1-2 of 2 Search Results for

Le Chatelier theorem

Sort by
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006221
EISBN: 978-1-62708-163-4
... coexist in equilibrium (three phases total in equilibrium) The iron-carbon system is the best example of a eutectoid system. Theorem of Le Châtelier and the Clausius-Clapeyron Equation Although the phase rule tells what lines and fields should be represented on a phase diagram, it does...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003085
EISBN: 978-1-62708-199-3
... of phases in adjacent fields in a multicomponent diagram must differ by one. Theorem of Le Châtelier The theorem of Henri Le Châtelier, which is based on thermodynamic principles, says that “if a system in equilibrium is subjected to a constraint by which the equilibrium is altered, a reaction...