Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 142
Carbon-carbon composites
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.9781627081955
EISBN: 978-1-62708-195-5
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003414
EISBN: 978-1-62708-195-5
Abstract
Vacuum infusion is a resin injection technique derived from resin transfer molding. This article discusses the characteristics of the technique and its applications. It presents the theory and background of the technique and provides an illustration of how parts are made. The article provides information on the equipment and material used for vacuum infusion. It describes the mechanical properties of components and summarizes the influence of production on the properties. The article concludes with a discussion on design guidelines.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003467
EISBN: 978-1-62708-195-5
Abstract
This article describes the results of several case history studies of the failure of polymer-matrix composite components to provide not only some representative types of failures that can encounter, but also to provide some insight into the investigative process. These case histories deal mainly with structures that exhibit an initial material and/or manufacturing defect or failures that are most prevalent and most easily solved. The components include helicopter rotor blade, composite wing spar, and aircraft rudder.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003481
EISBN: 978-1-62708-195-5
Abstract
This article provides information on the potential applications of fiber-reinforced polymer (FRP) composites for maritime craft and offshore drilling platforms. The key benefits gained from using FRP materials together with an examination of the drawbacks and major issues impeding the more widespread use of composites in marine structures are presented.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003386
EISBN: 978-1-62708-195-5
Abstract
This article addresses the issue of the implementation of composite damage tolerance requirements as it relates to military aircraft. It presents a brief introduction on the durability impact threat, damage tolerance impact threat, and other damage tolerance damage threats. The article summarizes damage tolerance criteria and durability criteria for military aircraft. It discusses the damage tolerance design philosophy for metallic structures and composite structures of the aircraft. The article describes the implementation of a damage tolerance analysis methodology in terms of the mechanics based model, the regression algorithm, and the semi-empirical analysis.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003447
EISBN: 978-1-62708-195-5
Abstract
This article discusses the materials and properties of polymer-matrix composites to characterize each generic material according to its composition and method of manufacture. It contains a table that lists the key physical, mechanical, thermal, and electrical properties, and in-service conditions of concern for resin-matrix composites. Axes definitions, symbols, and special property calculations for composite material property tests are reviewed. The article provides an overview of the performance capabilities of selected polymer-matrix composite materials such as thermoplastic-matrix composites and thermoset-matrix composites. The thermoplastic-matrix composites include thermoplastic polyester resins and fiber resin composites; thermoplastic polyamide resins and fiber-resin composites; and thermoplastic polysulfone resins and fiber-resin composites.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003468
EISBN: 978-1-62708-195-5
Abstract
This article describes the fatigue properties of particle-reinforced metal-matrix composites (PR-MMCs) in terms of mechanisms of crack initiation, fatigue life, and fatigue crack growth. It reviews specimen preparation and microscopic procedures that are used in fatigue testing of MMCs. It also describes the evaluation of the long fatigue crack growth behavior of MMCs by using the test methods and specimens that are used for unreinforced metallic alloys. Fractography of MMCs under plane-strain conditions is also described with information on the observed features of MMC fatigue fracture surfaces and their observation methods.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003387
EISBN: 978-1-62708-195-5
Abstract
This article discusses the methods of analyzing the directional dependence of the mechanical properties of composites, especially those perpendicular to the major plane of the laminate. It provides a description of the common indirect load cases and direct out-of-plane load cases. The article concludes with a discussion on composite materials that are reinforced in the z-direction (also known as three-dimensional, or 3-D composites).
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003482
EISBN: 978-1-62708-195-5
Abstract
Composites, particularly fiber-reinforced polymer materials, are increasingly being adopted or considered as alternatives to conventional materials for civil infrastructure applications, such as bridges, buildings, waterfront structures, waste treatment facilities, and facilities for transmission and transport of utilities. This article provides information on seismic retrofit applications and discusses the repair and strengthening of components, such as beams, slabs, large-diameter pipes, and bridge decks.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003427
EISBN: 978-1-62708-195-5
Abstract
This article focuses on the factors to be considered for selecting fasteners for joining carbon fiber composites. These considerations include corrosion compatibility, fastener materials, strength, stiffness, head configurations, importance of clamp-up, hole fit, and lightning protection.
Book Chapter
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003378
EISBN: 978-1-62708-195-5
Abstract
The properties of unidirectional composite (UDC) materials are quite different from those of conventional, metallic materials. This article provides information on the treatment of UDC stress-strain relations in the forms appropriate for analysis of thin plies of material. It explains the development of the relations between mid-surface strains and curvatures and membrane stress and moment resultants. The article discusses the properties, such as thermal expansion, moisture expansion, and conductivity, of symmetric laminates and unsymmetric laminates. It describes the distribution of temperature and moisture through the thickness of a laminate. Stresses caused due to mechanical loads, temperature, and moisture on the laminate are analyzed. The article concludes with information on interlaminar cracking, free-edge delamination, and transverse cracks of laminates.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003469
EISBN: 978-1-62708-195-5
Abstract
Interpretation of failures of ceramic-matrix composites, and in particular continuous fiber reinforced ceramic-matrix composites is complicated by the complex structure of the composite material. This article describes the failure characteristics and evidence of failure mechanisms of these composites, with illustrations.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003486
EISBN: 978-1-62708-195-5
Abstract
The applications of discontinuously reinforced ceramic-matrix composites (CMCs) fall into four major categories, namely, cutting tool inserts; wear-resistant parts; aerospace and military applications; and other industrial applications, including engines and energy-related applications. This article provides examples for these four categories, with an emphasis on those applications/materials that have achieved commercial viability. The applications for continuous fiber ceramic composites are also summarized.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003470
EISBN: 978-1-62708-195-5
Abstract
This article provides an introduction to the concepts discussed in the articles under the Section “Recycling and Disposal of Composites” in ASM Handbook, Volume 21: Composites. This Section presents the reader the most recent developments in the open-and closed-loop recycling of polymer and metal matrix composites.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003448
EISBN: 978-1-62708-195-5
Abstract
Metal-matrix composites (MMCs) are used in structural applications, and in applications requiring wear resistance, thermal management, and weight savings. This article summarizes the mechanical and thermal properties of discontinuously reinforced aluminum MMCs, laminated metallic composites, and continuously aligned fiber reinforced MMCs.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003484
EISBN: 978-1-62708-195-5
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003428
EISBN: 978-1-62708-195-5
Abstract
Environmental effects of ground and flight environments, including temperature extremes, damage by chemical fluids, moisture, and so forth, affect the durability of polymer-matrix composites. This article provides information on corrosion control methods in aircraft structures. It discusses the design considerations for sealants in joints. The article describes the common methods to seal aircraft structures: fay surface, fillet, butt joint, channel, brush, and form-in-place seals. It discusses the surface preparation and application method of primer and topcoat systems. Primer and paint application equipment as well as sealant application equipment are reviewed.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003449
EISBN: 978-1-62708-195-5
Abstract
This article discusses the mechanisms for enhancing the reliability of three types of ceramic-matrix composites: discontinuously reinforced ceramic-matrix composites, continuous fiber ceramic composites, and carbon-carbon composites. It also presents examples of their mechanical and physical properties. Examples that illustrate the properties of commercially available materials are also provided.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003388
EISBN: 978-1-62708-195-5
Abstract
A sandwich structure is comprised of layered composite materials formed by bonding two or more thin facings or facesheets to a relatively thick core material. This article describes the sandwich panel failure modes. It tabulates the nomenclature and definitions for loads, geometry, and material properties. The article illustrates critical strength-check locations for a flat sandwich panel. It discusses the analysis methods formulated for flat rectangular honeycomb panels; curved sandwich panel; and for each of the various sandwich panel failure modes. The article concludes with a discussion on flat panel stability analysis methods.
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003485
EISBN: 978-1-62708-195-5
Abstract
The primary motivation for the insertion of metal-matrix composites (MMCs) into aeronautical systems is the excellent balance of specific strength and stiffness offered by MMCs. This article provides information on the aerostructural, aeropropulsion, and aeronautical subsystem applications of MMCs. The applications include ventral fin, fuel access door covers, helicopter blade sleeve, fan exit guide vane, nozzle actuator piston rod, nozzle actuator links, T-1 racks, and hydraulic manifold.