... diameter boiler drum fabricated of 18 cm (7 in.) thick ASTM A515, grade 70 steel plate failed during final hydrotesting at a pressure of approximately 26 MPa (3.8 ksi). The shock wave from the vessel rupture also damaged several connected headers and piping runs. A schematic of the crack path, including...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001818
EISBN: 978-1-62708-180-1
... inadvertently incorporated stress raisers from reaching service, but they occasionally do. Example 4: Failure of a Steam Accumulator Due to Lack of Complete Weld Penetration A 1.2-m (4-ft) OD ├Ś 4.3-m (14-ft) long steam accumulator, constructed with 10.3-mm ( 13 32 -in.) thick SA515-70 steel...