... 9.5 1.4 HF Excellent general corrosion resistance to 815 °C (1500 °F) with moderate mechanical properties 870 1600 27 3.9 HH (a) High strength; oxidation resistant to 1090 °C (2000 °F); most widely used 980 1800 7.5 (type I) 14.5 (type II) 1.1 (type I) 2.1 (type II) H1 Improved...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003118
EISBN: 978-1-62708-199-3
... No. Composition (b) , % C Cr Ni Si (max) … HA … 0.20 max 8–10 … 1.00 446 HC J92605 0.50 max 26–30 4 max 2.00 327 HD J93005 0.50 max 26–30 4–7 2.00 312 HE J93403 0.20–0.50 26–30 8–11 2.00 302B HF J92603 0.20–0.40 19–23 9–2 2.00 309 HH J93503 0.20–0.50 24...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003198
EISBN: 978-1-62708-199-3
... belts, wrought Chain link Sprockets, rolls, guides, trays Wrought Cast Wrought Cast Wrought Cast 595–675 °C (1100–1250 °F) 430 304 HF 430 304 430 304 HF 430 304 HF 675–760 °C (1250–1400 °F) 304 347 309 HF HH 309 309 HF HH 304 316 309 HF HH 760–925 °C (1400...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002433
EISBN: 978-1-62708-194-8
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001461
EISBN: 978-1-62708-173-3
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005930
EISBN: 978-1-62708-166-5
... 6.1 28 4.0 870 1600 27 3.9 19 2.7 12 1.7 980 1800 … … … … … … HH J93503 0.20–0.50 24–28 11–14 650 1200 124 18.0 97 14.0 62 9.0 760 1400 43 6.3 33 4.8 19 2.8 870 1600 27 3.9 15 2.2 8 1.2 980 1800 14 2.1 6 0.9 3 0.4 HK J94224 0.20...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005329
EISBN: 978-1-62708-187-0
... 0.04 0.04 26–30 8–11 0.5 (c) HF 302B 0.20–0.40 2.00 2.00 0.04 0.04 18–23 8–12 0.5 (c) HH 309 0.20–0.50 2.00 2.00 0.04 0.04 24–28 11–14 0.5 (c) HI … 0.20–0.50 2.00 2.00 0.04 0.04 26–30 14–18 0.5 (c) HK 310 0.20–0.60 2.00 2.00 0.04 0.04 24–28 18–22...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005445
EISBN: 978-1-62708-196-2
... 78% Ni 11 16 77% Ni (Cu, Cr) 3 60 79% Ni (Mo) 3 58 Stainless and heat-resisting alloys Type 302 3 72 Type 309 2.5 78 Type 316 2.5 74 Type 317 2.5 74 Type 347 2.5 73 Type 403 3 57 Type 405 3 60 Type 501 4.5 40 HH 2.5 80 HK 2 90 HT...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003001
EISBN: 978-1-62708-200-6
...) 17.4 (gg) … 4.524 (y) 4.523 (y) 7.661 (y) 2.437 Germanium (Ge) 32 72.60 5.32 (0.192) 937.4 ± 1.5 (1719.3 ± 2.7) 2830 (5125) 0.073 (310) … (…) Ge 5.75 (3.19) 0.14 46 (hh) … 5.658 … … 2.449 Gold (Au) 79 197.0 19.3 (0.697) 1063.0 ± 0.0 (1945.4 ± 0.0) 2970 (5380...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005441
EISBN: 978-1-62708-196-2
... 16.75 0.014 0.047 32 (9.3) (200) (58) Tb 7 … 0.044 24.54 (3.88) (180) (44.17) Tl 28 0.093 0.031 5.04 (16) (130) (9.07) Th 12.5 (hh) 0.090 (ii) 0.034 <19.82 (6.9) (hh) (140) (<35.68) Tm … … 0.038 26.04 (…) (160) (46.87) Sn 23 (jj...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001413
EISBN: 978-1-62708-173-3
... Cr Ni Si (max) HA … A217 0.20 max 8–10 … 1.00 HC J92605 A 297, A 608 0.50 max 26–30 4 max 2.00 HD J93005 A 297, A 608 0.50 max 26–30 4–7 2.00 HE J93403 A 297, A 608 0.20–0.50 26–30 8–11 2.00 HF J92603 A 297, A 608 0.20–0.40 19–23 9–12 2.00 HH...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006624
EISBN: 978-1-62708-210-5
... A95657 Nominal … … … … 0.8 … … … … … … … … Limits 0.08 0.1 0.1 0.03 0.6–1.0 … … 0.05 … 0.02 0.05 bal (hh) 5754 A95754 Nominal … … … 0.20(ii) 3.1 0.15 … … … … … … (ii) Limits 0.4 0.4 0.1 0.50(ii) 2.6–3.6 0.3 … 0.2 0.15 0.05 0.15 bal (ii...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005442
EISBN: 978-1-62708-196-2
... CK-20 7.75 0.280 CN-7M 8.00 0.289 Heat-resistant alloy castings HA 7.72 0.279 HC 7.53 0.272 HD 7.58 0.274 HE 7.67 0.277 HF 7.75 0.280 HH 7.72 0.279 HI 7.72 0.279 HK 7.75 0.280 HL 7.72 0.279 HN 7.83 0.283 HT 7.92 0.286 HU 8.04...
Book Chapter

By Volker Heuer
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005770
EISBN: 978-1-62708-165-8
... determined in the tooth root of gear shafts for a 20 bar He and a 10 bar N 2 quench. Again, the hardenability curves of typical HH steel qualities are displayed. After determination of the local Jominy value of the component, it can be predicted what tooth-root core hardness values can be achieved when...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006543
EISBN: 978-1-62708-183-2
... J94202 7.75 0.280 CN-7M N08007 8.00 0.289 Heat-resistant alloy castings HA … 7.72 0.279 HC J92605 7.53 0.272 HD J93005 7.58 0.274 HE J93403 7.67 0.277 HF J92603 7.75 0.280 HH J93503 7.72 0.279 HI J94003 7.72 0.279 HK J94224 7.75 0.280 HL...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003082
EISBN: 978-1-62708-199-3
... 0.280 HH 7.72 0.279 HI 7.72 0.279 HK 7.75 0.280 HL 7.72 0.279 HN 7.83 0.283 HT 7.92 0.286 HU 8.04 0.290 HW 8.14 0.294 HX 8.14 0.294 Wrought stainless and heat-resistant steels Type 301 7.9 0.29 Type 302 7.9 0.29 Type 302B 8.0 0.29 Type...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003748
EISBN: 978-1-62708-177-1
... mL H 2 SO 4 310 g sodium dichromate, 96 mL acetic acid (glacial) Zinc … … (gg) VI-15 260 mL H 2 O 2 (30%), 240 mL HF, 500 mL H 2 SO 4 Stainless steel … 5 min (hh) VI-16 520 mL H 2 O, 80 mL HF, 400 mL H 2 SO 4 Stainless steel … 1 2 –4 min (jj) VI-17 600 mL H...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.9781627081665
EISBN: 978-1-62708-166-5
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003737
EISBN: 978-1-62708-177-1
... 18.0–23.0 8.0–12.0 0.50 HH 25 chromium, 12 nickel 0.20–0.50 2.00 2.00 0.04 0.04 24.0–28.0 11.0–14.0 0.50 HI 28 chromium, 15 nickel 0.20–0.50 2.00 2.00 0.04 0.04 26.0–30.0 14.0–18.0 0.50 HK 25 chromium, 20 nickel 0.20–0.60 2.00 2.00 0.04 0.04 24.0–28.0 18.0–22.0...
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009016
EISBN: 978-1-62708-187-0
...-base rules. Multipliers for high-alloy steel castings have been developed for steel alloys CF-8M, CA-15, HH, HK, and HP ( Ref 18 ). In other alloys, such as 88-10-2 bronze, 85-5-5-5 bronze, Al- 8Mg, and Al-4.5Cu, the centerline feeding resistance is so great that FD is virtually nonexistent unless...