...Nominal compositions of pertinent Ni-Fe-Cr-(Mo) corrosion-resistant alloys Table 1 Nominal compositions of pertinent Ni-Fe-Cr-(Mo) corrosion-resistant alloys UNS No. Name Composition, wt% Ni Cr Fe Mo W Cu C Nb Ti Al Others … 27-7Mo 27 22 42 7.2 … 1...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003821
EISBN: 978-1-62708-183-2
...Abstract Abstract This article reviews the corrosion behavior in various environments for seven important nickel alloy families: commercially pure nickel, Ni-Cu, Ni-Mo, Ni-Cr, Ni-Cr-Mo, Ni-Cr-Fe, and Ni-Fe-Cr. It examines the behavior of nickel alloys in corrosive media found in industrial...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006265
EISBN: 978-1-62708-169-6
...-Cu), Inconel (Ni-Cr-Mo), Hastelloy (Ni-Mo-Cr), and Incoloy (Ni-Fe-Cr) families of alloys. The heat treatment processes for gamma prime nickel alloys, gamma prime nickel-iron superalloys, and gamma double-prime nickel-iron superalloys are also included. The article also provides information on age...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006238
EISBN: 978-1-62708-163-4
...Abstract Abstract This article is a compilation of ternary alloy phase diagrams for which cobalt (Co) is the first-named element in the ternary system. The other elements are Cr, Cu, Fe, Mo, Ni, Ti, V, and W. The diagrams are presented with element compositions in weight percent. The article...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006239
EISBN: 978-1-62708-163-4
...Abstract Abstract This article is a compilation of ternary alloy phase diagrams for which chromium (Cr) is the first-named element in the ternary system. The other elements are Fe, Mn, Mo, N, Nb, Ni, Ti, V and W. The diagrams are presented with element compositions in weight percent...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006233
EISBN: 978-1-62708-163-4
...Abstract Abstract This article is a compilation of ternary alloy phase diagrams for which aluminum (Al) is the first-named element in the ternary system. The other elements are C, Co, Cr, Cu, Fe, Ga, Li, Mg, Mn, Mo, Nb, Ni, Sb, Si, Ti, U, V and Zn. The diagrams are presented with element...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006236
EISBN: 978-1-62708-163-4
...Abstract Abstract This article is a compilation of ternary alloy phase diagrams for which carbon (C) is the first-named element in the ternary system. The other elements are Co, Cr, Cu, Fe, Mn, Mo, N, Ni, S, Si, Ti, V, and W. The diagrams are presented with element compositions in weight...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006241
EISBN: 978-1-62708-163-4
....” “B-C-Fe (Boron - Carbon - Iron)” in the article “B (Boron) Ternary Phase Diagrams.” “C-Cr-Fe (Carbon - Chromium - Iron)” , “C-Cu-Fe (Carbon - Copper - Iron)” , “C-Fe-Mn (Carbon - Iron - Manganese)” , “C-Fe-Mo (Carbon - Iron - Molybdenum)” , “C-Fe-N (Carbon - Iron - Nitrogen)” , “C-Fe-Ni...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006243
EISBN: 978-1-62708-163-4
... - Molybdenum).” and “Co-Mo-Ni (Cobalt - Molybdenum - Nickel).” in the article “Co (Cobalt) Ternary Phase Diagrams.” “Cr-Fe-Mo (Chromium - Iron - Molybdenum).” , “Cr-Mo-Ni (Chromium - Molybdenum - Nickel).” , “Cr-Mo-W (Chromium - Molybdenum - Tungsten).” , “Fe-Mo-Nb (Iron - Molybdenum - Niobium...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003619
EISBN: 978-1-62708-182-5
...Nominal compositions of selected corrosion-resistant nickel alloys Table 2 Nominal compositions of selected corrosion-resistant nickel alloys UNS No. Alloy name Composition, % Ni Cr Cu Mo Fe W Others Commercially pure nickel N02200 Ni-200 99.6 … … … 0.2 … 0.2...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001072
EISBN: 978-1-62708-162-7
... alloys with about 0.03% B or greater; borides appear similar to carbides, but are not attacked by preferential carbide etchants; M elements can be molybdenum, tantalum, niobium, nickel, iron, or vanadium c 0 = 0.300–0.330 V 3 B 2 Nb 3 B 2 (Mo,Ti,Cr,Ni,Fe) 3 B 2 Mo 2 FeB 2 MN Cubic...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006341
EISBN: 978-1-62708-179-5
... Austenite + carbide Fe 0 Fe Al + + Cr − + Cu + − Mn − − Mo − − Ni + − Si + − Ti − + V − + Compositions in wt% of the high-silicon ferritic iron castings of ASTM A1095 Table 2 Compositions in wt% of the high-silicon ferritic iron castings of ASTM...
Book Chapter

Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006292
EISBN: 978-1-62708-163-4
... , Be 13 Ho, Be 13 Zr, Cd 13 Cs, KZn 13 Fe 3 W 3 C Fd 3 m η-carbide. For Fe 3 W 3 C, a = 11.06 Å. Examples: CoNb 2 (C, N, O) x , Co 2 Mo 4 C, Cr 3 Nb 3 C, η Fe 2 Nb 3 , Fe 3 Mo 3 C, Fe 3 Mo 3 N, Fe 3 W 3 C, Mn 3 Mo 3 C, Mo 3 Ni 3 C, NiTi 2 , Ni 3 W 3 C cF 116 Cr 23 C 6 Fm 3 m...
Book Chapter

Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003722
EISBN: 978-1-62708-177-1
... , Co 2 Mo 4 C, Cr 3 Nb 3 C, η Fe 2 Nb 3 , Fe 3 Mo 3 C, Fe 3 Mo 3 N, Fe 3 W 3 C, Mn 3 Mo 3 C, Mo 3 Ni 3 C, NiTi 2 , Ni 3 W 3 C cF 116 Cr 23 C 6 Fm 3 m For Cr 23 C 6 , a = 10.66 Å. Examples: Mn 23 C 6 , Fe 21 Mo 2 C 6 Mn 23 Th 6 (Cu 16 Mg 6 Si 7 ) Fm 3 m For Mn 23 Th 6...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006111
EISBN: 978-1-62708-175-7
..., Fe-Cu-Ni-C 1120–1250 2050–2280 Fe-Cu-Ni-Mo (diffusion alloyed)-C 1120–1250 2050–2280 Fe-Mn, Fe-Mn-C 1120–1280 2050–2335 Fe-Cr, Fe-Cr-C, Fe-Cr-Mo-C 1120–1280 2050–2335 Fe-Mn-Cu 1120 2050 Fe-Cr-Cu 1200–1280 2190–2335 Fe-Mo, Fe-Mo-C 1120–1280 2050–2335 Fe-Cr-carbide...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003737
EISBN: 978-1-62708-177-1
...Compositions of Fe-Cr-Ni heat-resistant casting alloys Table 1 Compositions of Fe-Cr-Ni heat-resistant casting alloys Grade Type Composition, % C Mn, max Si, max P, max S, max Cr Ni Mo, max (a) HF 19 chromium, 9 nickel 0.20–0.40 2.00 2.00 0.04 0.04...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004189
EISBN: 978-1-62708-184-9
... , 1990 Sulfidation High-Temperature Corrosion by Halogen and Halides Nitridation Metal Dusting Carburization Oxidation Carbon and Chromium-Molybdenum (Cr-Mo) Steels Stainless Steels Iron-Nickel-Chromium (Fe-Ni-Cr) and Nickel-Base Alloys Metals and alloys are susceptible...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003148
EISBN: 978-1-62708-199-3
... alloys Table 2 Compositions of various cobalt-base alloys Alloy tradename UNS No. Nominal composition, wt% Co Cr W Mo C Fe Ni Si Mn Others Stellite wear-resistant alloys Stellite 1 R30001 bal 30 13 0.5 2.5 3 1.5 1.3 0.5 … Stellite 4 … bal 30 14 1 (max...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006364
EISBN: 978-1-62708-192-4
...-, and iron-base alloys typically used for wear-protection applications Table 4 Nickel-, cobalt-, and iron-base alloys typically used for wear-protection applications Designation Co Ni Fe Cr C B Si Mn Mo W Hardness (a) , HV 30 Application Nickel-base alloys Ni40 … bal 2.0...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003617
EISBN: 978-1-62708-182-5
... m.p. 1290 m.p. A,D,F Sigma σ AB (Fe,Cr,Mo,Ni) 550–1050 1020–1920 A,D,F Chi χ A 48 B 10 Fe 36 Cr 12 Mo 10 (FeNi) 36 Cr 18 (TiMo) 4 600–900 1110–1650 D,F Alpha prime α′ … CrFe(Cr 61–83%) 350–550 660–1020 A,D,F Laves η A 2 B (FeCr) 2 (Mo,Nb,Ti,Si) 550–900 1020–1650...