1-20 of 624 Search Results for

Cements

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001104
EISBN: 978-1-62708-162-7
... Abstract Cemented carbides belong to a class of hard, wear-resistant, refractory materials in which the hard carbide particles are bound together, or cemented, by a soft and ductile metal binder. The performance of cemented carbide as a cutting tool lies between that of tool steel and cermets...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002124
EISBN: 978-1-62708-188-7
... Abstract This article discusses the manufacturing steps and compositions of cemented carbides, as well as their microstructure, classifications, applications, and physical and mechanical properties. It provides information on new tool geometries, tailored substrates, and the application of thin...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003838
EISBN: 978-1-62708-183-2
... Abstract Cemented carbides are extremely important in corrosion conditions in which high hardness, wear resistance, or abrasion resistance is required. This article describes the effect of binder composition and carbide addition on corrosion behavior of cemented carbides. It lists the examples...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005775
EISBN: 978-1-62708-165-8
... Abstract Pack cementation is the most widely employed method of diffusion coating. This article briefly reviews pack cementation processes of aluminizing, chromizing, and siliconizing. It contains tables that list typical characteristics of pack cementation processes and commercial applications...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003152
EISBN: 978-1-62708-199-3
... Abstract Cemented carbides belong to a class of hard, wear-resistant, refractory materials in which the hard carbide particles are bound together, or cemented, by a ductile metal binder. Cermet refers to a composite of a ceramic material with a metallic binder. This article discusses...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003686
EISBN: 978-1-62708-182-5
... Abstract This article focuses on the pack-cementation coatings, in particular, halide-activated pack cementation coatings on nickel alloys. It also describes the thermodynamics and kinetics of, and simultaneous deposition of various types of, pack cementation processes. These include pack...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003797
EISBN: 978-1-62708-177-1
... has a value of 0.0000 V. Reactions with more than one voltage indicate that results have not been reconciled. Parenthetical materials not needed to balance reactions are catalysts. electrochemical series potential value standard hydrogen electrode CEMENTED CARBIDES belong to a class...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006064
EISBN: 978-1-62708-175-7
... Abstract Cemented carbide is, in its simplest form, a metal-matrix composite of tungsten carbide particles in a cobalt matrix. This article describes the microstructure, physical, and mechanical properties of cemented carbides. The properties discussed include thermal conductivity, magnetic...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006054
EISBN: 978-1-62708-175-7
... Abstract This article describes the secondary operations for cemented carbide parts, namely, diamond grinding, honing, electrical discharge machining, and brazing after sintering to achieve desired results, such as specified size, shape, edge condition, and surface finish. brazing...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006056
EISBN: 978-1-62708-175-7
... Abstract Quality control of cemented carbides includes the evaluation of physical and chemical properties of constituent raw material powders, powder blends/formulations, green compacts, and fully dense finished product. This article provides a summary of the underlying principles and size...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000626
EISBN: 978-1-62708-181-8
... Abstract This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of one specific type of cemented carbide, tungsten carbide. It also assists in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006418
EISBN: 978-1-62708-192-4
... Abstract Cemented carbides, best known for their superior wear resistance, have a range of industrial uses more diverse than that of any other powder metallurgy product including metalworking and mining tools and wear-resistant components. This article discusses raw materials and manufacturing...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006583
EISBN: 978-1-62708-290-7
... Abstract Tungsten, molybdenum, and cemented carbide parts can be produced using several additive manufacturing technologies. This article classifies the most relevant technologies into two groups based on the raw materials used: powder-bed methods, such as selective laser melting, electron beam...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003843
EISBN: 978-1-62708-183-2
... Abstract Portland cement concrete has low environmental impact, versatility, durability, and economy, which make it the most abundant construction material in the world. This article details the types and causes of concrete degradation. Concrete can be degraded by corrosion of reinforcing steel...
Image
Published: 01 January 1994
Fig. 10 Use of an inert filler during application of pack cementation coating to the internal surfaces of a nozzle More
Image
Published: 01 January 1994
Fig. 11 Designs of retorts used in the pack cementation process More
Image
Published: 01 January 1994
Fig. 12 Fluidized-bed cementation process More
Image
Published: 01 January 1994
Fig. 6 Pack-cementation chromizing/siliconizing apparatus. Pack material composed of 3 wt% Cr, 11 wt% Si, 0.25 wt% NH 4 I, and balance, Al 2 O 3 More
Image
Published: 01 January 1994
Fig. 5 Chromium diffusion coatings on a nickel superalloy by (a) pack cementation and (b) out-of-contact gas-phase processing. Both at 500×. Source: Ref 37 More
Image
Published: 01 January 1994
Fig. 6 Flow diagram for typical pack cementation processes. Source: Ref 37 More