Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-1 of 1
Neil Hopkinson
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006546
EISBN: 978-1-62708-290-7
Abstract
This article focuses on four industrial additive manufacturing approaches that are used to create polymer parts. The first section focuses on material extrusion, providing information on lumped-parameter material flow models and higher-fidelity models developed to estimate temperature distribution. The second section covers polymer powder-bed sintering/ fusion, discussing the different levels of scale used to address modeling and the impact of process settings: thermodynamics at the powder-bed surface, consolidation of adjacent particles in the fusion process, and fusion and molecular-level behavior within particles. The third section on vat photopolymerization (VPP) discusses two primary approaches to modeling VPP processes, namely a lumped-parameter approach to estimate cured regions in the vat, known as the Jacobs model, and a high-fidelity, continuum approach that uses finite-element methods. The final section is devoted to material jetting, focusing on simulations used to study droplet generation at the nozzle and droplet impact.