Published: 01 January 1993
Fig. 1 Photomicrographs showing corrosion attack in Hastelloy C-276 (UNS N10276) caused by grain boundary precipitation in the heat-affected zone of the weld. The sample was taken from a pipe removed after 18 months of service in a hydrochloric acid vapor environment in a chemical plant More
Image
Published: 01 June 2016
Fig. 17 Hastelloy C-276 time-temperature precipitation corrosion diagram. Solution annealed at 1125 °C (2045 °F). Nominal composition: Ni-16%Cr-3.4%W-6%Fe-0.01%C-0.02%Si-1%Co-0.45%Mn-0.2%V-16%Mo More
Image
Published: 01 January 1990
Fig. 4 Galling data of various cobalt-base alloys, Hastelloy C-276, and Nitronic-60 stainless steel. Data are from a 120°-10 stroke test with a 26.7 kN (6000 lbf) load. More
Image
Published: 01 January 1993
Fig. 1 Solidification crack in a pulsed Nd:YAG laser weld joining Hastelloy C-276 to 17-4 PH stainless steel. YAG, yttrium-aluminum-garnet More
Image
Published: 01 January 2003
Fig. 8 Time-temperature transformation curves for Hastelloy alloys C and C-276. Intermetallics and carbide phases precipitate in the regions to the right of the curves. Source: Ref 9 More
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003623
EISBN: 978-1-62708-182-5
... are rich in molybdenum, tungsten, and chromium and therefore create adjacent areas of alloy depletion that can be selectively attacked. Carbide precipitation can be retarded considerably by lowering carbon and silicon; this is the principle behind Hastelloy alloy C-276. The time- temperature behaviors...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003664
EISBN: 978-1-62708-182-5
... with the material. However, such confidence may be misplaced. For example, there have been a number of accounts in which alloys have been substituted, resulting in premature failure. In one case, this occurred when Hastelloy B (UNS N10001) valves were substituted for the Hastelloy C-276 (UNS N10276) valves...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001429
EISBN: 978-1-62708-173-3
... precipitation in the heat-affected zone ( Fig. 1 ). Fig. 1 Photomicrographs showing corrosion attack in Hastelloy C-276 (UNS N10276) caused by grain boundary precipitation in the heat-affected zone of the weld. The sample was taken from a pipe removed after 18 months of service in a hydrochloric acid...
Image
Published: 01 January 2003
Fig. 12 Corrosion of the weld metal and the HAZ in Hastelloy alloys (a) C-22 and (b) C-276 in an aerated mixture of 6 vol% H 2 SO 4 + 3.9% Fe 2 (SO 4 ) 3 + other chemicals at 150 °C (300 °F). Source: Ref 11 More
Image
Published: 01 January 1990
Fig. 5 Cavitation erosion data on various cobalt-base alloys, Hastelloy alloy C-276, and 316L stainless steel More
Image
Published: 01 December 1998
Fig. 2 Cavitation erosion data on various cobalt-base alloys, Hastelloy alloy C-276, and 316L stainless steel More
Image
Published: 01 January 2003
Fig. 10 Typical microstructure of the HAZ of a multipass submerged arc weld in Hastelloy alloy C-276. Source: Ref 11 More
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003619
EISBN: 978-1-62708-182-5
... … 1.2 … … Nickel-molybdenum alloys N10665 Hastelloy B-2 72 … … 28 … … … N10675 Hastelloy B-3 68.5 1.5 … 28.5 1.5 … … Nickel-chromium-molybdenum alloys N10276 Hastelloy C-276 59 16 … 16 5 4 … N06455 Hastelloy C-4 68 16 … 16 … … … N06022...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001073
EISBN: 978-1-62708-162-7
... data of various cobalt-base alloys tested per ASTM G 65B Galling Data Galling data (under self-mated conditions) are presented for five of the popular alloys in Fig. 4 , along with data for corrosion-resistant Ni-Cr-Mo alloy (Hastelloy alloy C-276) and stainless steel noted for its resistant...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003834
EISBN: 978-1-62708-183-2
... to localized corrosion can be selected. In seawater service, type 304 stainless steel that is clad to a thin layer of Hastelloy C-276 (UNS N10276) provides a substitute for solid Hastelloy C-276. In this corrosion barrier system, localized corrosion of the type 304 stainless steel is arrested at the C-276...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003147
EISBN: 978-1-62708-199-3
... 12.5–14.5 2.5–3.5 … … … 0.015 0.5 0.08 … 0.35 V Alloy C-276 N10276 bal 14.5–16.50 4.0–7.0 2.5 15.0–17.0 3.0–4.5 … … … 0.02 1.0 0.08 … 0.35 V Alloy G N06007 bal 21.0–23.5 18.0–21.0 2.5 5.5–7.5 1.0 1.75–2.5 … … 0.05 1.0–2.0 1.0 … … Alloy G-2 N06975 47.0...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006261
EISBN: 978-1-62708-169-6
... N10276 Alloy C-276 Ni-15.5Cr-16Mo-5.5Fe-3.75W-1.25Co + V Wrought 785 114 372 54 62 209 HB N06625 Alloy 625 Ni-21.5Cr-9Mo-3.65Nb + Ta-2.5Fe Wrought 930 135 517 75 42.5 190 HB N06035 Hastelloy G-35 Ni-33Cr-8Mo-2Fe(max) Wrought 586 85 241 35 30 … N06022 Hastelloy C-22...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006265
EISBN: 978-1-62708-169-6
... 1095–1175 2000–2150 5–10 AC or WQ 1095–1175 2000–2150 1 AC or WQ Hastelloy C-276 1215 2220 5–10 WQ 1215 2220 1 WQ Hastelloy X 1175 2150 1 2 –15 AC or WQ 1175 2150 1 AC or WQ (a) Processing times are shown in minutes. The time should be sufficient to assure...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002473
EISBN: 978-1-62708-194-8
... 0 … RA-333 −12.35 32 45.2 3 18 25 0 0 3 3 0 0 … MAR-M-200 −14.23 33 58.6 10 0 9 5 2 0 12.5 2.7 0 … IN-706 −19.74 37 77.5 1 0 16 0.4 1.8 0 0 2.9 0 … IN-600 −29.33 39 76.5 0 7.2 15.8 0 0 0 0 0 0 … Hastelloy C-276 −34.36 40 55.4...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003148
EISBN: 978-1-62708-199-3
... C-276 and 316L stainless steel are illustrated in Fig. 2 . This information was generated using ASTM G 32 procedures. The samples were prepared from solution-annealed plates (in the case of Haynes alloy 6B, Hastelloy alloy C-276, and 316L stainless steel) or from two-layer GTA deposits (in the case...