Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-2 of 2
Iron-cobalt alloys
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003153
EISBN: 978-1-62708-199-3
Abstract
This article discusses the ferromagnetic properties of soft magnetic materials, explaining the effects of impurities, alloying elements, heat treatment, grain size, and grain orientation on soft magnetic materials. It describes the types of soft magnetic materials, which include high-purity iron, low-carbon irons, silicon (electrical) steels, nickel-iron alloys, iron-cobalt alloys, ferritic stainless steels, amorphous metals, and ferrites (ceramics). Finally, the article provides a short note on alloys for magnetic temperature compensation.
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001099
EISBN: 978-1-62708-162-7
Abstract
Low-expansion alloys are characterized by their dimensional stability, suiting them for applications such as geodetic tape, bimetal strip, glass-to-metal seals, and electronic components. This article describes the composition of such alloys along with related properties and behaviors. It explains how humidity and other factors, such as heat treating and cold drawing, influence thermal expansion rates. It also provides machining information on some of the more common low-expansion alloys, and reviews special alloy types including iron-cobalt-chromium alloys, hardenable alloys, and high-strength controlled-expansion alloys.