1-20 of 420 Search Results for

EN 25

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 January 2005
Fig. 25 Effects of (a) maximum and (b) minimum temperatures on the fatigue life of En 25 mild steel. Source: Ref 2 More
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006719
EISBN: 978-1-62708-210-5
...) Mechanical properties for standard tempers are similar to those listed in BS EN 755-2, 1997. Minimum properties can vary slightly depending on specification and product form. Data are provided for reference only. (a) The thickness of the cross section from which the tension test specimen is taken...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006598
EISBN: 978-1-62708-210-5
... in Table 6 , and tensile property minimums are listed in Tables 7 and 8 . Available product tempers include: Products Tempers Sheet (bare and clad) O, T3, T361, T4, T81, T861, and T351 sheet tempers in AMS 4033, 4034, 4037 and EN 3999, 4001 Plate (bare and clad) O, T3, T361, T4, T81...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0006000
EISBN: 978-1-62708-168-9
... 1095 304 S 25 304 640 M 40 3140 En. 47 6150 304 S 40 304 708 A 37 4135 En. 47 6150H 310 S 24 310 708 A 37 4135H En. 56 A 410 310 S 24 314 708 A 42 4137 En. 56 B 403 316 S 12 316L 708 A 42 4137H En. 58 B 321 316 S 14 316L 708 A 42 4140 En. 58 C 321 316...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006325
EISBN: 978-1-62708-179-5
... 18 130–175 30 27 Ferrite EN-GJS-500-7 500 73 320 46 7 170–230 25 23 Ferrite + pearlite EN-GJS-800-2 800 116 482 70 2 245–335 14 13 Pearlite or tempered martensite In the European designation system (EN 1560 and 1563), ductile cast irons are given the prefix “EN-GJS...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006686
EISBN: 978-1-62708-210-5
... in Table 6 . Alloy 3003 products specifications Table 5 Alloy 3003 products specifications Product ASTM ISO EN JIS AMS ASME Federal Military Sheet and plate B 209 ISO 6361 EN 485-1 H 4000 4006, 4008 SB 209 QQ-A-250/2 … Wire, rod, and bar: rolled, drawn or cold finished...
Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006727
EISBN: 978-1-62708-210-5
... quenching. Product specifications include: Specification number Product form ISO 6362 Extruded rods/bars, tubes, and profiles EN 755 Extruded rod/bar, tube, and profiles JIS H 4040 Bars and wire JIS H 4080 Extruded tubes and cold-drawn tubes JIS H 4100 Extruded profiles...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006592
EISBN: 978-1-62708-210-5
... ASTM ISO EN JIS Government Sheet and plate 4001, 4003 SB209 B 209 ISO-6361 EN-485 H 4000 QQ-A-250/1 Wire, rod, and bar (drawn, rolled or cold finished) 4102 … B 211 ISO-6363 … H 4040 QQ-A-225/1 Wire, rod, bar, shapes, and tube (extruded) … SB221 B 221 ISO 6362 EN 755...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006591
EISBN: 978-1-62708-210-5
... grades of aluminum including the 1050A European grade (WS 3.0255, EN AW- Al99). Aluminum 1060 typical physical properties Table 2 Aluminum 1060 typical physical properties Property Value Poisson’s ratio at 20 °C (68 °F) 0.33 Elastic modulus at 20 °C (68 °F) 69 GPa (10 × 10 6 psi...
Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006706
EISBN: 978-1-62708-210-5
... demanding applications in the watch or automotive industries. Properties of alloy 5754 are given in Tables 2 and 3 . Specification equivalents include: Designation AlMg3 EN 3.3535 in EN 485-2 ASTM B 209 Alloy 5754 composition limits Table 1 Alloy 5754 composition limits Element...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006593
EISBN: 978-1-62708-210-5
... workability. Alloy 1350 is the most common electrical conductor alloy used in the industry today. Equivalent designations include: UNS: A91350 European: WS 3.0257, EN AW- Al99.5(A) France: NF A5/L Spain: UNE AL99.5E United Kingdom: BS 1E Germany: DIN E-A199.5 Alloy 1350...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006695
EISBN: 978-1-62708-210-5
... Other (each) 0.05 max 0.03 max Other (total) 0.15 max 0.10 max Al bal bal Mill product specifications of alloy 5052 Table 2 Mill product specifications of alloy 5052 Product ASTM International ISO U.S. federal AMS ASME EN JIS Sheet and plate B 209 ISO 6361...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006596
EISBN: 978-1-62708-210-5
... bar O, T4, T451, T6, T651 Rolled and worked wire O, T4, T6 Forgings and forging stock F, T4, T6, T652 Alloy 2014 (Al Cu4SiMg) mill-product specifications Table 2 Alloy 2014 (Al Cu4SiMg) mill-product specifications Product ASTM Federal AMS ASME ISO EN JIS Sheet...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006597
EISBN: 978-1-62708-210-5
... wire O, H13, T4 Rivets T4 Mill product specifications of aluminum 2017 and/or 2017A Table 5 Mill product specifications of aluminum 2017 and/or 2017A Product ASTM Federal AMS ISO EN JIS Sheet, strip, and plate … … … ISO 6361 EN 485 JIS H 4000 Extruded tubes...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006693
EISBN: 978-1-62708-210-5
..., and rivets. Mill product specifications of alloy 5005 include: Sheet and plate: ASTM B 209, ISO 6361, EN 485, JIS H 4000 Drawn rod, bar, tube, or wire: ASTM B 210 and B 483 (tube), ISO 6363, EN 754, JIS H 4080 (tube) Extrusions (rod, bar, profile): ISO 6362, EN 755, JIS H 4080 (tube), JIS H...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005747
EISBN: 978-1-62708-171-9
...” 32535 May 2012 “Thermal Spraying—Tubular Coating Tensile Test” EN 582 Jan 1994 “Thermal Spraying—Determination of Tensile Adhesive Strength” EN 657 June 2005 “Thermal Spraying—Terminology, Classification” EN 1274 Feb 2005 “Thermal Spraying—Powders—Composition, Technical Supply...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006737
EISBN: 978-1-62708-210-5
... specifications for aluminum alloy 7075 Table 2 Product specifications for aluminum alloy 7075 Product ASTM AMS ISO EN JIS Federal Sheet and plate (bare or clad) B 209 4024, 4044. 4045, 4046,4048, 4049, 4078, 4196, 4197 ISO 6361 EN 485 JIS H 4000 QQ-A-250/ (12, 13, 24, 25, 18) Wire...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006552
EISBN: 978-1-62708-210-5
... and 8 xxx series aluminum alloys Aluminum Association (AA) designation UNS designation EN AA composition, max unless a range or min is specified, wt% Si Fe Cu Mn Mg Zn Al, min 1050 A91050 … 0.25 0.40 0.05 0.05 0.05 0.05 99.50 1050A A91050 Al 99.5 0.25 0.40 0.05...
Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006717
EISBN: 978-1-62708-210-5
... alloy 6063 Product ASTM ISO EN JIS Military AMS ASME Wire, rod, bar, profiles (shapes), and tube: extruded B 221 ISO 6362 EN 755 JIS H 4100 … 4156 SB221 Tube: extruded, seamless B 241 … … JIS H 4080 … … SB241 Tube: extruded, coiled B 491 … … … … … … Cold...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006312
EISBN: 978-1-62708-179-5
..., and double the fatigue strength of conventional gray cast iron. In cylinder block applications, these properties enable the use of fracture-split main bearing caps. When fracture splitting is specified, the CGI specification also requires a Charpy impact energy of 2 to 4 J (1.5 to 3.0 ft ⋅ lbf) (EN 10045-1...