1-20 of 22 Search Results for

5xxx series aluminum alloys

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006707
EISBN: 978-1-62708-210-5
...Abstract Abstract This article provides an overview of key metallurgy, properties, and applications of the non-heat-treatable 5xxx series of aluminum alloys. It also shows the relationships between some of the more commonly used alloys in the 5xxx series. 5xxx series aluminum alloys...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006545
EISBN: 978-1-62708-210-5
... on statically loaded precracked samples, and tests using slowly straining samples. The article describes SCC susceptibility and ratings of SCC resistance for high-strength wrought aluminum products, such as 2xxx, 5xxx, and 7xxx series alloys, aluminum-lithium alloys, and 7xxx alloys containing copper...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003618
EISBN: 978-1-62708-182-5
...Abstract Abstract This article provides an overview of the metallurgical effects on corrosion of different series of aluminum alloys (1xxx, 2xxx, 3xxx, 4xxx, 5xxx, 6xxx, and 7xxx) that are classified into two categories. The first category includes the effects from insoluble, intermetallic...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006694
EISBN: 978-1-62708-210-5
...Abstract Abstract The general-purpose alloy 5050 is a binary aluminum-magnesium alloy with more magnesium content than 5005. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of this 5xxx series...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006581
EISBN: 978-1-62708-210-5
... physical properties The 511.0, 512.0 and 513.0 alloys ( Table 1 ) are variations of alloy 514.0. As part of the 5xxx series, they are essentially single-phase binary alloys. Their most important characteristic is corrosion resistance, including exposure to seawater and marine atmospheres. The Al-Mg...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006693
EISBN: 978-1-62708-210-5
... product specifications, processing effects on physical and mechanical properties, and fabrication characteristics of this 5xxx series alloy. aluminum alloy 5005 aluminum mill products architectural sheet corrosion-resistant siding materials fabrication characteristics mechanical properties...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006696
EISBN: 978-1-62708-210-5
...Abstract Abstract Alloy 5056 can be used for nails and for redrawing rod to make wire. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of this 5xxx series alloy. aluminum alloy 5056...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006701
EISBN: 978-1-62708-210-5
...Abstract Abstract Alloy 5254 is a higher-purity Al-Mg-Cr alloy used in heat exchangers, steam-jacketed kettles, and pumps. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of this 5xxx series...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006697
EISBN: 978-1-62708-210-5
... on physical and mechanical properties, and applications of this 5xxx series alloy. aluminum alloy 5083 fabrication characteristics mechanical properties moderate-strength weldable alloys physical properties Alloy 5083 is among the most widely used shipyard alloys (along with 5086 and 5456...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003664
EISBN: 978-1-62708-182-5
... alloys to IGA. It describes the most serious forms of structure-dependent corrosion, such as stress-corrosion cracking and exfoliation, in aluminum alloys including strain-Hardened 5xxx (Al-Mg) alloys and heat treated high-strength alloys. The article concludes with information on the evaluation tests...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002406
EISBN: 978-1-62708-193-1
...: the second letter is the direction of crack growth. L, longitudinal; T, transverse; S, thickness direction Tough aluminum alloys such as those from the 1XXX, 3XXX, 4XXX, 5XXX, and most 6XXX series do not normally exhibit elastic unstable fracture, either in test panels or in real structures...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006527
EISBN: 978-1-62708-207-5
... , 12 . For comparison, typical forming limit diagrams for different sheet metals are shown in Fig. 13 . Fig. 10 Forming-limit diagrams for two 3xxx-series aluminum alloys. Source: Ref 36 Fig. 11 Forming-limit diagrams for four 5xxx-series aluminum alloys. Source: Ref 36...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006522
EISBN: 978-1-62708-207-5
... and alloy designation (wrought and cast) Maximum solid solubility, wt% Solubility at room temperature, wt% Copper, 2XXX series, 3XX series 5.65 at 548 °C (1020 °F) 0.02 Magnesium, 5XXX and 6XXX series, 5XX series 14.9 at 451 °C (845 °F) 2.50 Manganese, 3XXX series 1.82 at 657 °C (1215 °F...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006702
EISBN: 978-1-62708-210-5
... and mechanical properties, and fabrication characteristics of this 5xxx series alloy. aluminum alloy 5454 aluminum-magnesium-manganese-chromium solid solution alloys chemical and process industries chemical handling fabrication characteristics mechanical properties physical properties...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006546
EISBN: 978-1-62708-210-5
.... aluminum alloy ratings aluminum alloys cladding corrosion corrosion data corrosion properties surface treatments weathering data ALUMINUM, as indicated by its position in the electromotive force series, is a thermodynamically reactive metal; among structural metals, only beryllium and magnesium...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006529
EISBN: 978-1-62708-207-5
..., and joinability of select aluminum alloys Table 2 Characteristics, applications, and joinability of select aluminum alloys Series Alloys Major features Applications Joining 1xxx Al Commercially pure 1100 (99.00% min Al) 1050 (99.50% min Al) 1350 (99.50% min Al) 1175 (99.75% min Al) High...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
.... Performance of Alloy Groupings Magnesium Magnesium occupies an extremely active position in most galvanic series and is therefore highly susceptible to galvanic corrosion. Metals that combine active potentials with higher hydrogen overvoltages, such as aluminum, zinc, cadmium, and tin, are much less...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006503
EISBN: 978-1-62708-207-5
... with a metal matrix as solute atoms that differ from the matrix atoms in size and/or shear modulus, which can cause a variation of strain fields. The principal alloys that are strengthened by alloying elements in solid solution (often coupled with cold work) are those in the aluminum-magnesium (5 xxx ) series...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006698
EISBN: 978-1-62708-210-5
... specifications, and fabrication characteristics of this 5xxx series alloy. corrosion resistance fabrication characteristics marine environment moderate-strength weldable alloy 5086 physical properties tensile properties Alloy 5086 provides higher strength than alloy 5052 while maintaining good...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005637
EISBN: 978-1-62708-174-0
... a fusion-based process where a filler metal is used for joining. The approach, although applicable to a wide variety of commercial alloys, has its own specific limitations due to the nature of the process. As an example, high-strength precipitation-strengthened aluminum alloys are nonweldable by fusion...