Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-11 of 11
Submerged arc welding
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006391
EISBN: 978-1-62708-192-4
Abstract
Hardfacing refers to the deposition of a specially selected material onto a component in order to reduce wear in service as a preventative measure or return a worn component to its original dimensions as a repair procedure. This article provides information on various hardfacing materials, namely, iron-base overlays, chromium carbide-based overlays, nickel- and cobalt-base alloys, and tungsten carbide-based metal-matrix composite overlays. It discusses the types of hardfacing processes, such as arc welding processes, and laser cladded, oxyacetylene brazing and vacuum brazing processes. The arc welding processes include shielding metal arc welding, gas metal arc welding/flux cored arc welding, gas tungsten arc welding, submerged arc welding, and plasma transferred arc welding. The article also reviews various factors influencing the selection of the appropriate hardfacing for specific applications.
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006301
EISBN: 978-1-62708-179-5
Abstract
This article describes some examples of the different welding processes for gray, ductile, and malleable irons. These processes include fusion welding, repair welding, shielded metal arc welding, gas metal arc welding, flux cored arc welding, gas tungsten arc welding, submerged arc welding, oxyfuel welding, and braze welding. The article discusses various special techniques, such as groove-face grooving, studding, joint design modifications, and peening, for improving the strength of a weld or its fitness for service. The article describes other fusion welding methods such as electrical resistance welding and thermite welding. It reviews thermal spraying processes, such as flame spraying, arc spraying, and plasma spraying, of a cast iron.
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005566
EISBN: 978-1-62708-174-0
Abstract
Submerged arc welding (SAW) is suited for applications involving long, continuous welds. This article describes the operating principle, application, advantages, limitations, power source, equipment, and fluxes in SAW. It reviews three different types of electrodes manufactured for SAW: solid, cored, and strip. The article highlights the factors to be considered for controlling the welding process, including fit-up of work, travel speed, and flux depth. It also evaluates the defects that occur in SAW: lack of fusion, slag entrapment, solidification cracking, and hydrogen cracking. Finally, the article provides information on the safety measures to be followed in this process.
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005558
EISBN: 978-1-62708-174-0
Abstract
This article provides information on the various types of welds and joints. It reviews the weld joint design considerations: the ability to transfer load and the cost. The article explains the throat size and weld size requirements of fillet welds, and presents a comparison of fillet and groove welds. It details the various design considerations for groove-weld selection, including the groove angle, root opening, and depth of the groove. The article also describes the methods of edge preparation and concludes with an illustration of the recommended proportions of grooves for arc welding.
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005579
EISBN: 978-1-62708-174-0
Abstract
Fluid flow is important because it affects weld shape and is related to the formation of a variety of weld defects in gas tungsten arc (GTA) welds. This article describes the surface-tension-driven fluid flow model and its experimental observations. The effects of mass transport on arc plasma and weld pool are discussed. The article reviews the strategies for controlling poor and variable penetration and describes the formation of keyhole and fluid flow in electron beam and laser welds. It also explains the fluid flow in gas metal arc welding and submerged arc welding, presenting its transport equations.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001334
EISBN: 978-1-62708-173-3
Abstract
High-velocity gas motion occurs in and around the arc during welding. This article describes the phenomena of gas flow in gas tungsten arc welding (GTAW) and gas metal arc welding (GMAW). The effect of trace element impurities on GTA weld penetration of selected alloys is presented in a table. The article concludes with a discussion on submerged arc welding (SAW).
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001432
EISBN: 978-1-62708-173-3
Abstract
This article discusses the susceptibility of carbon steels to hydrogen-induced cracking, solidification cracking, lamellar tearing, weld metal porosity, and heat-affected zone (HAZ) mechanical property variations. The composition and mechanical properties of selected carbon steels used in arc welding applications are listed in a table. The article presents process selection guidelines for arc welding carbon steels. It provides information on the shielded metal arc welding, gas-metal arc welding, and flux-cored arc welding, gas-tungsten arc and plasma arc welding, submerged arc welding, electrogas welding, electroslag welding, and stud arc welding.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001359
EISBN: 978-1-62708-173-3
Abstract
Submerged arc welding (SAW) is an arc welding process in which the arc is concealed by a blanket of granular and fusible flux. This article provides a schematic illustration of a typical setup for automatic SAW and discusses the advantages and limitations and the process applications of SAW. The article discusses flux classification relative to production method, relative to effect on alloy content of weld deposit, and relative to basicity index. It describes the procedural variations and the effect of weld current, weld voltage, electrical stickout, travel speed, and flux layer depth on weld bead characteristics. The article concludes with information on weld defects, such as lack of fusion, slag entrapment, solidification cracking, hydrogen cracking, or porosity.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001339
EISBN: 978-1-62708-173-3
Abstract
Fluxes are added to the welding environment to improve arc stability, to provide a slag, to add alloying elements, and to refine the weld pool. This article describes the effect of oxygen that directly reacts with alloying elements to alter their effective role by reducing hardenability, promoting porosity, and producing inclusions. It proposes basicity index for welding as a measure of expected weld metal cleanliness and mechanical properties. The article discusses alloy modification in terms of slipping and binding agents, slag formation, and slag detachability. It reviews the types of fluxes for different arc welding processes, such as shielded metal arc welding (SMAW), flux-cored arc welding (FCAW), and submerged arc welding (SAW).
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001437
EISBN: 978-1-62708-173-3
Abstract
Nickel alloys can be joined reliably by all types of welding processes or methods, with the exception of forge welding and oxyacetylene welding. This article discusses the heat treatment of nickel alloys and tabulates nominal compositions of selected weldable wrought nickel and nickel alloys. It provides information on gas-tungsten arc welding, gas-metal arc welding, plasma arc welding, shielded metal arc welding, and submerged arc welding for welding nickel alloys. The article reviews the defects encountered in the arc welding of nickel alloys, including porosity, cracking, and stress-corrosion cracking. It provides information on the factors that influence the choice of filler metal and welding process of nickel alloys.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001438
EISBN: 978-1-62708-173-3
Abstract
Copper and copper alloys offer a unique combination of material properties that makes them advantageous for many manufacturing environments. This article begins with a discussion on common metals that are alloyed with copper to produce the various copper alloys. It then reviews the factors that affect the weldability of copper alloys, including thermal conductivity of the alloy being welded, shielding gas, type of current used during welding, joint design, welding position, and surface condition. The article provides information on arc welding processes such as gas-metal arc welding, shielded metal arc welding, submerged arc welding, plasma arc welding, and gas-tungsten arc welding. It concludes with a discussion on safe welding practices.