1-20 of 81 Search Results for

CALPHAD

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 June 2016
Fig. 32 Phase field simulation prediction obtained using CALPHAD free-energy models in the Pandat database, mobility database, an interfacial energy of 100 mJ/m 2 , and isothermal aging at 700 °C (1290 °F) with four different molybdenum concentrations, (a) to (d) composition profile; (e) to (h More
Image
Published: 01 December 2009
Fig. 2 The Calphad or phenomenological thermodynamic approach to obtain a thermodynamic description or database of a multicomponent system More
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005517
EISBN: 978-1-62708-197-9
... Abstract This article presents the background to the CALculation of PHAse Diagrams (CALPHAD) method, explaining how it works, and how it can be applied in industrial practice. The extension of CALPHAD methods as a core basis for the modeling of generalized material properties is explored...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005511
EISBN: 978-1-62708-197-9
... with kinetic and microstructural evolution models greatly enhances the power of the CALPHAD approach in materials design and processing development. It also discusses the limitations of the CALPHAD approach. CALPHAD approach industrial applications microstructural evolution models phase diagram...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005206
EISBN: 978-1-62708-187-0
... diagrams, which forms the basis for the calculation of phase diagrams (CALPHAD) method. The article also discusses the calculation of phase diagrams and solidification by using the Scheil-Gulliver equation. phase diagram solidification Gibbs energy function CALPHAD method Scheil-Gulliver equation...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006257
EISBN: 978-1-62708-169-6
..., and microstructural scale for homogenization of metal alloys. It also discusses the CALPHAD software to optimize the homogenization heat treatment and the Scheil module of the commercial thermodynamic modeling software. castings computational algorithm heat treatment homogenization incipient melt point...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006277
EISBN: 978-1-62708-169-6
... of Burgers correspondence variants and orientation variants. The article also includes calculation of the transformation strain with contributions from defect structures developed at alpha/beta interfaces as a precipitates grow in size. In the CALculation of PHAse Diagram (CALPHAD) framework, the Gibbs free...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006151
EISBN: 978-1-62708-163-4
...) C-Zr crystallographic data References References 1. Ishida K. and Nishizawa T. , J. Phase Equilib. , Vol 12 ( No. 4 ), 1991 , p 417 – 424 2. Khvan A.V. , Hallstedt B. , and Chang K. , Calphad , Vol 39 , 2012 , p 54 – 61 3. Subramanian...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006176
EISBN: 978-1-62708-163-4
... – 3281 3. Islam F. and Medraj M. , Calphad , Vol 29 ( No. 4 ), 2005 , p 289 – 302 4. Okamoto H. , J. Phase Equilib. Diff. , Vol 35 ( No. 2 ), 2014 , p 208 – 219 5. Paliwal M. and Jung I.H. , Calphad , Vol 33 , 2009 , p 744 – 754 6...
Image
Published: 27 April 2016
Source: J. Miettinen, Thermodynamic Description of the Cu-Mn-Zn System in the Copper-Rich Corner, CALPHAD , Vol 28, 2004, p 313–320 ( Ref 7 ) More
Image
Published: 27 April 2016
Source: J. Miettinen, Thermodynamic Description of the Cu-Mn-Zn System in the Copper-Rich Corner, CALPHAD , Vol 28, 2004, p 313–320 ( Ref 7 ) More
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006165
EISBN: 978-1-62708-163-4
.... , Du Y. , Xu H. , and Chang K. , Calphad , Vol 37 , 2012 , p 72 – 76 11. Geng T. , Li C. , Du Z. , Guo C. , Zhao X. , and Xu H. , J. Alloy. Compd. , Vol 509 , 2011 , p 3080 – 3088 12. Gokhale A.B. and Abbaschian G.J. , Bull...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006207
EISBN: 978-1-62708-163-4
... – 80 3. Yin F. , Tedenac J-C. , and Gascoin F. , Calphad , Vol 31 , 2007 , p 370 – 379 4. Binary Alloy Phase Diagrams , 2nd ed. , Massalski T.B. , Okamoto H. , Subramanian P.R. , and Kacprzak L. , Ed., ASM International , 1990 , p 3407 – 3408...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006158
EISBN: 978-1-62708-163-4
.... , Calphad , Vol 34 , 2010 , p 134 – 137 4. Ren X. , Li C. , Du Z. , and Guo C. , Calphad , Vol 35 , 2011 , p 446 – 454 5. Bale C.W. , Bull. Alloy Phase Diagrams , Vol 3 ( No. 3 ), 1982 , p 310 – 313 6. Okamoto H. , J. Phase Equilib. Diff...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006190
EISBN: 978-1-62708-163-4
... 148 – 165 5. Chevalier P.Y. , Fischer E. , and Cheynet B. , Calphad , Vol 28 , 2004 , p 15 – 40 6. wriedt H.A. , Bull. Alloy Phase Diagrams , Vol 10 ( No. 3 ), 1989 , p 271 – 277 7. wriedt H.A. , Bull. Alloy Phase Diagrams , Vol 10 ( No. 4...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006166
EISBN: 978-1-62708-163-4
... , p 62 – 83 7. Chen C. , Wang M. , Du Y. , Gao Q. , Hu B. , and Liu S. , Calphad , Vol 38 , 2012 , p 17 – 22 8. San-Martin A. and Manchester F.D. , J. Phase Equilib. , Vol 12 ( No. 3 ), 1991 , p 332 – 343 9. Wang K...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006189
EISBN: 978-1-62708-163-4
... References References 1. Kowalski M. and Spencer P.J. , Calphad , Vol 19 , 1995 , p 229 – 239 2. Okamoto H. , J. Phase Equilib. Diff. , Vol 31 ( No. 2 ), 2010 , p 200 – 201 3. Kainulainen I. , Taskinen P. , and Gisby J. , Calphad , Vol 34...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006175
EISBN: 978-1-62708-163-4
... element in the binary pair. Lu-Pb (Lutetium-Lead) Lu-Pb crystallographic data Lu-Tl (Lutetium-Thallium) Lu-Tl crystallographic data References References 1. Wang D. , Yu Y. , Liu X.J. , and Wang C.P. , Calphad , Vol 41 , 2013 , p 20 – 25...
Image
Published: 01 August 2013
with the calculated isothermal section according to the CALPHAD database (2008). Source: Ref 45 More
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006167
EISBN: 978-1-62708-163-4
... – 446 8. Shin D. , Arróyave R. , and Liu Z.K. , Calphad , Vol 30 , 2006 . p 375 – 386 9. Binary Alloy Phase Diagrams , 2nd ed. , Massalski T.B. , Okamoto H. , Subramanian P.R. , and Kacprzak L. , Ed., ASM International , 1990 , p 2105 , 2107...