1-20 of 128 Search Results for

Al-Si bronze (wrought aluminum-silicon bronze)

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006281
EISBN: 978-1-62708-169-6
... bronze cast silicon bronze copper alloys heat treatment strengthening wrought aluminum bronze wrought beryllium bronze wrought silicon bronze BRONZES GENERALLY ARE USED to describe many different copper-base alloys in which the major alloying addition is neither zinc nor nickel. However...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005444
EISBN: 978-1-62708-196-2
... Cupro-nickel, 30% 0.07 Cupro-nickel, 10% 0.095 Nickel silver, 65-18 0.08 Nickel silver, 55-18 0.07 Nickel silver, 65-12 0.10 High-silicon bronze (A) 0.09 Low-silicon bronze (B) 0.14 Aluminum bronze, 5% Al 0.198 Aluminum bronze, (3) 0.18 Aluminum-silicon bronze 0.108...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003131
EISBN: 978-1-62708-199-3
... bronzes C50100-C52400 Cu-Sn-P Leaded phosphor bronzes C53200-C54800 Cu-Sn-Pb-P Copper-phosphorus and copper-silver-phosphorus alloys C55180-C55284 Cu-P-Ag Aluminum bronzes C60600-C64400 Cu-Al-Ni-Fe-Si-Sn Silicon bronzes C64700-C66100 Cu-Si-Sn Other copper-zinc alloys C66400...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005442
EISBN: 978-1-62708-196-2
..., 5% Al 8.17 0.294 Aluminum bronze, (3) 7.78 0.281 Aluminum-silicon bronze 7.69 0.278 Aluminum bronze, (1) 7.58 0.274 Aluminum bronze, (2) 7.58 0.274 Beryllium copper 8.23 0.297 Casting alloys Chromium copper (1% Cr) 8.7 0.31 88Cu-10Sn-2Zn 8.7 0.31 88Cu-8Sn...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006274
EISBN: 978-1-62708-169-6
... 4032 wrought alloy and 4643 aluminum-silicon filler metal. Alloy 4643 is a 4% Si-Al filler that contains a small amount of magnesium and is primarily recommended for welding of thick or heavy 6 xxx -series base metals when postweld heat treating may follow. This alloy provides better response...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006276
EISBN: 978-1-62708-169-6
... (brasses): contain up to 40% Zn Copper-tin alloys (phosphor bronzes): contain up to 10% Sn and 0.2% P Copper-aluminum alloys (aluminum bronzes): contain up to 13.5% Al Copper-silicon alloys (silicon bronzes): contain up to 3% Si Copper-nickel alloys: contain up to 30% Ni Copper...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001068
EISBN: 978-1-62708-162-7
... C95600 Silicon-aluminum bronze B 148-9E 91 … … … … 7 2 Si C95700 Aluminum bronze … 75 … … … 3 8 2 Ni, 12 Mn C95800 Nickel-aluminum bronze … 81.5 … … … 4 9 4 Ni, 1.5 Mn ASTM B 176 C85700 Yellow brass … 61 1 1 37 … … … C85800 Yellow brass Z30A 58 1...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003167
EISBN: 978-1-62708-199-3
... composition of aluminum-base bearing alloys Table 8 Designations and nominal composition of aluminum-base bearing alloys No. Designation Composition, % Product form Applications UNS SAE ISO Other Al Si Cu Ni Mg Sn Other High-tin alloys 1 A08081 Alloy 783 AlSn20Cu … 79...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003772
EISBN: 978-1-62708-177-1
... Sn, 37 Zn Wrought bronzes C51000 Phosphor bronze, 5% A Bal Cu, 5.0 Sn, 0.2 P C52100 Phosphor bronze, 8% C Bal Cu, 8.0 Sn, 0.2 P C63000 Aluminum bronze, 10% 82.2 Cu, 10 Al, 3 Fe, 4.8 Ni C64700 Silicon-nickel bronze Bal Cu, 1.9 Ni, 0.6 Si C67500 Manganese bronze A 58.5 Cu...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005332
EISBN: 978-1-62708-187-0
... UNS No. Nominal composition, % Yield strength, 0.5% Tensile strength Elongation, % ASTM specification Cu Sn Pb Zn Ni Fe Al Mn Si Other MPa ksi MPa ksi Aluminum bronze C95300 89 … … … … 1 10 … … … 235 34 565 82 20 B 806 C95400 84 … … … 1 4 11...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001438
EISBN: 978-1-62708-173-3
...-aluminum alloys (aluminum bronzes) , which contain up to 10% Al Copper-silicon alloys (silicon bronzes) , which contain up to 3% Si Copper-nickel alloys , which contain up to 30% Ni Copper-zinc-nickel alloys (nickel silvers) , which contain up to 27% Zn and 18% Ni Special alloys , which...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002185
EISBN: 978-1-62708-188-7
... (1.40 Fe) 1.00 30 C61300 Aluminum bronze 90.00 (7 Al) … (2.7 Fe) 0.3 … C61800 Aluminum bronze 89.00 (9.8 Al) … (1.0 Fe) … … C63000 Nickel-aluminum bronze 82.00 5 (10 Al) (3.0 Fe) … 30 C66100 Leaded silicon bronze (D) 95.60 (0.4 Pb, 1.5 Mn, 1.5 Zn, 3 Si) 60...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005445
EISBN: 978-1-62708-196-2
... and aluminum alloys Aluminum (99.996%) 64.95 2.65 EC (O, H19) 62 2.8 5052 (O, H38) 35 4.93 5056 (H38) 27 6.4 6101 (T6) 56 3.1 Copper and copper alloys Wrought copper Pure copper 103.06 1.67 Electrolytic (ETP) 101 1.71 Oxygen-free copper (OF) 101 1.71 Free...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006412
EISBN: 978-1-62708-192-4
... in the dark phase and copper-tin is present in the light phase. Original magnification: 50× Mixed Microstructures Mixed microstructures that combine the characteristics of types I and III are exhibited by Al-Si-Sn alloys and Al-Si-Pb alloys. In these alloys, the aluminum matrix contains both...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001065
EISBN: 978-1-62708-162-7
... C68700 (aluminum bronze, arsenical) 77.5 Cu, 20.5 Zn, 2.0 Al, 0.1 As T 414 60 186 27 55 30 C68800 73.5 Cu, 22.7 Zn, 3.4 Al, 0.40 Cu F 565–889 82–129 379–786 55–114 36–2 … C69000 73.3 Cu, 3.4 Al, 0.6 Ni, 22.7 Zn F 496–896 72–130 345–807 50–117 40–2 … C69400 (silicon red...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005644
EISBN: 978-1-62708-174-0
..., arc welding fair … … Welding not recommended at or above 9% Sn Silicon bronzes (Cu3%Si1%Mn) TIG, MIG, resistance Preheat 20–65 °C (70–150 °F) … Can be welded by arc, resistance methods. Avoid stressing joints. Filler as parent metal Aluminum bronzes (Cu-5%Al, Cu-10%Al, 5%Fe, 5%Ni) TIG...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006280
EISBN: 978-1-62708-169-6
... Bronze, low fuming 56.0–60.0 0.05 0.25–1.25 bal 0.75–1.10 Sn; 0.01 Al; 0.01–0.50 Mn; 0.04–0.15 Si C68700 Aluminum brass, arsenical 76.0–79.0 0.07 0.06 bal 1.8–2.5 Al; 0.02–0.06 As C68800 … bal 0.05 0.2 21.3–24.1 3.0–3.8 Al; 0.25–0.55 Co C69050 … 70.0–75.0 … … bal 0.50–1.5...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005887
EISBN: 978-1-62708-167-2
... xxxx , C66400–C698000 Phosphor bronze Sn C5 xxxx Aluminum bronzes Al C60600–C64200 Silicon bronzes Si C54700–C66100 Copper-nickel, nickel silvers Ni C7 xxxx Source: Ref 3 Brasses are divided into two classes: The α alloys, with less than 37% Zn. These alloys...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003082
EISBN: 978-1-62708-199-3
... Admiralty brass 940 1720 Naval brass 900 1650 Phosphor bronze      5% Sn 1050 1920  10% Sn 1000 1830 Aluminum bronze, 7% Al, 2.5% Fe 1045 1915 High-silicon bronze, 3.3% Si 1025 1880 Copper-nickel      10% Ni 1150 2100  21% Ni 1150–1200 2100–2190  30% Ni...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002411
EISBN: 978-1-62708-193-1
... composition, % C17200 1.9 Be, 0.25 Co C17410 0.3 Be, 0.4 Co C17510 0.4 Be, 1.8 Ni C26000 30 Zn C51000 5.0 Sn, 0.2 P C63800 2.8 Al, 1.8 Si, 0.4 Co C65400 3.1 Si, 1.6 Sn, 0.05 Cr C68800 23 Zn, 3.4 Al, 0.4 Co C72050 3.2 Ni, 0.75 Si, 0.2 Mg C72900 15 Ni, 8 Sn C76200...