Skip Nav Destination
Close Modal
Search Results for
Coinage
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 27 Search Results for
Coinage
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book: Corrosion: Materials
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003834
EISBN: 978-1-62708-183-2
... with a low coefficient of thermal expansion. When heated, the resulting bimetal will bend about its neutral axis. Thermostat bimetals are used in various temperature-sensing devices, including motor protectors, circuit breakers, automotive chokes, vent dampers, and room thermostats. Clad metal coinage...
Abstract
This article describes the principal cladding processes and methods for calculating properties of clad metals. It reviews the designing processes of clad metals to achieve specific requirements. The article discusses six categories of clad metal systems designed for corrosion control: noble metal clad systems, corrosion barrier systems, sacrificial metal systems, transition metal systems, complex multilayer systems, and clad diffusion alloys.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003150
EISBN: 978-1-62708-199-3
..., Tableware, and Coinage The high reflectivity of silver makes it particularly attractive for applications in jewelry and tableware. Strength, hardness, and wear resistance are obtained through the use of alloys, in particular sterling silver, which contains 92.5% Ag and 7.5% Cu. There are two grades...
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001263
EISBN: 978-1-62708-170-2
... in the duplication of printing plates for coinage and currency because of its facility to produce the highest accuracy in copying engraved masters. Modern Applications Today, the electroforming industry sees a number of high-tech uses for nickel, copper, iron, and alloy deposits to electrofabricate...
Abstract
Electroforming is the process by which articles or shapes can be exactly reproduced by electrodeposition on a mandrel or form that is later removed, leaving a precise duplicate of the original. This article discusses electroforming applications, and explains electroforming of nickel, cobalt, iron, and copper, providing information on mandrel design and selection, electroforming solutions and operating variables. It discusses the significant aspects of electroforming that demand special considerations, such as metal distribution, internal deposit stress, roughness, and treeing. The article concludes with an overview of alloy electroforming.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001351
EISBN: 978-1-62708-173-3
... conventional fusion welding techniques are metallurgically inappropriate, because of the formation of intermetallic compounds. Applications of explosive bonding are diverse and include the production of sandwiched metal for coinage (1965 to 1971), the more-sophisticated use of titanium-to-stainless steel...
Abstract
Explosion welding (EXW), also known as explosive bonding, is accomplished by a high-velocity oblique impact between two metals. This article describes the practice of producing an explosive bond/weld and draws on many previous research results in order to explain the mechanisms involved. It provides a schematic illustration of the arrangement used in the parallel gap explosive bonding process. The article discusses several important concepts pertaining to explosive parameters, hydrodynamic flow, jetting, and metal properties. It summarizes the criteria used to model the explosive bonding process. The article describes bond morphology in terms of wave formation, bond microstructure, and bond strength determination.
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001065
EISBN: 978-1-62708-162-7
Abstract
Copper and copper alloys constitute one of the major groups of commercial metals due to their excellent electrical and thermal conductivities, corrosion and fatigue resistance, ease of fabrication, and good strength. This article lists the types, properties, fabrication characteristics, corrosion ratings, temper designations, and applications of wrought copper and copper alloys. It also presents an outline of the most commonly used mechanical working and heat treating processes. The copper industry in the United States is broadly composed of two segments: producers (mining, smelting, and refining companies) and fabricators (wire mills, brass mills, foundries, and powder plants). The article discusses copper production methods and describes major changes in the structure of the U.S. copper and copper alloys industry.
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001072
EISBN: 978-1-62708-162-7
... to the invention of German silver or nickel-silver (Cu-Sn-Pb-Zn alloys containing 12 to 25 wt% Ni). Nickel plating, coinage, and nickel-silver were the main applications for the small quantity of nickel that was produced through the second half of the nineteenth century. Additional nickel was provided from...
Abstract
Nickel in elemental form or alloyed with other metals and materials has made significant contributions to our present-day society and promises to continue to supply materials for a demanding future. This article provides a historical overview and physical metallurgy of nickel and nickel alloys. It lists and describes the compositions, mechanical and physical properties, and applications of commercial nickel and its alloys. The article briefly explains the forms of corrosion resulting from the exposure of nickel alloys to aqueous environments. It provides valuable information on the commercial forms of nickel alloys, namely, nickel-copper alloys, nickel-chromium and nickel-chromium-iron series, iron-nickel-chromium alloys, controlled-expansion alloys, nickel-iron low-expansion alloys, soft magnetic alloys, and welding alloys.
Book Chapter
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006276
EISBN: 978-1-62708-169-6
..., wire, tube, sheet, and foil. Besides the more familiar copper wire, copper and its alloys are used in electrical and electronic connectors and components, heat-exchanger tubing, plumbing fixtures, hardware, bearings, and coinage. The basic types of processes and equipment for the heat treating...
Abstract
This article provides information on the Unified Numbering System designations and temper designations of copper and copper alloys. It discusses the basic types of heat treating processes of copper and copper alloys, namely, homogenizing, annealing, and stress relieving, and hardening treatments such as precipitation hardening, spinodal hardening, order hardening, and quench hardening and tempering. The article presents tables that list the compositions and mechanical properties of copper alloys. It also discusses two strengthening mechanisms of copper alloys, solid-solution strengthening and work hardening. Finally, the article provides information on the equipment used for the heat treating of copper and copper alloys, including batch-type atmosphere furnaces, continuous atmosphere furnaces, and salt baths.
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005143
EISBN: 978-1-62708-186-3
... drawing, and stretch forming operations Heat exchangers Roll forming, bending, sinking, blanking Coinage Blanking, coining, embossing Bellows, flexible hose Cupping, deep drawing, bending Musical instruments Blanking, drawing, coining, bending, spinning Ammunition Blanking, deep...
Abstract
This article reviews the general characteristics of copper and copper alloys and explains how these characteristics affect the behavior of strip in different types of forming operations. These forming operations include blanking, piercing, bending, drawing and stretch forming, spinning, rubber-pad forming, and contour roll forming. Specialized forming operations such as hydraulic forming, embossing and swaging, and high-velocity metal forming are also reviewed. The article discusses the forming of smaller and larger parts from copper and copper alloy strips, as well as their property requirements and applications.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003135
EISBN: 978-1-62708-199-3
... resistance, wear resistance, and aesthetic appearance play important roles. Copper-Nickel P/M Parts Copper-nickel P/M alloys containing 75Cu-25Ni and 90Cu-10Ni have been developed for coinage and corrosion-resistance applications. The 75Cu-25Ni alloy powder pressed at 772 MPa (112 ksi) has a green...
Abstract
This article discusses the characteristics, properties, and production methods of copper powders and copper alloy powders. Bulk of the discussion is devoted to production and applications of powder metallurgy (P/M) parts, including pure copper P/M parts, bronze P/M parts, brass and nickel silver P/M parts, copper-nickel P/M parts, copper-lead P/M parts, copper-base P/M friction materials, copper-base P/M electrical contact materials, copper-base P/M brush materials, infiltrated parts, and oxide-dispersion-strengthened copper P/M materials.
Book: Powder Metallurgy
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006122
EISBN: 978-1-62708-175-7
... with a “cauliflower” surface ( Fig. 11 ). Generally, these powders are further screened into more usable fractions. PM applications for these powders include welding electrodes and nickel strip for coinage. Hydrometallurgical powder is also used to produce nickel salts and catalysts. However, the vast majority...
Abstract
This article discusses the methods for producing powder metallurgy (PM) nickel powders, including carbonyl process, hydrometallurgical process, hydrogen reduction process, and atomization process, as well as their applications. It describes three processes for producing nickel alloy powders: water atomization, high-pressure water atomization, and gas atomization. The article also provides information on the applications of PM hot isostatic pressing in the oil and gas industry.
Book Chapter
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003987
EISBN: 978-1-62708-185-6
... to more than 1,000,000 strikes, depending on the type of coinage alloy and on coin diameter. Dies for Coining Silverware Probably the greatest amount of industrial coining is done with drop hammers in the silverware industry. Water-hardening steels such as W1 are almost always used for making...
Abstract
Coining is a closed-die forging operation in which all surfaces of the workpiece are confined or restrained, resulting in a well-defined imprint of the die on the workpiece. This article focuses on the coining equipment (hammers and presses), lubricants, and general and special die materials used in the coining process. It discusses the coinability of metals such as steels, copper, and composite metals. The article describes the control of dimensions, surface finishes, and weight of coined items. It concludes with a discussion on processing problems and solutions.
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003803
EISBN: 978-1-62708-177-1
... produced by early Chinese metallurgists and used for many purposes, including statuary, bells, and coinage. In modern times, white cast irons are not much used, and then normally only as a precursor for malleable iron. Furthermore, this early material can have sulfur and/or phosphorus contents that are far...
Abstract
Archaeometallurgists use metallography to reveal and interpret the microstructures of objects, in conjunction with the results of their chemical analyses and microanalyses. This article describes a number of special problems that occur while performing metallographic analyses on archaeological materials. It also presents case studies, with examples that illustrate situations where metallography has contributed to archaeometallurgical studies.
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005602
EISBN: 978-1-62708-174-0
... clad plates of almost any metal combination can be manufactured economically. Applications of EXW are diverse and include the production of sandwiched metal for coinage ( Ref 4 ), the production of titanium-to-stainless steel transition joints in the Apollo spacecraft ( Ref 5 ), and production...
Abstract
This article provides an overview of the important mechanistic aspects of explosion welding (EXW), the process-material interactions, and the critical aspects or parameters that must be controlled. The procedure for ensuring the control of process parameters is also discussed. The article explains the primary variables used to predict EXW parameters and the characteristics of the explosion weld. It concludes with a description of the manufacturing process and practice, and applications of the EXW.
Book: Corrosion: Materials
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003829
EISBN: 978-1-62708-183-2
... in jewelry, coinage, and sterling ware is well known. Also of commercial significance are the uses of silver in manufacturing and processing equipment within the food, chemical, and pharmaceutical industries. Silver has been used for decades within the food industry to maintain purity and freedom from...
Abstract
This article characterizes the corrosion resistance of precious metals, namely, ruthenium, rhodium, palladium, silver, osmium, iridium, platinum, and gold. It provides a discussion on the general fabricability; atomic, structural, physical, and mechanical properties; oxidation and corrosion resistance; and corrosion applications of these precious metals. The article also tabulates the corrosion rates of these precious metals in corrosive environment, namely, acids, salts, and halogens.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003131
EISBN: 978-1-62708-199-3
.... cupronickel coinage). Fig. 1 Relationship between strength and electrical conductivity for copper and copper alloys Corrosion Resistance Copper is a noble metal, but, unlike gold and other precious metals, it can be attacked by common reagents and environments. Pure copper resists attack...
Abstract
Copper and copper alloys are widely used because of their excellent electrical and thermal conductivities, outstanding resistance to corrosion, and ease of fabrication, together with good strength and fatigue resistance. This article provides an overview of property and fabrication characteristics, markets, and applications of copper and its alloys. It contains several tables that provide helpful information on the chemical composition, classification, designation, uses, and mechanical properties of wrought copper and copper alloys.
Book Chapter
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001087
EISBN: 978-1-62708-162-7
... a more significant use as solar energy technology is developed), bearings, catalysts, coinage, and nuclear control rods. The use of silver in photography is based on the ability of exposed silver halide salts to undergo a secondary image amplification process called development. In silver solders...
Abstract
Precious metals are of inestimable value to modern civilization. This article discusses the resources and consumption, trade practices, and special properties of precious metals and its alloys, including ruthenium, rhodium, palladium, silver, osmium, iridium, platinum, and gold, and tabulates the industrial applications of precious metals. It provides information on the commercial forms (wire, rod, sheet, strip, ribbon, and foil) and uses of precious metals, including semifinished products, precious metal powders, industrial uses, coatings, and jewelry.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003144
EISBN: 978-1-62708-199-3
... applications of wrought zinc and zinc alloys Alloy Applications Pure zinc Deep-drawn hardware, expanded metal Zn-Cu Building construction materials, deep-drawn hardware, coinage Zn-Cu-Ti Roofing, gutters, and downspouts; building construction materials; deep-drawn hardware; address plates...
Abstract
This article provides information on the properties, compositions, designations, and applications of zinc and zinc alloys. It discusses the principal areas of application of zinc: in coatings and anodes for corrosion protection of irons and steels; in zinc casting alloys; as an alloying element in copper, aluminum, magnesium, and other alloys; in wrought zinc alloys; and in zinc chemicals. The zinc coating applications of hot dip galvanizing, electrogalvanizing, plating, and thermal spray are presented. The use of zinc alloys in both gravity and pressure die castings is discussed as well as the three main types of wrought products: flat-rolled products, wire-drawn products, and extruded and forged products. The article also provides a section on the corrosion resistance of zinc and zinc coatings in various atmospheres.
Book: Powder Metallurgy
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006018
EISBN: 978-1-62708-175-7
... carbide, titanium carbide, silver, cadmium Vacuum metallizing Aluminum, copper, zinc Coinage Nickel, copper-nickel, titanium Diffusion coating Aluminum-titanium alloys, chromium, zinc, hafnium Electrical and electronic Acoustical elements to improve microphone response Stainless steel...
Abstract
Metal powders are used as fuels in solid propellants, fillers in various materials, such as polymers or other binder systems, and for material substitution. They are also used in food enrichment, environmental remediation market, and magnetic, electrical, and medical application areas. This article reviews some of the diverse and emerging applications of ferrous and nonferrous powders. It also discusses the functions of copier powders and the processes used frequently for copier powder coating.
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003687
EISBN: 978-1-62708-182-5
... analysis of the potentials shown in the emf or galvanic series. Much depends on environmental exposure and the oxidized films formed in pores and discontinuities of plated coatings. For example, some corrosion specialists predicted copper-plated zinc one-cent pieces would be unsuitable coinage because...
Abstract
This article discusses the various factors that affect the corrosion performance of electroplated coatings. It describes the effects of environment and the deposition process on substrate coatings. The article provides a discussion on the electrochemical techniques capable of predicting the corrosion performance of a plated part. It reviews the designs of coating systems for optimal protection of the substrate. The article also discusses controlled weathering tests and accelerated tests used to predict and determine the relative durability of the coating.
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001077
EISBN: 978-1-62708-162-7
... hardware, expanded metal Zn-Cu Building construction materials, deep-drawn hardware, coinage Zn-Cu-Ti Roofing, gutters, and downspouts; building construction materials; deep-drawn hardware; address plates; solar collectors Zn-Pb-Cd-Fe Building construction materials, dry-cell battery cans, deep...
Abstract
This article describes the zinc and zinc alloys for decorative and functional applications. It focuses on the types of zinc coatings, namely, hot dip galvanizing, electrogalvanizing, metallizing, and mechanical galvanizing. The article covers the uses of zinc alloy castings, including pressure die castings, and gravity castings. It details the wrought products of zinc and zinc alloys, including flat-rolled products, wire-drawn products, extruded products, and forged products. The article also describes various properties of zinc alloys, including mechanical, thermal, electrical, chemical, and magnetic properties. The listing for each alloy includes chemical compositions, relevant specifications, mass characteristics, and fabrication characteristics.