1-1 of 1 Search Results for

API J55

Sort by
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001020
EISBN: 978-1-62708-161-0
..., the specifications of the American Petroleum Institute (API) govern. Table 3 lists the current ASTM, API, and Canadian Standards Association (CSA) specifications covering pipe. Some of these involve several grades. The specifications listed cover carbon and alloy steels other than stainless, all methods...