides a detailed account of the selection criteria of coating types in a nuclear plant. The article concludes by highlighting...
Abstract
Surface coatings are essential in all facilities that process nuclear materials or use nuclear fission for power generation. This article describes the coatings used in two basic types of Generation 3 nuclear reactor designs in the United States and their containment size. These reactors are the boiling water reactor (BWR) and pressurized water reactor (PWR). The article provides information on the loss-of-coolant accident (LOCA) identified as the design basis accident (DBA), which can rapidly de-water the core of an operating nuclear reactor. To avoid LOCA, both the BWR and the PWR include emergency core cooling systems. The article describes a DBA test and other coating performance parameters necessary for safety-related coating systems. It provides a detailed account of the selection criteria of coating types in a nuclear plant. The article concludes by highlighting protective coating strategies in Generation 3 Plants.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004176
EISBN: 978-1-62708-184-9
... a chemical processing plant, considerable attention is paid to fluid flows, sizing of lines, pumps and processing equipment, and temperatures and pressures. Materials are selected on the basis of past experience, corrosion tests, corrosion literature, and the recommendations of materials suppliers...
Abstract
This article focuses on the effects of process variables on corrosion of metals in processing plants: plant environments; startup, shutdown, and downtime conditions; and seasonal temperature changes. It also tabulates the effects of process variables on corrosion of metals in aggressive environments.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004133
EISBN: 978-1-62708-184-9
... improvement over a subcritical 16.5 MPa/538 °C/538 °C plant with an efficiency of 37% (high heating value) Steam conditions Power plant examples Net percentage point increase in efficiency Net plant efficiency, % 28.4 MPa/538 °C/538 °C … 2.5 39.5 28.4 MPa/538 °C/566 °C Schwarze Pump, 1998...
Abstract
This article describes the control of water chemistry in the steam cycle of a power plant for achieving corrosion control, deposition prevention, and higher cycle efficiency. It discusses the materials requirements of the components exposed to supercritical water in supercritical (SC) and ultrasupercritical (USC) power plants. These components include high-pressure steam piping and headers, superheater and reheater tubing, water wall tubing in the boiler, high-and intermediate-pressure rotors, rotating blades, and bolts in the turbine section. The article reviews the boiler alloys, used in SC and USC boilers, such as ferritic steels, austenitic steels, and nickel-base alloys. It provides information on the materials used in turbine applications such as ferritic rotor steels, turbine blade alloys, and bolting materials. The article explains various factors influencing steamside corrosion in SC power plants. It also deals with the role of overall efficiency in the USC power generation.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004223
EISBN: 978-1-62708-184-9
..., that is, boiling water reactors (BWRs) and pressurized water reactors (PWRs), is necessary. Although corrosion was considered in all plant designs, corrosion was not considered as a serious problem. The major concern was general corrosion, and it was well known at the time of LWR design and construction...
Abstract
This article reviews a series of serious corrosion problems that have plagued the light water reactor (LWR) industry. It discusses the complex corrosion mechanisms involved, and the development of practical engineering solutions for their mitigation. The article contains tables that present the corrosion history of LWRs, and the ten most expensive operation and maintenance costs of corrosion for a particular reactor site.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005350
EISBN: 978-1-62708-187-0
... an electric motor rather than an air motor. Plant air is the most expensive energy source in the plant. A small blower keeps the pump cool. Treat the Cause of Dross Buildup Treat the cause of dross buildup, not the symptom. Investigate why the furnace is generating dross. Typical reasons are: Air...
Abstract
This article illustrates the basic components of dry and wet hearth reverberatory furnaces. It discusses stack melters that are used for aluminum metal casting, as they are efficient in sealing the furnace and using the flue gases to preheat the charge materials. The article describes the various factors for improving and maintaining furnace efficiencies. It explains the benefits of circulating molten metal in reverberatory furnaces and circulation methods.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004102
EISBN: 978-1-62708-184-9
... condenser cooling system that condenses the main process steam for reuse in the cycle. Service water systems cool a wide range of plant components, some common to most power plants regardless of fuel type, including turbine lubricating oil coolers, generator hydrogen coolers, and pump lubricating oil...
Abstract
This article describes the corrosion mechanisms, challenges, and control methods in service water distribution systems. It provides a discussion on typical designs and water qualities for distribution systems used in fossil-fueled and nuclear power plants. The article also explains the techniques for controlling corrosion in service water systems.
Book Chapter
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004161
EISBN: 978-1-62708-184-9
... with conventional fly ash/bottom ash handling systems may be grouped into two categories: Corrosion and erosion (material deterioration) Scaling and plugging (material buildup) These problem areas must be addressed by designers of ash-handling systems and plant operators, who should consider factors...
Abstract
Ash handling is a major challenge for utilities and industries using coal as a primary fuel. This article discusses the operating problems associated with conventional fly ash/bottom ash handling systems. It describes the two types of fly ash systems, namely, dry and wet fly ash systems. The article presents the ways to minimize operating problems that occur due to corrosion, erosion, scaling, and plugging.
Book Chapter
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003567
EISBN: 978-1-62708-180-1
... increase wear damage in wet and aqueous environments have been identified ( Ref 1 ). Slurry Handling The movement of materials as a slurry is an efficient means of transportation that is used in many industries. However, the movement of these slurries can cause significant corrosive wear. Pumps...
Abstract
This article focuses on the corrosion-wear synergism in aqueous slurry and grinding environments. It describes the effects of environmental factors on corrosive wear and provides information on the impact and three-body abrasive-corrosive wear. The article also discusses the various means for combating corrosive wear, namely, materials selection, surface treatments, and handling-environment modifications.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004137
EISBN: 978-1-62708-184-9
... and will attack most metal compounds. Fiberglass or other thermoplastics have found extensive use in wastewater plants for this reason ( Fig. 6 ). The scrubber housing, recycle pump, and related components are typically made of fiberglass using vinyl-ester resins with synthetic veils. Where critical components...
Abstract
Corrosion problems and materials selection for emissions control equipment can be difficult because of varied corrosive compounds present and the severe environments encountered. This article discusses the selection of materials for construction of flue gas desulfurization systems. It addresses the problems associated with materials for incinerator off-gas treatment equipment. The off-gases can be classified according to their corrosiveness as: industrial chemical, hospital, municipal solid, and sewage sludge. The article provides information on the selection of materials for the three most common types of dust collection equipment used in bulk solids processing, namely, fabric filters, electrostatic precipitators, and wet scrubbers. It also discusses a wide variety of corrosion problems encountered in chemical and pharmaceutical industries.
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005923
EISBN: 978-1-62708-166-5
... Abstract Quenchant agitation can be obtained by circulating quenchant in a quench tank through pumps and impellers. The selection of the agitation method depends on the tank design, type and volume of the quenchant, part design, and the severity of quench required. This article describes flow...
Abstract
Quenchant agitation can be obtained by circulating quenchant in a quench tank through pumps and impellers. The selection of the agitation method depends on the tank design, type and volume of the quenchant, part design, and the severity of quench required. This article describes flow measurement methods, temperature control, materials handling, and filtration processes during the agitation process. The maintenance of quenching installations is also discussed.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005285
EISBN: 978-1-62708-187-0
... implications of dross, and in-plant enhancement or recovery of dross. It discusses the influence of the melter type on dross generation and the influence of charge materials and operating practices on melt loss. Fluxing is a word applied in a broad sense to a number of melt-treating methods. The article also...
Abstract
Dross, which is the oxide-rich surface that forms on melts due to exposure to air, is a term that is usually applied to nonferrous melts, specifically the lighter alloys such as aluminum or magnesium. This article describes dross formation and ways to reduce it, the economic implications of dross, and in-plant enhancement or recovery of dross. It discusses the influence of the melter type on dross generation and the influence of charge materials and operating practices on melt loss. Fluxing is a word applied in a broad sense to a number of melt-treating methods. The article also discusses the in-furnace treatment with chemical fluxes.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004153
EISBN: 978-1-62708-184-9
... Abstract This article begins with a discussion on the components and importance of flue gas desulfurization (FGD) technology used in power plant for pollution control. It further discusses the corrosion problems encountered in different operating zones of FGD system and the major forms...
Abstract
This article begins with a discussion on the components and importance of flue gas desulfurization (FGD) technology used in power plant for pollution control. It further discusses the corrosion problems encountered in different operating zones of FGD system and the major forms of corrosive attack encountered in those zones, including crevice corrosion, pitting corrosion, and acid attack. The article concludes with information on the materials selection and design features for minimizing the possibility of corrosion.
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001080
EISBN: 978-1-62708-162-7
... Chemical processing Storage tanks, agitators, pumps, columns, frames, screens, mixers, valves, pressurized reactors, filters, piping and tubing, heat exchangers, electrodes and anode baskets for metal and chlorine-alkali electrolysis Energy industry Power generating plants Condensers, cooling...
Abstract
Titanium has been recognized as an element with good mechanical and physical properties, alloying characteristics, and corrosion resistance. Providing an outline of general characteristics and types of titanium alloys, this article discusses the contemporary technology of titanium along with its market developments. It also discusses the application of titanium and titanium alloys in corrosive environments and in aerospace and automotive industries. The article describes the developments in titanium processing and materials technologies, which include the development of sponge production and melting processes, oxide dispersion-strengthened alloys by powder metallurgy techniques, titanium-base intermetallic compounds, and titanium-matrix composites.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003660
EISBN: 978-1-62708-182-5
... equipment, such as in piping, pumps, valves, and condensers. Although techniques are available commercially for on-line insertion and retrieval of test specimens, that is, without plant shutdown, they are not used routinely in all industries because of cost. Mass-Loss Tests For engineering...
Abstract
Uniform corrosion refers to the attack on an exposed metal surface that results in homogeneous thickness loss that is evaluated by mass loss or measurement of thickness change. This article focuses on the various processes involved in mass loss tests, namely, selection and preparation of suitable test specimens, planning of the experimental technique, posttest sample cleaning, data acquisition, and reporting. It further discusses the test variables addressed during the experimental planning and provides an overview of the other test and evaluation methods of evaluating uniform corrosion.
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006400
EISBN: 978-1-62708-192-4
... of maintenance philosophies. The article concludes with a discussion on various condition monitoring in industrial sectors, including condition-monitoring techniques in nuclear power plants, road condition monitoring, and condition monitoring in wind turbines. acoustic emission testing condition...
Abstract
This article introduces the concept of condition monitoring (CM) and summarizes various techniques used for CM across the industrial sectors. The techniques include visual inspection, performance monitoring, vibration condition monitoring, vibration condition monitoring, lubricant oil analysis, acoustic emission testing, temperature monitoring, motor current signature analysis, and ultrasound emission. The article describes the evolution of condition-based maintenance in CM. It also describes the basics of integrated vehicle health management, a capability that enables a number of maintenance philosophies. The article concludes with a discussion on various condition monitoring in industrial sectors, including condition-monitoring techniques in nuclear power plants, road condition monitoring, and condition monitoring in wind turbines.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004152
EISBN: 978-1-62708-184-9
...-to-tubesheet joint heater shell IN STEAM TURBINE ELECTRICAL POWER GENERATION PLANTS, turbine exhaust steam is condensed, and the condensate is reheated for return as feedwater to the boiler. Water from the condenser to the feedwater pump is called condensate, and from the pump to the boiler...
Abstract
This article addresses the major heat-transfer components of the water-steam loop of a power plant. It describes the various types of condensers, including water-cooled condensers and air-cooled condensers. The article explains the corrosion mechanisms encountered in the condensers, including erosion-corrosion, galvanic corrosion, and pitting corrosion. It discusses the types of deaerators and deals with their corrosion problems. The article provides a discussion on two types of feedwater heaters: channel feedwater heaters and header feedwater heaters. It summarizes the corrosion problems associated with common feedwater heater tube materials.
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005899
EISBN: 978-1-62708-167-2
...% Figure 24 shows a diagram of the furnace cooling circuit for a tandem plant. It is characterized by a 40 °C (104 °F) inlet temperature and a maximum 67 °C (152.6 °F) outlet temperature, a tank automatically filled via level probes and switchoff in case of a lack of water, a second pump to act...
Abstract
This article provides a detailed discussion on the components of a high-performance induction crucible furnace system, namely, furnace body, power supply, and peripheral components. The furnace body contains refractory lining, coil and transformer yokes, and tilting frame and furnace cover. The power supply consists of the following: transformers, frequency converters, capacitor banks, and power cables and furnace coils. The peripheral components comprise recooling device, charging system, and skimming devices. The article also presents a three-dimensional representation of the induction crucible furnace system.