Update search
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-1 of 1
Robert C. Tucker
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001282
EISBN: 978-1-62708-170-2
Abstract
This article introduces thermal spray coatings and describes the various types of coating processes and coating devices, including the flame spray, electric-arc spray, plasma spray, transferred plasma arc, high-velocity oxyfuel, and detonation gun. It provides information on the surface preparation methods and finishing treatments of coated parts. The article also explains the tests to evaluate the coating quality and the effects of coating structures and mechanical properties on coated parts. It concludes with a discussion on the uses of thermal spray coatings.