Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-2 of 2
Interior coatings
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006006
EISBN: 978-1-62708-172-6
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006037
EISBN: 978-1-62708-172-6
Abstract
Polymeric floor coatings refer to flooring materials composed of multicomponent thermoset resins formulated with various fillers and pigments that are installed in situ, usually over concrete substrates. Polymeric flooring systems, specified for all industrial and commercial environments, use a variety of polymer chemistries and are constructed in a variety of methods and designs. This article provides a description of the service conditions for the polymeric flooring systems. It provides information on polymeric flooring systems, including thin-film coatings, self-leveling systems, membrane systems, broadcast systems, troweled systems, and terrazzo. The article also focuses on properties, applications, testing, and factors and requirements to be considered during the installation of polymeric floor coatings. It concludes with a discussion about coating failures, including bonding, cracking, chemical attack, and moisture that affect the polymeric floor coatings on concrete.