Update search
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
Filter
- Title
- Authors
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-1 of 1
Colin McCullough
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book: Composites
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003359
EISBN: 978-1-62708-195-5
Abstract
For the reinforcement of metal-matrix composites, four general classes of materials are commercially available: oxide fibers based primarily on alumina and alumina silica systems, nonoxide systems based on silicon carbide, boron fibers, and carbon fibers. This article discusses the key aspects of the aluminum oxide fibers, silicon carbide fibers, boron fibers, and carbon fibers. The commercial fibers for reinforcement of metal-matrix composites are presented in a table. A tabulation of coating schemes for silicon carbide monofilament fibers is also provided.