... Abstract The aluminum alloy 7099 is a Kaiser aluminum high-strength Al-Mg-Zn-Cu alloy with zirconium that offers a less quench-sensitive alloy for properties in thicker sections for airframe structures such as wing ribs, spars, and skins, as well as fuselage frames and floor beams...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006713
EISBN: 978-1-62708-210-5
... composition free-machining heat treatment mechanical properties physical properties Alloys 6033, 6040 and 6041 ( Table 1 ) are free-machining alloys introduced by Kaiser Aluminum ( Ref 1 ). Alloy 6033 has significantly higher strength compared with alloys 6061 and 6262. The alloy contains higher Cu...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006723
EISBN: 978-1-62708-210-5
... requiring high strength and precise control of dimensional tolerances. References References 1. Kaiser Aluminum Alloy 6262: Heat Treatable Wrouhgt Aluminum Alloy , Alloy Digest: Data on Worldwide Metals and Alloys , Data Sheet Al-361, ASM International , Sept 1999 2. Aluminum 6262: Free...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006607
EISBN: 978-1-62708-210-5
... methods have been developed. References References 1. Alcoa 2124 Plate: Aerospace Aluminum Alloy , Alloy Digest: Data on Worldwide Metals and Alloys , Data Sheet Al-399, July 2006 2. Kaiser Aluminum Alloy 2124: Aluminum Aerospace Alloy , Alloy Digest: Data on Worldwide Metals...
Image
Published: 30 November 2018
electrolytic etch. Courtesy of Kaiser Aluminum More
Image
Published: 30 November 2018
, but there was less of it, and the critical grain size was smaller than for 2024 (see also Fig. 19 ). Barker’s electrolytic etch. Courtesy of Kaiser Aluminum More
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006569
EISBN: 978-1-62708-210-5
... – 2618 10.1007/s11661-999-0301-8 2. Granger D.A. , Sawtell R.R. , and Kersker M.M. , Effect of Beryllium on the Property of A357.0 Castings , AFS Transactions , Vol 92 , 1984 , p 579 – 586 3. Kaiser Aluminum Alloy 2024: Heat Treatable Wrought Aluminum Alloy , Alloy...
Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006740
EISBN: 978-1-62708-210-5
... effects on mechanical properties of alloy 7097-T7651 plate. aluminum alloy 7097 aluminum alloy plates aluminum-magnesium-zinc-copper-zirconium alloys corrosion resistance fracture toughness mechanical strength thick structural applications Alloy 7097 ( Table 1 ) from Kaiser Aluminum...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006733
EISBN: 978-1-62708-210-5
... Source: Ref 1 Reference Reference 1. Alcoa Aluminum Alloy 7050 : Heat Treatable Aluminum Alloy , Alloy Digest: Data on Worldwide Metals and Alloys , Data Sheet Al-233, ASM International , Jan 1990 2. Kaiser Aluminum Alloy 7050 : Heat Treatable Wrought Aluminum Alloy , Alloy...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001418
EISBN: 978-1-62708-173-3
... 5. Martukanitz R.P. and Michnuk P.R. , Sources of Porosity in Gas Metal Arc Welding of Aluminum , Trends in Welding Research , ASM International , 1982 , p 315 – 330 6. “Welding Kaiser Aluminum,” Kaiser Aluminum & Sales, Inc. , Oakland, CA , 1978 , p 3.25 – 3.26 ...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006726
EISBN: 978-1-62708-210-5
... of Kaiser Aluminum, Michael Niedzinski of Constellium, and Robert Sanders of Novelis for their assistance in collecting information for these datasheets. Reference Reference 1. Banhart J. , Age Hardening of Aluminum Alloys , Heat Treating of Nonferrous Alloys , Vol 4E , ASM Handbook...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006697
EISBN: 978-1-62708-210-5
... in the 1950s. Alloy 5083 is differentiated from alloy 5086 by the higher nominal magnesium and manganese contents ( Table 1 ). It was originally developed by Kaiser Aluminum for use in shipbuilding applications and has since become a standard across the aluminum industry. Equivalent designations include...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006732
EISBN: 978-1-62708-210-5
... not have a clear advantage compared with other alloys such as 7178 and 7050. In 1975, Kaiser introduced a lower Fe and Si version of the alloy as 7149. The alloy still sees some application and is still produced occasionally for forgings and extrusions. Physical properties of alloy 7049 are given...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006516
EISBN: 978-1-62708-210-5
... Abstract The development of aluminum alloys has progressed along two tracks: heat treatable and non-heat treatable. The Aluminum Association alloy composition limits and product temper are defined for major alloying elements. This article summarizes the historical evolution of the different...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006512
EISBN: 978-1-62708-207-5
.... Schering ( Ref 2 ) in Germany investigated acids with sulfonic groups that became the bases for the integral coloring processes. The use of sulfosalicylic acid with low concentrations of sulfuric acid and metal sulfates was developed by Kaiser Aluminum and commercialized as Kalcolor. The colors produced...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006595
EISBN: 978-1-62708-210-5
... without Pb emerged due to the environmental impact of Pb in industrial materials. Kaiser Alloy K211 ( Alloy Digest, Al-4566, Jan 2018) is a RoHS (restriction of hazardous substances) compliant rod and bar alloy with a controlled range of lead content (0.20–0.4 wt%). Alloy 2012 ( Table 1 ) substitutes tin...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001064
EISBN: 978-1-62708-162-7
... Scientists at Kaiser Aluminum & Chemical Corporation have also developed RS-P/M 7 xxx alloys ( Ref 43 ). The leading such alloy, 7064 (formerly called PM-64), is in parts strengthened by zirconium-, chromium-, and cobalt-containing dispersoids (see Table 1 ). It also displays attractive combinations...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006487
EISBN: 978-1-62708-207-5
... (see also Fig. 19 ). Barker’s electrolytic etch. Courtesy of Kaiser Aluminum Fig. 19 Effect of strain on recrystallization in alloy 2024 with 6 to 12% critical strain. 2024-O sheet was bent 180° and then solution heat treated. The bending resulted in residual cold work, and the thermal...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003996
EISBN: 978-1-62708-185-6
... Abstract This article begins with discussion on forgeability and the factors affecting the forgeability of aluminum and aluminum alloys. It describes the types of forging methods and equipment and reviews critical elements in the overall aluminum forging process: die materials, die design...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006737
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of 7075 series alloy. aluminum alloy 7075 fabrication characteristics mechanical properties physical properties Alloy...