Systems Failure Analysis
Chapter 14: Contaminants
-
Published:2009
Abstract
Contaminants can be a cause of numerous types of system failures. There are numerous techniques for confirming contaminant presence. When the presence of a contaminant is suspected, the failure analysis team must find and eliminate the contaminant source, which can be obvious or quite subtle. This chapter summarizes a few commonly encountered contaminant sources to stimulate the reader's thinking about potential contaminant sources. A case study of titanium component washing at Litton Lasers is presented to illustrate how the presence of contaminants leads to a system failure.
Sign in
ASM members
Member Sign InContaminants, Systems Failure Analysis, By Joseph Berk, ASM International, 2009, p 141–145, https://doi.org/10.31399/asm.tb.sfa.t52780141
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.