DOI: 10.31399/asm.hb.v11.a0003553
EISBN: 978-1-62708-180-1
... articles ( Ref 1 , 2 ), review articles ( Ref 3 , 4 , 5 , 6 , 7 , 8 ), and the Selected References listed at the end of this article. General Characteristics of SCC Based on extensive empirical investigations, a number of special characteristics of SCC have been observed and categorized...