1-20 of 38 Search Results for

ASTM A36

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 December 2004
Fig. 28 Microstructure of an ASTM A36 structural steel showing ferrite + pearlite. Note the remnants of scratches in the softer ferrite phase. These subsurface deformation zones from grinding (as shown in Fig. 26 ) were not removed in the polish. 2% nital etch. 100× More
Image
Published: 01 January 2000
Fig. 4 Effect of temperature and strain rate on plane-strain fracture-toughness behavior of ASTM type A36 steel More
Image
Published: 01 January 1996
Fig. 29 Effect of temperature and strain rate on plane-strain fracture-toughness behavior of ASTM type A36 steel. Source: Ref 44 More
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006759
EISBN: 978-1-62708-295-2
... be employed for alloy verification, or the results must indicate the potential that various alloys match the chemistry of the part. An example is the overlapping chemistry of the structural carbon steel ASTM A36 and the high-strength, low-alloy steel (HSLA) ASTM A572. The A36 structural steel has chemical...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005601
EISBN: 978-1-62708-174-0
... electrodes are available include the following. <italic>Mild Steels</italic> Mild steels , such as AISI 1010 to 1030 and ASTM A36, A285, A515, A516, and A572 grades 50 and 60, are commonly used in the fabrication of heavy equipment, mining machinery, oil storage tanks, water towers, bridge structures...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005589
EISBN: 978-1-62708-174-0
... force, and force from the impinging arc plasma, Ref 5 ). Figure 5 shows EPMA composition profiles for iron, nickel, and chromium acquired from a weld made with 308 stainless steel filler metal on A36 carbon steel with the gas metal arc welding process ( Ref 6 ). The composition trace was made from...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003264
EISBN: 978-1-62708-176-4
..., which includes offset yield strength, extension-under-load yield strength, and upper yield strength. The article concludes with a description of the general procedures for conducting the tension test based on ASTM standards and the variability of tensile properties. ductility elongation...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003305
EISBN: 978-1-62708-176-4
... of ductile tearing. Fig. 4 Effect of temperature and strain rate on plane-strain fracture-toughness behavior of ASTM type A36 steel An analysis of plane-strain fracture-toughness data that were obtained for constructional steels and that were valid according to ASTM standard procedures shows...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005259
EISBN: 978-1-62708-187-0
... and end plate material. Commonly used end plate materials are ASTM A36 steel, 1015 steel, or 1018 steel plate. In cases of extremely large-diameter plates (&gt;450 mm, or 18 in.), the end plate material can be pressure-vessel-quality ASTM A285 grade C or A515 grade 70. For maximum adhesion of the mold...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005972
EISBN: 978-1-62708-168-9
...). Source: Ref 1 Similar Steels (U.S. and/or Foreign) ASTM A686 (W-1); SAE J437 (W108), (W109), (W110), (W112), J438, (W108), (W109), (W110), (W112); (Ger.) DIN 1.1525, 1.1545, 1.1625, 1.1654, 1.1663, 1.1673, 1.1744, 1.1750, 1.1820, 1.1830; (Fr.) AFNOR A35-590 1102 Y(1) 105, A35-590 1103 Y (1...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003094
EISBN: 978-1-62708-199-3
... Width Other limitations Specification symbol (ASTM No.) mm in. mm in. Metric units English units Hot-rolled sheet 1.2–6.0 0.045–0.230 incl &gt;300–1200 incl &gt;12–48 incl Coils and cut lengths A 569M, A 621M, or A 622M A 569, A 621, or A 622 1.2–4.5 0.45–0.180 incl &gt;1200...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001818
EISBN: 978-1-62708-180-1
... a stream of gas consisting of 55% H 2 S, 39% CO 2 , 5% H 2 , and 1% hydrocarbons at 40 °C (100 °F) and 55 kPa (8 psi). Specifications required the clapper to be made of 13-mm ( 1 2 -in.) thick ASTM A36 steel, stress relieved and cadmium plated. Investigation Fracture occurred at the welded...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003095
EISBN: 978-1-62708-199-3
... for specific applications. Dimensions and Tolerances The nominal dimensions of hot rolled steel bars and shapes are designated in inches or millimeters with applicable tolerances, as shown in ASTM specifications A 6 and A 29. Surface Imperfections Surface Seams or Laps Surface seams or laps...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002397
EISBN: 978-1-62708-193-1
... strength or range, MPa C Mn Si Cr Ni Mo V Co Other Ferrite-pearlite steels A285, grade C K02801 0.17 0.52 0.06 … … … … … … 240 A36 … 0.25 1.0 … … … … … … … ≥250 St 37-3 … 0.08 0.45 0.17 … … … … … … 320 A588, grade A K11430 0.15 1.1 0.20...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006833
EISBN: 978-1-62708-329-4
... Welding Code,” in 1988. The NCHRP testing ( Ref 6 ) found that fatigue life was independent of yield strength (248 to 690 MPa, or 36 to 100 ksi) for the tested steels. Thus, the same detail configuration in ASTM International A36 steel would have the same fatigue life as in A514 steel. Because...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002395
EISBN: 978-1-62708-193-1
... in these applications. Although some of the end users of these structures have their own steel specifications, the vast majority rely on ASTM specifications, particularly for the basic strength properties and chemical composition. An end user who does have a steel specification often bases it on an ASTM grade with some...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006823
EISBN: 978-1-62708-329-4
... with chloride anions ( Ref 17 , 18 ). Carbon steels can also be susceptible to localized corrosion in nitrate-rich solutions ( Ref 19 ). Scott et al. ( Ref 20 ) have shown that pitting was observed in ASTM International A537 class 2 carbon steel material in solutions with low nitrite-to-nitrate ratios. Mild...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006812
EISBN: 978-1-62708-329-4
...—Repairs of Pressure Equipment and Piping Other industry standards: ASTM E 620—Standard Practice for Reporting Opinions of Technical Experts ASTM E 1188—Standard Practice for the Collection and Preservation of Information and Physical Items by a Technical Investigator ASTM E 678—Standard...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005558
EISBN: 978-1-62708-174-0
... factors for the weld size in relation to plate thickness in rigidity or non-full-strength designs are also given. Weld size factors for full-strength and rigidity fillet welds Table 2 Weld size factors for full-strength and rigidity fillet welds Steel ASTM grade Yield strength of base metal...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002364
EISBN: 978-1-62708-193-1
... (SAE FD&amp;E) and the E 08 Committee on Fatigue and Fracture Mechanics of the American Society for Testing and Materials (ASTM). The SAE FD&amp;E has published its second Fatigue Design Handbook , AE10, 1988, and has furthered these general principles to include multiaxial fatigue...