... thermal treatments are more typically used to stabilize properties that could otherwise change over long periods of time. Representative 5 xx.x alloys of interest include: 512.0.0-F 513.0.0-F 514.0.0-F 520.0.0-T4 535.0.0-F Aluminum-Zinc-Magnesium (7xx.x) Most alloys...