Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-2 of 2
Enthalpy
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005189
EISBN: 978-1-62708-187-0
Abstract
This article introduces the fundamental concepts of chemical thermodynamics and chemical kinetics in describing presolidification phenomena. For metallurgical systems, the most important thermodynamic variables are enthalpy and Gibbs free energy. A qualitative demonstration of the interrelationship between phase diagrams and thermodynamics is presented. The article discusses processes that generally limit the rates of chemical processes. These include nucleation of the product phase and interphase mass transport. The article provides a discussion on the dissolution of alloy with melting point lower than bath temperature and dissolution of alloy that is solid at bath temperatures.
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005240
EISBN: 978-1-62708-187-0
Abstract
There are several main sources of thermophysical property data that provide the most authoritative and comprehensive compilations of critically and systematically evaluated data that are presently available. This article provides thermophysical property data to assist in the materials properties selection for the simulation of casting processes. The measurements of thermophysical property are difficult due to high temperatures and the reactivity of some alloys. The article discusses the strategies adopted to minimize the effects of high temperatures and reactivity of alloys. It presents the thermophysical properties of pure metals and some commercial alloys and tabulates the enthalpy of fusion and solidus and liquidus temperatures for various alloys of commercial interest. The article also lists the density, thermal conductivity, surface tension, and viscosity for some commercial alloys.