Update search
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-3 of 3
Geoffrey Sigworth
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006524
EISBN: 978-1-62708-207-5
Abstract
Aluminum casting alloys are among the most versatile of all common foundry alloys and generally have high castability ratings. This article provides an overview of the common methods of aluminum shape casting. It discusses the designations of aluminum casting alloys categorized by the Aluminum Association designation system. The article summarizes the basic composition groupings of aluminum casting alloy and discusses the effects of specific alloying elements and impurities. The characteristics of the important casting processes are summarized and compared in a table. The article presents the advantages and disadvantages of green sand casting, permanent mold casting, semipermanent mold casting, and high-pressure die casting. A discussion on other casting processes, such as investment casting, lost foam, plaster mold casting, pressure casting, centrifugal casting, and semisolid casting, is also included.
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006496
EISBN: 978-1-62708-207-5
Abstract
Castability is a complex characteristic that depends on both the intrinsic fluid properties of the molten metal and the manner in which the particular alloy solidifies. This article discusses the practical aspects of solidification important to aluminum foundrymen. The primary focus is on the chemical segregation that occurs during freezing, because it determines the castability of the alloy. The article describes the two types of segregation, namely, microsegregation and macrosegregation. It discusses the effect of freezing range on castability of an alloy. The article lists the freezing range of a number of important alloys. It concludes with a discussion on castability of 2xx, 3xx, 4xx, 5xx, and 7xx alloys.
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006535
EISBN: 978-1-62708-207-5
Abstract
There are a wide variety of furnace types and designs for melting aluminum. This article discusses the various types of furnaces, including gas reverberatory furnaces, crucible furnaces, and induction melting furnaces. It describes the classification of solid fluxes: cover fluxes, drossing fluxes, cleaning fluxes, and furnace wall cleaner fluxes. The article reviews the basic considerations in proper flux selection and fluxing practices. It explains the basic principles of degassing and discusses the degassing of wrought aluminum alloys. The article describes filtration in wrought aluminum production and in shape casting. It also reviews grain refinement in aluminum-silicon casting alloys, aluminum-silicon-copper casting alloys, aluminum-copper casting alloys, aluminum-zinc-magnesium casting alloys, and aluminum-magnesium casting alloys. The article concludes with a discussion on aluminum-silicon modification.