Published: 01 January 1996
Fig. 13 Crack propagation rates in stress corrosion tests using precracked specimens of high-strength 2XXX series aluminum alloys, 25 mm thick, double cantilever beam, TL(S-L) orientation of plate, wet twice a day with an aqueous solution of 3.5% NaCl, 23 °C More
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006594
EISBN: 978-1-62708-210-5
... Abstract This article illustrates the relationships among commonly used 2xxx series alloys. It contains tables that list values for composition limits of aluminum-lithium alloys, and aerospace alloys and their temper conditions according to primary design requirements. 2xxx series...
Image
Published: 01 January 1996
Fig. 5 Relationships of plane-strain fracture toughness to yield strength for the 2XXX and 7XXX series of aluminum alloys. Source: R. Develay, Metals and Materials, Vol 6, 1972, p 404 More
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006555
EISBN: 978-1-62708-210-5
... metallurgy and fabrication characteristics of these 2xxx series alloys, as well as the effects of processing on their typical physical and mechanical properties. aerospace applications aluminum alloy 206.0 aluminum alloy A206.0 aluminum alloy B206.0 automotive applications cast aluminum alloys...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004015
EISBN: 978-1-62708-185-6
... Abstract Aluminum and aluminum alloys are very suitable for extrusion and many types of profiles can be produced from easily extrudable alloys. This article lists the basic characteristics of aluminum and its alloys. It tabulates the aluminum extrusion alloys by series and lists the typical...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006726
EISBN: 978-1-62708-210-5
... of the 7xxx aluminum alloy. It also illustrates the natural aging characteristics of 7050 aluminum sheet alloys at room temperature and relationships among commonly used alloys in the 7xxx series. 7xxx series aluminum alloys aging characteristics aluminum sheet alloys datasheets precipitation...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006545
EISBN: 978-1-62708-210-5
... on statically loaded precracked samples, and tests using slowly straining samples. The article describes SCC susceptibility and ratings of SCC resistance for high-strength wrought aluminum products, such as 2xxx, 5xxx, and 7xxx series alloys, aluminum-lithium alloys, and 7xxx alloys containing copper...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006557
EISBN: 978-1-62708-210-5
... characteristics, and applications of this 2xxx series alloy. aluminum alloy 238.0 cast aluminum-copper-silicon alloys fabrication characteristics general purpose casting alloys hardness machinability Alloy 238.0 is a standard general purpose Al-Si-Cu alloy ( Table 1 ) used for high hardness...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003618
EISBN: 978-1-62708-182-5
... Abstract This article provides an overview of the metallurgical effects on corrosion of different series of aluminum alloys (1xxx, 2xxx, 3xxx, 4xxx, 5xxx, 6xxx, and 7xxx) that are classified into two categories. The first category includes the effects from insoluble, intermetallic constituent...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006600
EISBN: 978-1-62708-210-5
... information on key alloy metallurgy and processing effects on mechanical properties of plate and extrusions of this 2xxx series alloy. aerospace plate alloys aluminum alloy 2027 aluminum-copper-magnesium-manganese-zirconium alloys damage tolerance alloy plates extrusion alloys mechanical properties...
Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006603
EISBN: 978-1-62708-210-5
... Abstract The Al-Cu-Li alloy 2050 was designed to replace 2xxx alloys at low thicknesses and 7xxx alloys on the thicker end of the range. This datasheet provides information on key alloy metallurgy and processing effects on mechanical properties of this 2xxx series alloy. A figure presents...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006613
EISBN: 978-1-62708-210-5
... as the effects of processing on mechanical properties of this 2xxx series alloy. A comparison of fracture toughness of 2324-T39 to 2024-T351 is presented. alloy composition aluminum alloy 2024-T351 aluminum alloy 2324 aluminum alloy 2324-T39 extrusions fracture toughness high-strength alloy plate...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006612
EISBN: 978-1-62708-210-5
... Abstract Alloys 2297 and 2397 were developed for thick plate integral structures. This datasheet provides information on composition limits of these 2xxx series alloys and processing effects on mechanical properties of alloy 2297-T87 plate. A figure provides a performance comparison of 2297-T87...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002406
EISBN: 978-1-62708-193-1
... Fig. 5 Relationships of plane-strain fracture toughness to yield strength for the 2XXX and 7XXX series of aluminum alloys. Source: R. Develay, Metals and Materials, Vol 6, 1972, p 404 The strength-fracture toughness interaction has been postulated to be the consequence of void link-up...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004127
EISBN: 978-1-62708-184-9
..., formability, and cost, during development of aircraft weapon systems. The most widely used materials in airframe structures and components are aluminum, steel, titanium, and magnesium alloy systems. Aluminum Alloys With the exception of magnesium, aluminum by its position in the electrochemical series...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006520
EISBN: 978-1-62708-207-5
... Abstract This article summarizes a typical solution and aging heat treatments of 2xxx (Al-Cu), 6xxx (Al-Mg-Si), and 7xxx (Al-Zn-Mg) wrought alloys. It discusses the general aging characteristics and the effects of reheating of aluminum alloys. Typical examples of hardness and conductivity...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006546
EISBN: 978-1-62708-210-5
... ratings aluminum alloys cladding corrosion corrosion data corrosion properties surface treatments weathering data ALUMINUM, as indicated by its position in the electromotive force series, is a thermodynamically reactive metal; among structural metals, only beryllium and magnesium are more...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006522
EISBN: 978-1-62708-207-5
...) 0.30 Silicon, 4XXX and 6XXX series, 4XX series 1.65 at 577 °C (1035 °F) 0.10 Zinc, 7XXX series 82.8 at 382 °C (720 °F) 2.00 Source: Ref 13 Because of the passive nature of aluminum, aluminum alloys typically exhibit good corrosion resistance. However, as alloy properties change...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006558
EISBN: 978-1-62708-210-5
... characteristics of these 2xxx series alloys. age-hardenable casting alloys aluminum alloy 242.0 aluminum alloy A242.0 fabrication characteristics mechanical properties physical properties Alloys 242.0 and A242.0 are age-hardenable casting alloys containing copper, nickel, and magnesium ( Table 1...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006605
EISBN: 978-1-62708-210-5
... Abstract The aerospace extrusion alloy 2065 has excellent corrosion resistance compared with high-strength 7xxx alloys. This datasheet provides information on key alloy metallurgy and processing effects on density and mechanical properties of this 2xxx series alloy. aerospace extrusion...