1-20 of 153 Search Results for

Ni-Al bronze (wrought nickel-aluminum bronze)

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005444
EISBN: 978-1-62708-196-2
... Cupro-nickel, 30% 0.07 Cupro-nickel, 10% 0.095 Nickel silver, 65-18 0.08 Nickel silver, 55-18 0.07 Nickel silver, 65-12 0.10 High-silicon bronze (A) 0.09 Low-silicon bronze (B) 0.14 Aluminum bronze, 5% Al 0.198 Aluminum bronze, (3) 0.18 Aluminum-silicon bronze 0.108...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006281
EISBN: 978-1-62708-169-6
... Si C91600 … 86.0 min to 90.0 (b) (c) max 0.25 max 0.20 max 9.7–1.8 0.25 max 0.30 (d) max 0.05 max S; 1.2 min to 2.0 max Ni (e) ; 0.20 max Sb; 0.005 max Al; 0.005 max Si C91700 Nickel gear bronze 84.0 (b) (c) min to 87.0 max 0.25 max 0.20 max 11.3–12.5 0.25 max 0.30 (d) max...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003772
EISBN: 978-1-62708-177-1
... Sn, 37 Zn Wrought bronzes C51000 Phosphor bronze, 5% A Bal Cu, 5.0 Sn, 0.2 P C52100 Phosphor bronze, 8% C Bal Cu, 8.0 Sn, 0.2 P C63000 Aluminum bronze, 10% 82.2 Cu, 10 Al, 3 Fe, 4.8 Ni C64700 Silicon-nickel bronze Bal Cu, 1.9 Ni, 0.6 Si C67500 Manganese bronze A 58.5 Cu...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005442
EISBN: 978-1-62708-196-2
... ksi 7.9 0.29  110 ksi 7.7 0.28 Aluminum bronze  Alloy 9A 7.8 0.28  Alloy 9B 7.55 0.272  Alloy 9C 7.5 0.27  Alloy 9D 7.7 0.28 Nickel silver  12% Ni 8.95 0.323  16% Ni 8.95 0.323  20% Ni 8.85 0.319  25% Ni 8.8 0.32 Silicon bronze 8.30 0.300...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006276
EISBN: 978-1-62708-169-6
... (brasses): contain up to 40% Zn Copper-tin alloys (phosphor bronzes): contain up to 10% Sn and 0.2% P Copper-aluminum alloys (aluminum bronzes): contain up to 13.5% Al Copper-silicon alloys (silicon bronzes): contain up to 3% Si Copper-nickel alloys: contain up to 30% Ni Copper...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003131
EISBN: 978-1-62708-199-3
... Aluminum bronzes C95200-C95810 Cu-Al-Fe-Ni Copper-nickels C96200-C96800 Cu-Ni-Fe Nickel silvers C97300-C97800 Cu-Ni-Zn-Pb-Sn Leaded coppers C98200-C98800 Cu-Pb Special alloys C99300-C99750 … Temper Designations Copper alloys are also described by their tempers, which...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006274
EISBN: 978-1-62708-169-6
... of wrought and cast aluminum alloys. The heat treatable aluminum alloys include: Aluminum-copper systems, with strengthening from coherent and transition precipitates prior to the formation of the equilibrium intermetallic CuAl 2 (in the 2 xxx and 2 xx.x alloy series) Al-Cu-Mg systems, in which...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001068
EISBN: 978-1-62708-162-7
... C95200 Aluminum bronze B 148-9A 88 … … … 3 9 … C95300 Aluminum bronze B 148-9B 89 … … … 1 10 … C95400 Aluminum bronze B 148-9C 85.5 … … … 4 10.5 … C95410 Aluminum bronze … 84 … … … 4 10 2 Ni C95500 Nickel-aluminum bronze B 148-9D 81 … … … 4 11 4 Ni...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003134
EISBN: 978-1-62708-199-3
... cast aluminum bronzes contain 9 to 14% Al and lesser amounts of iron, manganese, or nickel. They have a very narrow solidification range; therefore, they have a greater need for adequate gating and risering than do most other copper casting alloys and thus are more difficult to cast. A wide range...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005332
EISBN: 978-1-62708-187-0
..., and additional κ phases also form in this reaction. The phase diagrams of the aluminum bronze alloy systems are shown in Fig. 5 . Fig. 5 Phase diagrams of Cu-Al, Cu-Al-Fe, Cu-Al-Ni, and Cu-Al-Fe-Ni systems The κ phases, depending on the morphology and compositions, are identified as κ I , κ II , κ...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001065
EISBN: 978-1-62708-162-7
..., 8.0 Al R, W 483–552 70–80 207–379 30–55 65–25 20 C61300 92.65 Cu, 0.35 Sn, 7.0 Al F, R, T, P, S 483–586 70–85 207–400 30–58 42–35 30 C61400 (aluminum bronze, D) 91.0 Cu, 7.0 Al, 2.0 Fe F, R, W, T, P, S 524–614 76–89 228–414 33–60 45–32 20 C61500 90.0 Cu, 8.0 Al, 2.0 Ni...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001438
EISBN: 978-1-62708-173-3
...-aluminum alloys (aluminum bronzes) , which contain up to 10% Al Copper-silicon alloys (silicon bronzes) , which contain up to 3% Si Copper-nickel alloys , which contain up to 30% Ni Copper-zinc-nickel alloys (nickel silvers) , which contain up to 27% Zn and 18% Ni Special alloys , which...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006280
EISBN: 978-1-62708-169-6
... … C28000 Muntz metal, 60% 59.0–63.0 0.3 0.07 bal … Wrought leaded brasses C31200 … 87.5–90.5 0.7–1.2 0.1 bal 0.25 Ni C31400 Leaded commercial bronze 87.5–90.5 1.3–2.5 0.1 bal 0.7 Ni C31600 Leaded commercial bronze (nickel-bearing) 87.5–90.5 1.3–2.5 0.1 bal 0.7–1.2 Ni...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005644
EISBN: 978-1-62708-174-0
..., arc welding fair … … Welding not recommended at or above 9% Sn Silicon bronzes (Cu3%Si1%Mn) TIG, MIG, resistance Preheat 20–65 °C (70–150 °F) … Can be welded by arc, resistance methods. Avoid stressing joints. Filler as parent metal Aluminum bronzes (Cu-5%Al, Cu-10%Al, 5%Fe, 5%Ni) TIG...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003167
EISBN: 978-1-62708-199-3
... composition of aluminum-base bearing alloys Table 8 Designations and nominal composition of aluminum-base bearing alloys No. Designation Composition, % Product form Applications UNS SAE ISO Other Al Si Cu Ni Mg Sn Other High-tin alloys 1 A08081 Alloy 783 AlSn20Cu … 79...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005445
EISBN: 978-1-62708-196-2
...-Cr and Ni-Cr-Fe alloys 78.5Ni-20Cr-1.5Si (80-20) 1.6 108.05 73.5Ni-20Cr-5Al-1.5Si 1.2 137.97 68Ni-20Cr-8.5Fe-2Si 1.5 116.36 60Ni-16Cr-22.5Fe-1.5Si 1.5 112.20 35Ni-20Cr-43.5Fe-1.5Si 1.7 101.4 Fe-Cr-Al alloys 72Fe-23Cr-5Al 1.3 138.8 55Fe-37.5Cr-7.5Al 1.2 166.23...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003082
EISBN: 978-1-62708-199-3
... Admiralty brass 940 1720 Naval brass 900 1650 Phosphor bronze      5% Sn 1050 1920  10% Sn 1000 1830 Aluminum bronze, 7% Al, 2.5% Fe 1045 1915 High-silicon bronze, 3.3% Si 1025 1880 Copper-nickel      10% Ni 1150 2100  21% Ni 1150–1200 2100–2190  30% Ni...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002185
EISBN: 978-1-62708-188-7
... (a), low-carbon steel (b), and CA 104 aluminum bronze (10% Al, 5% Fe, 5% Ni) (c). The proximity of the high-temperature region to the cutting edge is the reason aluminum bronzes are considered difficult to machine. This problem can be offset by using cemented carbide tools of the appropriate composition...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006412
EISBN: 978-1-62708-192-4
... in the dark phase and copper-tin is present in the light phase. Original magnification: 50× Mixed Microstructures Mixed microstructures that combine the characteristics of types I and III are exhibited by Al-Si-Sn alloys and Al-Si-Pb alloys. In these alloys, the aluminum matrix contains both...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002411
EISBN: 978-1-62708-193-1
... composition, % C17200 1.9 Be, 0.25 Co C17410 0.3 Be, 0.4 Co C17510 0.4 Be, 1.8 Ni C26000 30 Zn C51000 5.0 Sn, 0.2 P C63800 2.8 Al, 1.8 Si, 0.4 Co C65400 3.1 Si, 1.6 Sn, 0.05 Cr C68800 23 Zn, 3.4 Al, 0.4 Co C72050 3.2 Ni, 0.75 Si, 0.2 Mg C72900 15 Ni, 8 Sn C76200...