1-20 of 53 Search Results for

Hastelloy

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006265
EISBN: 978-1-62708-169-6
...), Inconel (Ni-Cr-Mo), Hastelloy (Ni-Mo-Cr), and Incoloy (Ni-Fe-Cr) families of alloys. The heat treatment processes for gamma prime nickel alloys, gamma prime nickel-iron superalloys, and gamma double-prime nickel-iron superalloys are also included. The article also provides information on age-hardenable...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005443
EISBN: 978-1-62708-196-2
..., AZ80A 20 to 100 26 ZK60A, B 20 to 100 26 HM31A 20 to 93 26.1 Nickel and nickel alloys Nickel (99.95% Ni + Co) 0 to 100 13.3 Duranickel 0 to 100 13.0 Monel 0 to 100 14.0 Monel (cast) 25 to 100 12.9 Inconel 20 to 100 11.5 Ni-o-nel 27 to 93 12.9 Hastelloy B...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005442
EISBN: 978-1-62708-196-2
... Nimonic 90 8.27 0.299 M-252 8.27 0.298 Inconel 8.51 0.307 Inconel “X” 550 8.30 0.300 Inconel 700 8.17 0.295 Inconel “713C” 7.913 0.2859 Waspaloy 8.23 0.296 René 41 8.27 0.298 Hastelloy alloy B 9.24 0.334 Hastelloy alloy C 8.94 0.323 Hastelloy alloy X 8.23...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005444
EISBN: 978-1-62708-196-2
... Inconel 0.036 Hastelloy B 0.027 Hastelloy C 0.03 Hastelloy D 0.05 Illium G 0.029 Illium R 0.031 60Ni-24Fe-16Cr 0.032 35Ni-45Fe-20Cr 0.031 Constantan 0.051 Tin and tin alloys Pure tin 0.15 Soft solder (63Sn-37Pb) 0.12 Tin foil (92Sn-8Zn) 0.14 Titanium...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006543
EISBN: 978-1-62708-183-2
... 0.298 Inconel 600 N06600 8.41 0.304 Inconel “X” 550 … 8.30 0.300 Inconel 718 N07718 8.22 0.297 Inconel “713C” … 7.913 0.2859 Waspaloy N07001 8.23 0.296 René 41 N07041 8.27 0.298 Hastelloy alloy B N10001 9.24 0.334 Hastelloy alloy C N30002 8.94 0.323...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003082
EISBN: 978-1-62708-199-3
... René 41 8.27 0.298 Hastelloy alloy B 9.24 0.334 Hastelloy alloy C 8.94 0.323 Hastelloy alloy X 8.23 0.297 Udimet 500 8.07 0.291 GMR-235 8.03 0.290 CMSX-2 8.56 0.309 PWA 1484 8.95 0.323 Cobalt-chromium-nickel-base alloys N-155 (HS-95) 8.23 0.296 S-590...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003147
EISBN: 978-1-62708-199-3
... 0.03 … … M-30C … 0.30 1.0–2.0 1.50 26.0–33.0 3.50 max … 0.03 0.03 … 1.0–3.0 Nb Nickel-chromium-iron CY-40 Inconel 600 0.40 3.0 1.5 … 11.0 max 14.0–17.0 0.03 0.03 … … Nickel-chromium-molybdenum CW-12MW Hastelloy C 0.12 1.0 1.0 … 4.5–7.5 15.5–17.5 0.04...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003999
EISBN: 978-1-62708-185-6
... … 0.1Si GH4133 20.5 bal … … … 1.4 2.75 0.95 … <0.07 … … Hastelloy B 1 bal 2.5 29.5 … … … … 6 0.12 … … Hastelloy C 15.5 bal 2.5 16 3.75 … … … 5.5 0.08 … 0.35V Hastelloy S 21 bal … 15.3 3.7 … 0.2 … 3 0.02 0.015 0.35Cu Haynes 214 16 bal 2...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003203
EISBN: 978-1-62708-199-3
...-286 (f) (f) … 980 1800 1 Discaloy (f) (f) … 1035 1900 1 Nickel-base alloys Astroloy (f) (f) … 1135 2075 4 Hastelloy B (f) (f) … 1175 2150 1 Hastelloy C (f) (f) … 1215 2225 1 Hastelloy W (f) (f) … 1175 2150 1 Hastelloy X...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006261
EISBN: 978-1-62708-169-6
... commercially significant nickel alloys was alloy 400, developed by the International Nickel Company (now Inco) ( Ref 1 , 2 ). This was marketed in 1905 under the Monel trademark. Some 15 years later, Haynes Stellite Co. introduced alloy B and alloy C under the trademark Hastelloy. The next significant nickel...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006266
EISBN: 978-1-62708-169-6
... superalloys. Solid-solution- and carbide-hardened superalloys such as Hastelloy X or the cobalt-base superalloys generally have minimal unique aspects with respect to heat treatment, other than melting-point constraints. Various heat treatment temperatures and times have been tried, but significant property...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003148
EISBN: 978-1-62708-199-3
... various cobalt-base alloys tested per ASTM G 65B The outstanding cavitation erosion properties of the cobalt-base wear alloys as compared with Hastelloy alloy C-276 and 316L stainless steel are illustrated in Fig. 2 . This information was generated using ASTM G 32 procedures. The samples were...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003120
EISBN: 978-1-62708-199-3
... … RA 333 N06333 25.0 45.0 3.0 3.0 3.0 … … … 18.0 0.05 … Hastelloy B N10001 1.0 max 63.0 2.5 max 28.0 … … … … 5.0 0.05 max 0.03 V Hastelloy N N10003 7.0 72.0 … 16.0 … … 0.5 max … 5.0 max 0.06 Hastelloy S N06635 15.5 67.0 … 15.5 … … … 0.2 1.0 0.02...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003834
EISBN: 978-1-62708-183-2
... localized corrosion can be selected. In seawater service, type 304 stainless steel that is clad to a thin layer of Hastelloy C-276 (UNS N10276) provides a substitute for solid Hastelloy C-276. In this corrosion barrier system, localized corrosion of the type 304 stainless steel is arrested at the C-276...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
... weld may be anodic to the wrought parent metals. The combination of their passive surface with their inherent resistance places nickel-chromium alloys such as Inconel alloy 600 and Hastelloy alloy C-276 in more noble positions in the traditional galvanic series. In chloride-bearing solutions...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003993
EISBN: 978-1-62708-185-6
...) N09901 PH 42.5 12.5 … 36.2 6.0 … … 2.7 … 0.10 max … Alloy R-235 (Hastelloy R235) … PH bal 16 1.9 10 5.5 … … 2.5 2.0 0.10 Trace B Alloy W (Hastelloy W) N10004 SS 61 5.0 2.5 max 5.5 24.5 … … … … 0.12 max 0.6 V Alloy X (Hastelloy X) N06002 SS 49 22 1.5 max...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0005586
EISBN: 978-1-62708-170-2
... Corporation Inconel, Incoloy, and Nimonic are trademarks of Inco Alloys International, Inc. Haynes and Hastelloy are trademarks of Haynes International, Inc. Scotch-Brite and Scotch-Weld are trademarks of 3M Company Super D-Gun is a tradename of Praxair Surface Technologies, Inc...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003158
EISBN: 978-1-62708-199-3
..., nickel-base alloys (Hastelloy X and Inconel 600 and 702), and tantalum and niobium alloys. Depending on temperature and application, magnesia, alumina, beryllia, or thoria can be used for the insulation. The type J thermocouple is widely used, primarily because of its versatility and low cost. In...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.9781627081610
EISBN: 978-1-62708-161-0
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.9781627081733
EISBN: 978-1-62708-173-3