Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006347
EISBN: 978-1-62708-179-5
... castings Specification No. Class or grade Microstructure Typical applications Ferritic ASTM A47 32510 Temper carbon and ferrite General engineering service at normal and elevated temperatures for good machinability and excellent shock resistance 35018 ASTM A338 32510 Temper...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002178
EISBN: 978-1-62708-188-7
... (0.625) 21 (70) 0.75 (0.030) S4, S5 (M2, M3) 76 (250) 84 (275) 1.0 (0.040) P30, M30 (C-6) … … … Ferritic malleable irons: ASTM A47, grades 32510, 35018; ASTM A602, grade M3210; SAE J158, grade M3210 110–160 Malleablized 1 (0.040) 58 (190) 0.18 (0.007) S4, S5 (M2, M3) 230 (750) 245...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006333
EISBN: 978-1-62708-179-5
... . Specification No. Class or grade Microstructure Typical applications Ferritic ASTM A47 32510 Temper carbon and ferrite General engineering service at normal and elevated temperatures for good machinability and excellent shock resistance 35018 ASTM A338 32510 Temper carbon and ferrite...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
... in the electrolyte of interest against a reference electrode half-cell, such as saturated calomel, as described by the procedure in ASTM G 82 ( Ref 3 ). To prepare a valid galvanic series for a given set of materials and environment of interest, all the factors affecting the potential must be addressed...