1-20 of 275 Search Results for

AISI-SAE designations

Sort by
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0006000
EISBN: 978-1-62708-168-9
... Abstract This article is a compilation of tables that present information on cross-referencing of steel designations that are followed in France, Germany, Italy, Japan, Sweden, and Britain to AISI/SAE. cross reference steel Cross Reference of Steels to AISI/SAE Designations Cross...
Book Chapter

Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001030
EISBN: 978-1-62708-161-0
... for Forging; Hot Rolled Bars and Cold Finished Bars, Hot Rolled Deformed and Plain Concrete Reinforcing Bars,” Steel Products Manual, American Iron and Steel Institute , March 1986 SAE/AISI 1038H UNS H10380. Heat-treating temperatures recommended by SAE Normalize (for forged or rolled specimens...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003092
EISBN: 978-1-62708-199-3
... ranges, and product analysis tolerances of carbon and alloy steels. The major designation systems discussed include the Society of Automotive Engineers (SAE)-American Iron and Steel Institute (AISI) designations, Unified Numbering System (UNS) designations, American Society for Testing and Materials...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005949
EISBN: 978-1-62708-168-9
... on the steel compositions within the North American AISI-SAE system ( Tables 4 , 5 , 6 , 7 , 8 ). The first four digits of the UNS designations usually correspond to the standard AISI-SAE designations, while the last digit (other than zero) denotes some additional composition requirement such as lead...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001009
EISBN: 978-1-62708-161-0
... are by far the most frequently used steel. Tables 9 and 10 indicate that more than 85% of the steel produced and shipped in the United States is carbon steel. Chemical compositions for carbon steels are provided in the tables referenced in the section “SAE-AISI Designations” in this article. See...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001038
EISBN: 978-1-62708-161-0
... than about 10,000 cycles to failure), the second term dominates, and the fatigue behavior is adequately described by Eq 7 . Thus, it becomes possible to use Eq 7 in stress-based analysis and design. Fig. 12 Total strain versus fatigue life for annealed AISI-SAE 4340 steel. Data are same...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001013
EISBN: 978-1-62708-161-0
... fabrication issues, including formability, machinability, and weldability. AISI-SAE designations ASTM specifications chemical composition composition limits regular quality standards and grades steel plate structural quality UNS designations STEEL PLATE is any flat-rolled steel product more...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001014
EISBN: 978-1-62708-161-0
.... Hot-rolled alloy steel bars are covered by several ASTM specifications ( Tables 3 and 4 ). Many of the alloys covered in these specifications are standard AISI-SAE grades ( Table 5 ). AISI-SAE grades of hot-rolled alloy steel bars in ASTM specifications Table 5 AISI-SAE grades of hot-rolled...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005998
EISBN: 978-1-62708-168-9
...-grades. However, the graphs are not used for specification purposes. Hardenability bands of alloy steel Table 1 Hardenability bands of alloy steel AISI-SAE C Mn Si Ni Cr Mo Temperature Normalizing Austenitizing °C °F °C °F 1330H 0.27 to 0.33 1.45 to 2.05 0.20 to 0.35...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.9781627081689
EISBN: 978-1-62708-168-9
Series: ASM Handbook Archive
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000606
EISBN: 978-1-62708-181-8
... Classic bending overload fracture of automotive axle shaft (direct-on bearing design). Material and heat treatment: modified AISI 1050, induction hardened and tempered to 60 HRC at the bearing diameter. The part was broken in the laboratory. Fig. 228 : Fracture surface with chevrons in case-hardened zone...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002178
EISBN: 978-1-62708-188-7
... (in./rev) Tool material, grade, ISO (C) Speed, m/min (sfm) Feed, mm/rev (in./rev) Tool material, ISO (AISI) Brazed Indexable Ferritic gray irons: ASTM A48, class 20; SAE J431c, grade G1800 120–150 Annealed 1 (0.040) 56 (185) 0.18 (0.007) S4, S5 (M2, M3) 200 (650) 220 (725) 0.25 (0.010...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001018
EISBN: 978-1-62708-161-0
... specifications are necessary as a guide to proper design, application and installation. All American Society for Testing and Materials (ASTM) and Society of Automotive Engineers (SAE) specifications covering threaded fasteners require that the fastener be marked for grade identification ( Table 1 ). Grade...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001809
EISBN: 978-1-62708-180-1
... are of two types: tin-base with 4 to 8% Cu and 4 to 8% Sb (SAE 11 and 12; ASTM B23, grades 1, 2, 3, and 11) and lead-base with a maximum of 10.7% Sn and 9.5 to 17.5% Sb (SAE 13–16; ASTM B23, grades 7, 8, 13, and 15). These babbitts generally cause the least damage to steel shafts when operated...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003099
EISBN: 978-1-62708-199-3
... or section size applicability. SCM420 and 20MnCr5 are Japanese and German grades, respectively, found in carburized bearing components. In addition to standard SAE-AISI grades, bearing steels can also be designed so that their hardenability matches the requirements of specific section thicknesses. Alloy...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005631
EISBN: 978-1-62708-174-0
... Butt 15.9 0.625 12.0 Butt 12.7 0.50 12.0 Butt 9.5 0.375 10.8 Tee 9.5–12.7 0.375–0.5 11.9 Low-alloy carbon steel Tee 9.5–12.7 0.375–0.5 7.5 AISI 1010 Beam plate 4 0.157 1.8 (a) AISI 4130 Butt 15.2 0.60 14 Low-alloy high-strength steel, 300M Butt 19.0 0.75...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005947
EISBN: 978-1-62708-166-5
...-hardened disc with a hole (SAE 5120; 120 mm diameter by 45 mm diameter by 15 mm, or 5 in. diameter by 2 in. diameter by 0.6 in.). Besides tilting of the complete disc, additional effects occur near the bore and the outer lateral surface. These shape changes are unavoidable and are discussed later...
Book Chapter

Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005999
EISBN: 978-1-62708-168-9
... Abstract This article contains a table that presents information on cross-references to standard SAE carbon and low-alloy steel grades to selected chemically similar steels. alloy steel carbon steel AISI/SAE to Other Designations Cross-references to standard SAE carbon and low...
Series: ASM Handbook Archive
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0005697
EISBN: 978-1-62708-181-8
..., Metallurgical and Petroleum Engineers AISI American Iron and Steel Institute AMS Aerospace Material Specification (of SAE) ANSI American National Standards Institute API American Petroleum Institute ASME American Society of Mechanical Engineers ASTM American Society for Testing and Materials at.% atomic percent...
Series: ASM Handbook Archive
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.9781627081818
EISBN: 978-1-62708-181-8