1-20 of 75 Search Results for

Inconel 317

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005442
EISBN: 978-1-62708-196-2
... Nimonic 90 8.27 0.299 M-252 8.27 0.298 Inconel 8.51 0.307 Inconel “X” 550 8.30 0.300 Inconel 700 8.17 0.295 Inconel “713C” 7.913 0.2859 Waspaloy 8.23 0.296 René 41 8.27 0.298 Hastelloy alloy B 9.24 0.334 Hastelloy alloy C 8.94 0.323 Hastelloy alloy X 8.23...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006543
EISBN: 978-1-62708-183-2
... S64152 8.27 0.298 Inconel 600 N06600 8.41 0.304 Inconel “X” 550 … 8.30 0.300 Inconel 718 N07718 8.22 0.297 Inconel “713C” … 7.913 0.2859 Waspaloy N07001 8.23 0.296 René 41 N07041 8.27 0.298 Hastelloy alloy B N10001 9.24 0.334 Hastelloy alloy C N30002 8.94...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004218
EISBN: 978-1-62708-184-9
... of decreasing performance, was found to be as follows: Inconel alloy 600, Incoloy alloy 800, type 310 stainless steel, type 309 stainless steel, type 347 stainless steel, and type 304 stainless steel. Similar cyclic oxidation tests performed in air at 1150, 1205, and 1260 °C (2100, 2200, and 2300 °F), cycling...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001049
EISBN: 978-1-62708-161-0
... … … 0.3 … 1.0 0.5 0.4 … 0.009 … 0.05 La Hastelloy X 47.0 22.0 1.5 9.0 0.6 … … … 18.5 0.5 0.5 0.10 … … … Haynes 230 57.0 22.0 … 2.0 14.0 … 0.3 … … 0.5 0.4 0.10 … … 0.02 La Inconel 587 (a) bal 28.5 20.0 … … 0.7 1.2 2.3 … … … 0.05 0.003 0.05...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001361
EISBN: 978-1-62708-173-3
... be common low-carbon steel, stainless steel, or aluminum. Also used are medium-carbon steel, lead-free brass and copper, Inconel, titanium, René 41, zirconium, gold, silver, and platinum. Table 2 shows some of the more popular combinations of materials. Various studs and plate materials can be combined...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003203
EISBN: 978-1-62708-199-3
...) … 1175 2150 1 Incoloy 800 870 1600 1 1 2 980 1800 1 4 Incoloy 800H … … … 1175 2150 … Incoloy 825 … … … 980 1800 … Incoloy 901 (f) (f) … 1095 2000 2 Inconel 600 900 1650 1 1010 1850 1 4 (d) Inconel 601 … … … 980...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006265
EISBN: 978-1-62708-169-6
...), Inconel (Ni-Cr-Mo), Hastelloy (Ni-Mo-Cr), and Incoloy (Ni-Fe-Cr) families of alloys. The heat treatment processes for gamma prime nickel alloys, gamma prime nickel-iron superalloys, and gamma double-prime nickel-iron superalloys are also included. The article also provides information on age-hardenable...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003120
EISBN: 978-1-62708-199-3
... … … 0.35 3.0 max 0.10 0.015 max B, 0.02 La Inconel 600 N06600 15.5 76.0 … … … … … … 8.0 0.08 0.25 Cu Inconel 601 N06601 23.0 60.5 … … … … … 1.35 14.1 0.05 0.5 Cu Inconel 617 N06617 22.0 55.0 12.5 9.0 … … … 1.0 … 0.07 … Inconel 625 N06625 21.5 61.0...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002183
EISBN: 978-1-62708-188-7
... … 16.0 3.7 … … … 5.0 0.02 max … Hastelloy S … 15.5 67.0 … 15.5 … … … 0.2 1.0 0.02 max 0.02 La Hastelloy X N06002 22.0 49.0 1.5 max 9.0 0.6 … … 2.0 15.8 0.15 … Inconel 600 N06600 15.5 76.0 … … … … … … 8.0 0.08 0.25 max Cu Inconel 601 N06601 23.0...
Book Chapter

Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002141
EISBN: 978-1-62708-188-7
..., Inconel 617, Inconel 625, Inconel 700, Inconel 702, Inconel 706, Inconel 718, Inconel 721, Inconel 722, Inconel X-750, Inconel 751, M252, Nimonic 75, Nimonic 80, Nimonic 90, Nimonic 95, René 41, René 63, René 77, René 95, Udimet 500, Udimet 700, Udimet 710, Unitemp 1753, Waspaloy 200–390 HB Annealed...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001052
EISBN: 978-1-62708-161-0
... Inconel 713C 12 4.5 0 2.0 0 0 0 1956 Inconel 718 19 3 0 5.0 0 0 0 1960 TRW-NASA VIA 6.1 2 5.8 0.5 9 0 0.5 1968 René 150 5 1 5 0 6 2.2 3 1978 PWA 454 10 4 0 0 12 0 0 1980 (a) Approximate year of availability Fig. 2 Increased use...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004137
EISBN: 978-1-62708-184-9
...), then Incoloy 825, Inconel 625, Hastelloy G3, and alloy 904L (UNS N08904) or their equivalents are usually acceptable. Table 1 lists compositions of alloys commonly used in FGD systems. Compositions of some alloys used in flue gas desulfurization systems Table 1 Compositions of some alloys used in flue...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003082
EISBN: 978-1-62708-199-3
... 7.804 0.2819 17-4 PH 7.8 0.28 17-7 PH 7.81 0.282 Nickel-base alloys D-979 8.27 0.299 Nimonic 80A 8.25 0.298 Nimonic 90 8.27 0.299 M-252 8.27 0.298 Inconel 600 8.41 0.304 Inconel “X” 550 8.30 0.300 Inconel 718 8.22 0.297 Inconel “713C” 7.913 0.2859...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003664
EISBN: 978-1-62708-182-5
... 28-A) 120 0.043 (1.7) sheet, plate, and bar; 0.05 (2) pipe and tubing N06625 Inconel 625 None Ferric sulfate (G 28-A) 120 0.075 (3) N06690 Inconel 690 1 h at 540 °C (1000 °F) Nitric acid (A 262-C) 240 0.025 (1) N10276 Hastelloy C-276 None Ferric sulfate (G 28-A) 24 1 (40...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001046
EISBN: 978-1-62708-161-0
...–14.0 0.045 0.03 2.0–3.0 Mo 316LN S31653 0.03 2.00 1.00 16.0–18.0 10.0–14.0 0.045 0.03 2.0–3.0 Mo; 0.10–0.16 N 316N S31651 0.08 2.00 1.00 16.0–18.0 10.0–14.0 0.045 0.03 2.0–3.0 Mo; 0.10–0.16 N 317 S31700 0.08 2.00 1.00 18.0–20.0 11.0–15.0 0.045 0.03 3.0–4.0 Mo...
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005174
EISBN: 978-1-62708-186-3
... bronze 100–84 325–275 9.7–7.7 15–12 53–38 175–125 3.9–1.9 6–3  675, manganese bronze A 100–84 325–275 9.7–7.7 15–12 60–45 200–150 3.9–2.6 6–4 Nickel alloys  Inconel 30–18 100–60 1.9–1.3 3–2  Inconel X-750 24–18 80–60 1.0–0.3 1.5–0.5  Monel 400 30–18 100–60...
Book Chapter

By Ted A. Slezak
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002146
EISBN: 978-1-62708-188-7
... sawing superalloys such as Inconel 718, Waspaloy, Astroloy, and 6/4 alloy titanium in large sizes, improved efficiency may be achieved by using carbide-tip band blades. Special welded-edge blades are also available for these applications. They utilize changing width patterns to force the teeth to cut...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003192
EISBN: 978-1-62708-199-3
... 0.625 75 0.030 M2, M3 275 310 0.040 C-6 … … … Austenitic steels 201, 202, 301, 302, 302B, 304, 304L, 305, 308, 309, 309S, 310, 310S, 314, 316, 316L, 317, 321, 330, 347, 348, 384, 385 135–185 Annealed 0.040 95 0.007 M2, M3 325 375 0.007 C-3 500 0.007 CC-3 0.150 75...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003812
EISBN: 978-1-62708-183-2
... 0.10N S31603 316L 0.030 2.00 0.045 0.030 0.75 16.0–18.0 10.0–14.0 2.00–3.00 0.10N S31651 316N 0.08 2.00 0.045 0.030 0.75 16.0–18.0 10.0–14.0 2.00–3.00 0.10–0.16N S31700 317 0.08 2.00 0.045 0.030 0.75 18.0–20.0 11.0–15.0 3.0–4.0 0.10N S31703 317L 0.030 2.00...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002420
EISBN: 978-1-62708-193-1
...) Beryllium Inconel X A-286 aged A-286 34% cold reduced and aged D-979 Source: Ref 2 Fig. 2 Fracture stress versus tensile ductility. Source: Ref 5 Graphical Solution by Manson On the basis of the approximate equality in Eq 8 , Manson noted that when E is known, only...