1-20 of 814 Search Results for

Bolts Bolts

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 January 1990
Fig. 8 Hardness distribution for eight lots of 1038 steel bolts. Bolts, 13 mm ( 1 2 in.) in diameter, were all made from one heat of steel. The bolts were heat treated in one plant to eight different levels of nominal hardness. Tests were made in the originating plant and in seven More
Image
Published: 01 January 2006
Fig. 13 Use of a shaper for correction of springback in U-bolts, J-bolts, or rings More
Image
Published: 01 January 1990
Fig. 9 Fatigue data for 1040 and 4037 steel bolts. The bolts ( 3 8 by 2 in., 16 threads to the inch) had a hardness of 35 HRC. Tensile properties of the 1040 steel at three-thread exposure were yield strength, 1060 MPa (154 ksi); tensile strength (axial), 1200 MPa (175 ksi); tensile More
Image
Published: 09 June 2014
Fig. 64 Arcing in an inductor foot caused by loose bolts combined with dirt accumulation More
Image
Published: 01 January 2006
Fig. 11 Galvanic corrosion of type 304 stainless steel stud bolts that fastened two Alloy 20 (ACI CN-7M) pump components. The pump was pumping 45% H 2 SO 4 at 95 °C (200 °F). The stud bolts were anodic to the Alloy 20 pump housings. Courtesy of A.R. Wilfley & Sons, Inc., Pump Division More
Image
Published: 01 January 1996
Fig. 4 Stress concentration factor ( K t ) versus bolt diameter for bolts with standard metric threads. Source: Ref 14 More
Image
Published: 01 January 1996
Fig. 5 Nomograph for torque on bolts. Source: Ref 17 More
Image
Published: 01 January 1989
Fig. 3 Effect of hardness on fatigue strength for bolts with threads rolled before or after heat treatment More
Image
Published: 01 January 1989
Fig. 3 Four working methods used in shaping. (a) Standard T-slot with bolts, blocks, and clamp plates. (b) Toe dogs for thin workpieces. (c) Outboard support with jacks for irregular workpieces. (d) Vise More
Image
Published: 01 January 2001
Fig. 31 Bearing-bypass load interaction for loaded bolts in advanced composites More
Image
Published: 01 January 1987
Fig. 93 Example of quench cracks on the head of AISI 1040 steel bolts. Cracks were caused by incomplete development of the case. (a) Bolt heads at 0.72×; cracks accentuated using magnetic particles. (b) Quench crack near a corner. Etched with 2% nital. 54×. (c) Opened quench crack with arrows More
Image
Published: 01 January 2001
Fig. 5 Prototype C/SiC CMC disk brake assembly fabricated from CMC disks, bolts (right), and ribs (left). CMC brakes are now in use on two German production automobiles and provide greatly improved braking performance over metal disks. Courtesy of W. Krenkel, German Aerospace Research Center More
Image
Published: 01 January 2005
Fig. 27 Deep pitting attack was discovered on steel bolts used to retain parts in a metal-shaping (cutting) machine. The surfaces of the bolts were covered with a black, oily substance, which, on analysis, was found to contain sulfurous species. Other steel parts also failed by pitting attack More
Image
Published: 01 January 2003
Fig. 12 4137 steel (UNS G41370) bolts (hardness, 42 HRC) that failed by hydrogen-assisted stress-corrosion cracking caused by acidic chlorides from a leaking polymer solution. (a) Overall view of failed bolts. (b) Longitudinal section through one of the failed bolts in (a) showing multiple More
Image
Published: 01 January 1990
Fig. 1 Hardenability of 19 mm ( 3 4 in.) diam bolts made of 1541 steel and oil quenched. (a) Body section. (b) Threaded section. The curves represent the average as-quenched hardnesses of fifteen 19 mm ( 3 4 in.) diam bolts from one heat of each grade. C is center of the bolt More
Image
Published: 01 January 1990
Fig. 7 Relation of hardness and tensile strength for SAE grade 5 bolts made of 1038 steel More
Image
Published: 01 January 1990
Fig. 11 Fatigue limits for roll-threaded steel bolts. (a) Four different lots of bolts that were roll threaded, then heat treated to average hardness of 22.7, 26.6, 27.6, and 32.6 HRC. (b) Five different lots that were heat treated to average hardnesses of 23.3, 27.4, 29.6, 31.7, and 33.0 HRC More
Image
Published: 01 January 1990
Fig. 12 4137 steel bolts (hardness: 42 HRC) that failed by hydrogen-assisted SCC caused by acidic chlorides from a leaking polymer solution. (a) Overall view of failed bolts. (b) Longitudinal section through one of the failed bolts in (a) showing multiple, branched hydrogen-assisted stress More
Image
Published: 01 January 1990
Fig. 25 Manufacturing sequence for class 8.8 automotive bolts from microalloyed and carbon steels More
Image
Published: 01 January 2005
Fig. 31 Use of molded plastic caps on socket-head and hex-head bolts to avoid galvanic corrosion. Source: Ref 35 More