... 0.6 Si max Fe 0.70 Fe max 0.8 Fe max Cu 0.25 Cu max 0.05–0.25 Mn 1.0 to 1.5 0.8–1.4 Mg 0.8 to 1.3 0.8–1.3 Zn 0.25 Zn max 0.25 Zn max Ti … 0.10 Ti max Other (each), max 0.05 0.05 Other (total), max 0.15 0.15 Al bal bal Alloy 3004...
Image
Published: 01 December 1998
Fig. 5 Strain-hardening curves for aluminum (1100), Al-Mn (3003) alloys, and Al-Mg (5050 and 5052) alloys More
Image
Published: 01 January 1990
Fig. 7 Tensile properties in Al-Mg-Mn alloys in the form of annealed (O temper) plate 13 mm (0.5 in.) thick More
Image
Published: 30 November 2018
Fig. 4 Tensile properties in Al-Mg-Mn alloys in the form of annealed (O temper) plate 13 mm (0.5 in.) thick More
Image
Published: 01 December 1998
Fig. 4 Tensile properties in Al-Mg-Mn alloys in the form of annealed (O temper) plate 13 mm (0.5 in.) thick More
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005408
EISBN: 978-1-62708-196-2
... Abstract This article explores the potential of through-process simulations of the development of microstructure, texture, and resulting properties during the thermomechanical processing of Al-Mn-Mg alloys, starting from the as-cast ingot to final-gage sheet. It provides an introduction...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006702
EISBN: 978-1-62708-210-5
... Abstract Alloy 5454 is an Al-Mg-Mn-Cr solid solution alloy with relatively high strength used for handling chemicals at elevated temperatures in the chemical and process industries. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006703
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on composition limits, mill product specifications, fabrication characteristics, processing effects on physical and mechanical properties, and applications of high-strength Al-Mg-Mn-Cr alloy 5456. aluminum alloy 5456 aluminum mill products...
Image
Published: 15 December 2019
Fig. 36 Continuously cast aluminum alloy 3004 (Al-1.25%Mn-1.05%Mg) etched using Keller’s reagent and viewed using bright field (a) and DIC (b). Dendrites are visible using DIC but not in bright field, while intermetallic particles between dendrites are easier to see in bright field. More
Image
Published: 01 December 2009
Fig. 5 Total number density of all voids in an Al-Mg-Cu-Mn superplastic alloy as a function of strain at various temperatures and strain rates, showing that voids nucleate continuously during deformation More
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006600
EISBN: 978-1-62708-210-5
... Abstract Alloy 2027 is an Al-Cu-Mg-Mn-Zr alloy providing improved mechanical properties compared with those of alloy 2024. Alloy 2027-T3511 extrusions are typically used for stringers to stiffen wing skin panels machined from damage tolerant 2xxx alloy plates. This datasheet provides...
Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006722
EISBN: 978-1-62708-210-5
... Abstract Alloy 6156 is an Al-Si-Mg-Cu-Mn weldable alloy, developed for the lower portion of the fuselage, which required a T6 temper strength level and high damage tolerance properties. This datasheet provides information on key alloy metallurgy of this 6xxx series alloy. Fatigue crack growth...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006233
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of ternary alloy phase diagrams for which aluminum (Al) is the first-named element in the ternary system. The other elements are C, Co, Cr, Cu, Fe, Ga, Li, Mg, Mn, Mo, Nb, Ni, Sb, Si, Ti, U, V and Zn. The diagrams are presented with element compositions...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006241
EISBN: 978-1-62708-163-4
... (Aluminum - Chromium - Iron)” , “Al-Cu-Fe (Aluminum - Copper - Iron)” , “Al-Fe-Mn (Aluminum - Iron - Manganese)” , “Al-Fe-Ni (Aluminum - Iron - Nickel)” , “Al-Fe-Si (Aluminum - Iron - Silicon)” , and “Al-Fe-Zn (Aluminum - Iron - Zinc)” in the article “Al (Aluminum) Ternary Phase Diagrams.” “B-C...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003769
EISBN: 978-1-62708-177-1
... Alloy group Nominal chemical composition (a) , wt% Mg Si Ti Cr Mn Fe Ni Cu Zn Zr Other Wrought alloys 1 xxx (Al > 99.00%) 0.006–0.25 0.006–0.7 0.002–0.06 0.01–0.03 0.002–0.05 0.006–0.6 … 0.006–0.35 0.006–0.05 … … 2 xxx (Cu) 0.02–0.8 0.10–1.3 0.02–0.3 0.05...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003124
EISBN: 978-1-62708-199-3
... and silicon are also present and form the quaternary phase Al 12 (Fe,Mn) 3 Si. In alloys containing copper and manganese, the ternary phase Al 20 Cu 2 Mn 3 is formed. Most of the alloys in which chromium is present also contain magnesium, so that during solid-state heating they form Al 12 Mg 2 Cr, which...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006503
EISBN: 978-1-62708-207-5
... in commercial aluminum alloys Alloy Phase constituents (a) Rough state Treated state Wrought alloys 1 xxx (Al > 99.00%), Al-Fe-Si, Al-Cu Al 3 Fe, α-Al(FeSi) Al 6 Mn, α-Al(FeSi) 2 xxx (Cu), Al-Si-Cu-Mn-Mg, Al-Si-Cu-Mn, Al-Cu-Mg, Al-Cu-Mg-Ni, Al-Cu-Mn-Ti-V-Zr, Al-Cu-Mg-Ni-Fe-Ti Al...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006692
EISBN: 978-1-62708-210-5
...; Bi 1.8; Al bal 84 Galling-resistant bar and rod, age hardenable ( Alloy Digest, Al-385, Oct 2003) 4032 A94032 AlSi12.5MgCuNi Si 12.2; Cu 0.9; Mg 1; Ni 0.9; Al bal 85 Forgings, age hardenable, with wear resistance 4115 A94115 AlSi2MnMgCu Si 2; Mn 0.9; Cu 0.3; Mg 0.3; Al bal 96 Sheet...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006707
EISBN: 978-1-62708-210-5
... composition, wt% Approximate melting range Mn Mg Cr Ti Al °C °F 5183 0.75 4.75 0.15 … bal 579–638 1075–1180 5356 0.12 5.0 0.12 0.13 bal 571–635 1060–1175 5554 0.75 2.7 0.12 0.12 bal 602–646 1115–1195 5556 0.75 5.1 0.12 0.12 bal 568–635 1055–1175 5654...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006176
EISBN: 978-1-62708-163-4
... element in the binary pair. Additional binary systems that include magnesium are provided in the following locations in this Volume: “Ag-Mg (Silver - Magnesium)” in the article “Ag (Silver) Binary Alloy Phase Diagrams.” “Al-Mg (Aluminum - Magnesium)” in the article “Al (Aluminum) Binary...