Published: 01 December 2004
Fig. 68 Ferrite (dark) and austenite in alloy 255 (Ferralium) duplex stainless steel etched with aqueous 20% NaOH at 3 V dc for 3 s More
Image
Published: 01 January 2003
Fig. 43 Preferential corrosion of the ferrite phase in the weld metal of Ferralium alloy 255 gas tungsten arc welds in 10% FeCl 3 at room temperature. Base metal was 3.2 mm ( 1 8 in.) thick. More
Image
Published: 01 January 2006
Fig. 5 Isocorrosion diagram for a duplex stainless steel, Ferralium alloy 255, in H 2 SO 4 +HCl mixtures at 52 °C (125 °F). Data point values and contour lines are corrosion rate in mils/yr. More
Image
Published: 01 January 2003
Fig. 42 Effect of welding heat input on the corrosion resistance of autogenous gas tungsten arc welds in Ferralium alloy 255 in 10% FeCl 3 at 10 °C (40 °F). The base metal was 25 mm (1 in.) thick. Source: Ref 16 More
Image
Published: 01 January 2003
Fig. 44 Preferential attack of the continuous austenite phase in an autogenous gas tungsten arc weld in Ferralium alloy 255. Crevice corrosion test was performed in synthetic seawater according to ASTM D 1141 ( Ref 17 ) at 100 °C (212 °F). Etched with 50% HNO 3 . 100× More
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003622
EISBN: 978-1-62708-182-5
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004187
EISBN: 978-1-62708-184-9
... Others … 27-7Mo 27 22 42 7.2 … 1 … … … … 0.34N S34700 347 11 18 69 … … … 0.08 0.5 … … 2Mn S32550 Ferralium 255 5.5 25 64 3 … 1.7 … … … … 0.17N S32100 321 10.5 18 69 … … … 0.08 … 0.3 … 2Mn S31603 316L 12 17 65 2.5 … … 0.03...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003676
EISBN: 978-1-62708-182-5
...–26.0 5.5–8.0 3.0–5.0 0.5–3.00 Cu, 0.20–0.35 N 42.6 S32550 Ferralium 255 0.04 1.5 0.04 0.03 1.00 24.0–27.0 4.50–6.50 2.00–4.00 1.5–2.5 Cu, 0.1–0.25 N 38.28 S32750 SAF 2507 0.03 1.2 0.035 0.02 0.80 24.0–26.0 6.0–8.0 3.0–5.0 0.24–0.32 N 42.68 S32760 (c) Zeron 100 0.03...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0005549
EISBN: 978-1-62708-162-7
... of Sinter- E, E epsilon metallwerk Krebsoge GmbH. Z, t zeta DP3 is a registered tradename of Sumitomo Metal America, Inc. H, T) eta Elinvar and Invar are registered tradenames e,6 theta of Imphy, S.A. I, t iota Esshete is a registered tradename of British Steel Corporation. Ferralium is a registered...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001482
EISBN: 978-1-62708-173-3
... coherent light wave trains. Masubuchi et al. ( Ref 59 ) measured out-of-plane displacement using laser interferometer. Chavez et al. ( Ref 60 ) used Moire interferometry to obtain full-field strain data across welds in stainless steel plates with Ferralium or nickel filler. Moire interferometry...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003117
EISBN: 978-1-62708-199-3
... 7-Mo PLUS 15 60 S31803 2205 17.5 63.5 S32250 Ferralium 255 22.5 72.5 Austenitic grades S30400 Type 304 <−2.5 <27.5 S31600 Type 316 −2.5 27.5 S31703 Type 317L 0 32 N08020 20Cb-3 0 32 N08366 AL-6N 17.5 63.5 N08367 AL-6XN 32.5 90.5...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003203
EISBN: 978-1-62708-199-3
... ferritic alloys. Duplex stainless steels, such as SAF 2205, AF 22, DP 3, and Ferralium alloy 255, are alloyed with 0.15 to 0.20% N. This minimizes alloy element segregation between the ferrite and austenite, thereby improving as-welded corrosion resistance to a level greater than that of type 329 alloy...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001047
EISBN: 978-1-62708-161-0
... . Fig. 5 Yield strength and tensile strength versus percentage of ferrite for CF-8 and CF-8M alloys. Curves are mean values for 277 heats of CF-8 and 62 heats of CF-8M. Source: Ref 3 Other duplex alloys of interest include CD-4MCu and Ferralium. Alloy CD-4MCu is the most highly alloyed duplex...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003812
EISBN: 978-1-62708-183-2
... 2.00 0.030 0.020 1.00 21.0–23.0 4.5–6.5 2.5–3.5 0.014–0.2N S32304 2304 0.030 2.50 0.040 0.030 1.0 21.5–24.5 3.0–5.5 0.05–0.60 0.05–0.60Cu, 0.05–0.20N S32550 Ferralium 255 0.04 1.50 0.040 0.030 1.00 24.0–27.0 4.5–6.5 2.9–3.9 1.50–2.50Cu, 0.10–0.25N S32750 SAF 2507...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003767
EISBN: 978-1-62708-177-1
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004204
EISBN: 978-1-62708-184-9
... to hydrogen embrittlement, shielding gases containing hydrogen should not be used. Duplex alloys include alloy 2205 (UNS S31803), 44LN (UNS S31200), and Ferralium 255 (UNS S32550). High-Purity Ferritic Stainless Steels High-purity ferritic stainless steels were introduced in the United States...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001411
EISBN: 978-1-62708-173-3
... 0.16 0.2 … 38 S31260 CLI UR 52N 25 7 3.0 0.16 1.5 … 38 S32550 Langley Alloys Ferralium 255 26 5.5 3.3 0.17 2.0 … 39 S32550 Mather and Platt Zeron 25 25 4 2.5 0.15 … … 36 … Sumitomo DP-3 25 6.5 3.0 0.2 0.5 0.3 W 38 … Fe-25Cr-7Ni-3.5Mo-0.25N-Cu-W...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001046
EISBN: 978-1-62708-161-0
... 2.00 1.00 21.0–23.0 4.50–6.50 0.030 0.020 2.50–3.50 Mo; 0.08–0.20 N 2304 S32304 0.030 2.50 1.0 21.5–24.5 3.0–5.5 0.040 0.040 0.05–0.60 Mo; 0.05–0.60 Cu; 0.05–0.20 N Uranus 50 S32404 0.04 2.00 1.0 20.5–22.5 5.5–8.5 0.030 0.010 2.0–3.0 Mo; 1.0–2.0 Cu; 0.20 N Ferralium 255...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005990
EISBN: 978-1-62708-168-9
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002405
EISBN: 978-1-62708-193-1
...) UNS S31803 WNr 1.4462 NFA 36209 Z3CND2205AZ UR45N SAF 2205 AVESTA 2205 REMANIT 4462 22 5 2.7 0.14 … 33 UR 45N+ 23 6.2 3.2 0.19 36 Superduplex (d) UNS S32760 ZERON 100 25 7 3.6 0.24 0.7 Cu, 0.7 W 41 UNS S32550 Z3 CNDU 2506 UR 52 N+ FERRALIUM SD40 25 6.5 3.8 0.26...