EISBN: 978-1-62708-199-3
... and lead-base alloys grouped according to nominal chemical composition. The properties of lead that make it useful in a wide variety of applications are also discussed. The largest use of lead is in lead-acid storage batteries. Other applications include ammunition, cable sheathing, cast products...
Book Chapter

By Donald Wetzel
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001272
EISBN: 978-1-62708-170-2
... cascara extract Creosote (a) And other unspecified titanates. Source: Ref 2 Fig. 3 Effect of pH on corrosion of zinc. Source: Ref 1 Metallurgical Characteristics of Galvanized Coatings Iron and Steel Substrates The chemical composition of irons and steels, and even...