Skip Nav Destination
Close Modal
By
Joseph R. Pickens
By
S.L. Semiatin, J.J. Jonas
By
J.H. Miller, P.K. Liaw
By
John A. Bailey, Jamal Y. Sheikh-Ahmad
By
Howard A. Kuhn
By
Ralph S. Shoberg
By
Serope Kalpakjian
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-15 of 15
Torsion testing
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Useful Formulas for Metals Processing
Available to PurchaseSeries: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005542
EISBN: 978-1-62708-197-9
Abstract
This article is a comprehensive collection of tables containing formulas for metals processing, namely, casting and solidification, flat (sheet) rolling, conical-die extrusion, wire drawing, bending, and deep drawing. Formulas for compression, tension, and torsion testing of isotropic materials are included. The article also lists the formulas for effective stress, strain, and strain rate (isotropic material) in arbitrary and principal coordinates; dimensionless groups in fluid mechanics; and anisotropic sheet materials at various loading conditions.
Book Chapter
Useful Formulas for Deformation Analysis and Workability Testing
Available to PurchaseSeries: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005181
EISBN: 978-1-62708-186-3
Abstract
This article presents formulas for calculating the following: effective stress, strain, and strain rate (isotropic material) in arbitrary coordinates and in principal coordinates; compression testing, tension testing, and torsion testing of isotropic material; and Barlat's anisotropic yield function Yld2000-2d for plane-stress deformation of sheet material. It also contains formulas related to flat (sheet) rolling, conical-die extrusion, wire drawing, bending, and deep drawing of cups from sheet metal.
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0009007
EISBN: 978-1-62708-185-6
Abstract
This article discusses a number of workability tests that are especially applicable to the forging process. The primary tests for workability are those for which the stress state is well known and controlled. The article provides information on the tension test, torsion test, compression test, and bend test. It examines specialized tests including plane-strain compression test, partial-width indentation test, secondary-tension test, and ring compression test. The article explains that workability is determined by two main factors: the ability to deform without fracture and the stress state and friction conditions present in the bulk deformation process. These two factors are described and brought together in an experimental workability analysis.
Book Chapter
Hot Working Simulation by Hot Torsion Testing
Available to PurchaseSeries: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0009012
EISBN: 978-1-62708-185-6
Abstract
This article summarizes the types of hot working simulation tests such as hot tension, compression, and torsion testing used in the assessment of workability. It illustrates the use of hot torsion testing for the optimization of hot working processes. The article concludes with information on some hot torsion application examples.
Book Chapter
Torsion Testing to Assess Bulk Workability
Available to PurchaseSeries: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0009011
EISBN: 978-1-62708-185-6
Abstract
This article discusses the equipment design, procedures, experimental considerations, and interpretation of the torsion tests used to establish workability. It describes the application of torsion testing to obtain flow-stress data and to gage fracture-controlled workability and flow-localization-controlled failure. The article discusses the torsion test used to establish the processing parameters that are required to produce the desired microstructures.
Book Chapter
Fracture Toughness of Ceramics and Ceramic Matrix Composites
Available to PurchaseSeries: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003311
EISBN: 978-1-62708-176-4
Abstract
This article introduces the concepts of linear-elastic fracture mechanics (LEFM) and elastic-plastic fracture mechanics (EPFM). It reviews the fracture mechanics of ceramics and ceramic matrix composites (CMCs). The article describes some fracture toughness measurement techniques used on ceramics and CMCs: single edge notch bending, compact tension, double cantilever beam testing, chevron notch methods, and double torsion. It presents descriptions organized by their specimen types, and includes the advantages and disadvantages, as well as the experimental control schemes employed for each specimen type.
Book Chapter
Fundamental Aspects of Torsional Loading
Available to PurchaseSeries: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003263
EISBN: 978-1-62708-176-4
Abstract
Torsion tests can be carried out on most materials, using standard specimens, to determine mechanical properties such as modulus of elasticity in shear, yield shear strength, ultimate shear strength, modulus of rupture in shear, and ductility. This article discusses the torsional deformation of prismatic bars of circular cross-section and torsional response of prismatic bars of noncircular cross-section. It analyzes the elastic deformation, plastic deformation, and the effect of strain rate on plastic deformation. The article describes the theory of anisotropy in plastic torsion and the various components of a torsion testing machine. These include drive system, test section, torque and rotational displacement transducers, and rigid frame.
Book Chapter
High Strain Rate Shear Testing
Available to PurchaseSeries: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003295
EISBN: 978-1-62708-176-4
Abstract
This article reviews the dynamic factors, experimental methods and setup, and result analysis of different types of high strain rate shear tests. These include high strain rate torsion testing, double-notch shear testing and punch loading, drop-weight compression shear testing, thick-walled cylinder testing, and pressure-shear plate impact testing.
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003290
EISBN: 978-1-62708-176-4
Abstract
This article discusses stress relaxation testing on metallic materials, as covered by ASTM E 328. It reviews the two types of stress relaxation tests performed in tension, long-term and accelerated testing. The article illustrates load characteristics and data representation for stress relaxation testing used for the most convenient and common uniaxial tensile test. It concludes with information on compression testing, bend testing, torsion testing, and tests on springs.
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003300
EISBN: 978-1-62708-176-4
Abstract
This article provides a discussion on the generation of an incident wave with the help of the stored-torque torsional Kolsky bar and explosively loaded torsional Kolsky bar. It examines the procedures followed for measuring the waves in these bars. The article compares the compression Kolsky bar with the torsional Kolsky bar. It includes information on the various application areas of torsional Kolsky bar: limitations on strain rate, low- and high-temperature testing, quasi-static and incremental strain-rate testing, and localization and shear-banding experiments.
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003269
EISBN: 978-1-62708-176-4
Abstract
This article reviews the common methods of shear and multiaxial testing for the evaluation of engineering components such as fasteners and mill products. It discusses shear test methods, including through-thickness tests, in-plane shear tests, and double-notched shear test. The article provides information on torsional (rotational shear) tests as well as the basic equipment and setup of torsion testing. Motors, twist and torque transducers, torque sensors, and heating systems as well as the specimen preparation procedure are also discussed.
Book Chapter
Overview of Mechanical Properties and Testing for Design
Available to PurchaseSeries: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003257
EISBN: 978-1-62708-176-4
Abstract
An integral aspect of designing and material selection is the use of mechanical properties derived from various mechanical testing. This article introduces the basic concepts of mechanical design and its relation with the properties derived from various mechanical testings, namely, tensile, compressive, hardness, torsion and bend, shear load, shock, and fatigue and creep testings. It describes the design criteria for combined properties derived from each of the mechanical testing. The article concludes with a discussion on the effect of environment on the mechanical properties.
Book Chapter
Mechanical Testing of Threaded Fasteners and Bolted Joints
Available to PurchaseSeries: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003323
EISBN: 978-1-62708-176-4
Abstract
This article provides an overview of the relationships between torque, angle-of-turn, tension, and friction and explains how they are measured and evaluated. It focuses on the principle, test equipment, procedure, evaluation, and test report of various testing methods, namely, friction coefficient testing, torque tension testing, locknut testing, and angular ductility and rotational capacity tests. The article reviews the basic methods and fundamental principles for mechanical testing of externally and internally threaded fasteners and bolted joints. The test methods for externally threaded fasteners include product hardness, proof load, axial and wedge tension testing of full-sized products, tension testing of machined test specimens, and total extension at fracture testing. Product hardness, proof load, and cone proof-load test are the test methods for internally threaded fasteners. The article concludes with a description of torque-angle signature analysis and the specification of measurement accuracy for torque and clamp force.
Book Chapter
Mechanical Testing for Metalworking Processes
Available to PurchaseSeries: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003258
EISBN: 978-1-62708-176-4
Abstract
An important activity in metalworking facilities is the testing of raw materials for characteristics that ensure the integrity and quality of the products made. This article reviews the common material parameters that can have a direct or indirect influence on workability and product quality. These include strength, ductility, hardness, strain-hardening exponent, strain-rate effects, temperature effects, and hydrostatic pressure effects. The article also reviews the material behavior characteristics typically determined by mechanical testing methods. It discusses various mechanical testing methods, including the tension test, plane-strain tension test, compression test, plane-strain compression test, partial-width indentation test, and torsion test. Aspects of testing particularly relevant to workability and quality control for metalworking processes are also described. Finally, the article details the various factors influencing workability in bulk deformation processes and formability in sheet-metal forming.
Book Chapter
Mechanical Testing
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003241
EISBN: 978-1-62708-199-3
Abstract
This article reviews the various types of mechanical testing methods, including hardness testing; tension testing; compression testing; dynamic fracture testing; fracture toughness testing; fatigue life testing; fatigue crack growth testing; and creep, stress-rupture, and stress-relaxation testing. Shear testing, torsion testing, and formability testing are also discussed. The discussion of tension testing includes information about stress-strain curves and the properties described by them.