1-20 of 23 Search Results for

99.90 Sn

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006278
EISBN: 978-1-62708-169-6
... Phosphorus-deoxidized arsenical (DPA) copper 99.68 Cu, 0.3 As, 0.02 P … … C14300 Cadmium-copper, deoxidized 99.9 Cu, 0.1 Cd … … C14310 Cadmium-copper, deoxidized 99.8 Cu, 0.2 Cd … … C14410 … 99.90 Cu, 0.15 Sn, 0.012 P … … C14415 … 99.96 Cu, 0.12 Sn … … C14420 … 99.90 Cu (d...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003131
EISBN: 978-1-62708-199-3
... classification of copper alloys Generic name UNS No. Composition Wrought alloys Coppers C10100-C15760 >99% Cu High-copper alloys C16200-C19600 >96% Cu Brasses C20500-C28580 Cu-Zn Leaded brasses C31200-C38590 Cu-Zn-Pb Tin brasses C40400-C49080 Cu-Zn-Sn-Pb Phosphor...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003146
EISBN: 978-1-62708-199-3
... … 0.002 0.002 99.90 min 0.002 Sb + As + Sn (a) Compositions are maximums unless a range or minimum (min) is specified. Commercially pure grades in strip, sheet, or plate product forms are covered in ASTM B 749. Composition limits for the five grades covered in this standard are given...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003772
EISBN: 978-1-62708-177-1
... Admiralty, arsenical 71.5 Cu, 27.5 Zn, 1 Sn, (0.04 As) C44400 Admiralty, antimonial 71.5 Cu, 27.5 Zn, 1 Sn, (0.06 Sb) C44500 Admiralty, phosphorized 71.5 Cu, 27.5 Zn, 1 Sn, (0.06 P) C46400 Uninhibited naval brass 61 Cu, 38 Zn, 1 Sn C48500 High-leaded naval brass 60.5 Cu, 1.75 Pb, 0.75...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001078
EISBN: 978-1-62708-162-7
... protection anode alloy (2.0% Ag, 98% Pb) L50140 Solder alloys (1.0–1.5% Ag, 1.0 Sn, bal Pb) L50121, L50131 Solder alloys (1.5–2.5% Ag, with no tin) L50132, L50150, L50151 Solder alloy (1.5% Ag, 5.0% Sn, 93.5% Pb) L50134 Solder alloy (2.5% Ag, 2.0% Sn, 95.5% Pb) L50152 Solder alloy (5.0...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001065
EISBN: 978-1-62708-162-7
... 57–1 20 C16500 98.6 Cu, 0.8 Cd, 0.6 Sn F, R, W 276–655 40–95 97–490 14–71 53–1.5 20 C17000 (beryllium-copper) 99.5 Cu, 1.7 Be, 0.20 Co F, R 483–1310 70–190 221–1172 32–170 45–3 20 C17200 (beryllium-copper) 99.5 Cu, 1.9 Be, 0.20 Co F, R, W, T, P, S 469–1462 68–212 172...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001077
EISBN: 978-1-62708-162-7
... of slab zinc (ASTM B 6) Grade UNS number Composition, % Pb Fe max Cd max Al max Cu max Sn max Total nonzinc max Zn min by difference Special high grade Z13001 0.003 max 0.003 0.003 0.002 0.002 0.001 0.010 99.990 High grade Z15001 0.03 max 0.02 0.02 0.01 … … 0.10...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005143
EISBN: 978-1-62708-186-3
..., 2.35 Fe, 0.125 Zn, 0.05 P C19500 Iron-cobalt-bearing copper 97 (min) Cu, l.5 Fe, 0.18 P, 0.8 Co, 0.6 Sn C19700 … 99 (min) Cu, 0.6 Fe, 0.2 P, 0.05 Mg Wrought brass alloys C21000 Gilding metal, 95% bal Cu, 5 Zn C22000 Commercial bronze, 90% bal Cu, 10 Zn C23000 Red brass, 85...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003210
EISBN: 978-1-62708-199-3
... Car radiators, heat exchangers, honeycomb aircraft structures, structural parts 2 Cu-X, solid solution Cu-Zn, peritectic Cu-Sn, peritectic BCu RBCuZn None Preforms, wire, rods, foil, powder, RS foil Copper and copper alloys, copper to mild steel, copper to stainless steel Heat exchangers...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003144
EISBN: 978-1-62708-199-3
... agent in chemical processes, and as a common additive in the production of rubber products. Grades and compositions of slab zinc (ASTM B 6) Table 1 Grades and compositions of slab zinc (ASTM B 6) Grade UNS No. Composition, % Pb Fe max Cd max Al max Cu max Sn max Total nonzinc max...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001438
EISBN: 978-1-62708-173-3
... groups. These major groups are: Coppers , which contain a minimum of 99.3% Cu High-copper alloys , which contain up to 5% alloying elements Copper-zinc alloys (brasses) , which contain up to 40% Zn Copper-tin alloys (phosphor bronzes) , which contain up to 10% Sn and 0.2% P Copper...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001058
EISBN: 978-1-62708-162-7
... A98079 … 0.05–0.30 0.7–1.3 0.05 … … … … 0.10 … … … … 0.05 0.15 rem 8280 A98280 … 1.0–2.0 0.7 0.7–1.3 0.10 … … 0.20–0.7 0.05 … … 5.5–7.0 Sn 0.10 0.05 0.15 rem 8081 A98081 … 0.7 0.7 0.7–1.3 0.10 … … … 0.05 … … 18.0–22.0 Sn 0.10 0.05 0.15 rem 8090...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001439
EISBN: 978-1-62708-173-3
... ASTM UNS No. Si Ag Cd Ni Pb Other Each Total 9980A M19980 … … … 0.001 0.01 0.01 Sn 0.05 … 99.80 min 9980 B M19981 … … … 0.005 0.01 0.01 Sn 0.05 … 99.80 min 9990A M19990 0.005 … 0.0001 0.001 … 0.00007 B 0.01 … 99.90 min 9990B M19991 0.005...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003123
EISBN: 978-1-62708-199-3
... 0.7 0.7–1.3 0.10 … … 0.20–0.7 0.05 … … 5.5–7.0 Sn 0.10 0.05 0.15 bal 8081 0.7 0.7 0.7–1.3 0.10 … … … 0.05 … … 18.0–22.0 Sn 0.10 0.05 0.15 bal 8090 0.20 0.30 1.0–1.6 0.10 0.6–1.3 0.10 … 0.25 … … 0.04–0.16 Zr (hh) 0.10 0.05 0.15 bal (a) 0.0008...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002185
EISBN: 978-1-62708-188-7
... No. Alloy name Nominal composition, % Machinability (a) Cu Ni Zn Pb Sn Group 1: free-cutting alloys C17300 Beryllium copper 97.50 (0.2 min, Ni + Co) (1.9 Be) 0.4 … 50 C18700 Leaded copper 99.00 … … 1.00 … 80 C14500 Tellurium copper 99.40 (0.50 Te) 80 C33000...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001067
EISBN: 978-1-62708-162-7
... specifications: Rod, MIL-C-12166; wire, MIL-W-3318, MIL-W-6712 Chemical Composition Composition Limits 99.90 Cu min (silver counted as copper) Silver Silver has little effect on mechanical and electrical properties, but does raise the recrystallization temperature and tends to produce a fine...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003082
EISBN: 978-1-62708-199-3
...-2Zn 11 15 Electrical contact materials Copper alloys 0.04 oxide 100 1.72 1.25 Sn + P 48 3.6 5 Sn + P 18 11 8 Sn + P 13 13 15 Zn 37 4.7 20 Zn 32 5.4 35 Zn 27 6.4 2 Be + Ni or Co (b) 17–21 9.6–11.5 Silver and silver alloys Fine silver 104...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003181
EISBN: 978-1-62708-199-3
.... Spinodal and/or precipitation hardening is available in the Cu-Ni-Sn and Cu-Ni-Cr systems. Hardening by martensite transformation is available in the copper-aluminum system, but is rarely used commercially. Copper alloys are classified using the Unified Numbering System (UNS). The designations...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.9781627081627
EISBN: 978-1-62708-162-7
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003206
EISBN: 978-1-62708-199-3