Skip Nav Destination
Close Modal
By
Michael Rugg, Gary Gariglio
By
Justin Mortimer, Andrew Bernhard, Carlos Rodriguez, Gregg Warner, Tim Williams
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-3 of 3
Switches
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Fundamentals and General Aspects of Power Supply Design for Induction Heating, Heat Treating, Welding, and Melting
Available to PurchaseSeries: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005836
EISBN: 978-1-62708-167-2
Abstract
This article reviews the performance of power electronics components, namely, power rectifiers, insulated-gate bipolar transistors, metal-oxide semiconductor field-effect transistors, diodes, and silicon-controlled rectifiers. It provides information on induction heating power supplies with multiple heat stations, such as switching units and multiple (zone) outputs. The article describes power supply operational control and power supply protection circuits. It details duty cycle, power factor, and harmonics of power supplies. The article also describes system parameters, software analysis-calculations, human analysis-decisions, multiple system arrangements, and zone control systems for power supply selection. It provides information on the maintenance of induction power supplies, detailing the safety precautions to be taken and the need for routine inspection and servicing.
Book Chapter
Power Supplies for Induction Heat Treating, Brazing, and Soldering
Available to PurchaseSeries: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005838
EISBN: 978-1-62708-167-2
Abstract
This article provides a brief description of load conditions for single-shot heat treating, vertical scanning, and brazing and soldering. It discusses the various power components used in power supplies. These include capacitors, integrated power module, transformers, and various switching devices, namely, silicon-controlled rectifiers, insulated-gate bipolar transistors, and metal-oxide semiconductor field-effect transistors. The article also provides information on frequency-multiplication harmonic-induction power supplies, namely, push-pull and half-bridge inverters and full-bridge inverters. Series resonant and parallel resonant circuits and their tuning calculations associated with output networks are also discussed. The article describes the frequency range of simultaneous dual-frequency induction heating power supply, and discusses the advantages, applications, and technical background of independently controlled frequency and power (IFP) induction heating power supply. It concludes with a description of the developments in control systems for modern induction power supplies.
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004173
EISBN: 978-1-62708-184-9
Abstract
This article focuses on the various types of corrosion-related failure mechanisms and their effects on passive electrical components. The types include halide-induced corrosion, organic-acid-induced corrosion, electrochemical metal migration, silver tarnish, fretting, and metal whiskers. The passive electrical components include resistors, capacitors, wound components, sensors, transducers, relays, switches, connectors, printed circuit boards, and hardware.