Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-3 of 3
Precision hot forging
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005144
EISBN: 978-1-62708-186-3
Abstract
In terms of forming, magnesium alloys are much more workable at elevated temperatures due to their hexagonal crystal structures. This article describes the deformation mechanisms of magnesium and provides information on the hot and cold forming processes of magnesium alloys and the lubricants used in the processes. It discusses the various forming processes of magnesium alloys. These include press-brake forming, deep drawing, manual and power spinning, rubber-pad forming, stretch forming, drop hammer forming, and precision forging.
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003975
EISBN: 978-1-62708-185-6
Abstract
This article addresses dies and die materials used for hot forging in vertical presses, hammers, and horizontal forging machines (upsetters). It reviews the properties of die materials for hot forging, including good hardenability, resistance to wear, plastic deformation, thermal fatigue, and mechanical fatigue. The article describes heat treating practices commonly employed for chromium- and tungsten-base AISI hot-work tool steels. It discusses the fabrication of impression dies, and the advantages and disadvantages of cast dies. The article concludes with a discussion on the factors that affect die life and safety precautions to be considered during die construction.
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003986
EISBN: 978-1-62708-185-6
Abstract
Precision forging is defined as a closed-die forging process in which the accuracy of the shape, dimensional tolerances, and surface finish exceed normal expectations to the extent that some of the postforge operations can be eliminated. This article provides an overview of the key factors that impact the precision forging process. It provides information on the achievable tolerances and presents examples of precision forging. A discussion on forging of bevel gears/spiral bevel gears is also presented.