Abstract
Leaks can occur as the result of several failure causes. This chapter reviews the causes, features, and impact of various types of leaks, namely gasket leaks, O-ring leaks, bond-joint leaks, weld leaks, polyvinyl chloride leaks, valve leaks, and structural leaks.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Leaks, Systems Failure Analysis, By Joseph Berk, ASM International, 2009, p 131–139, https://doi.org/10.31399/asm.tb.sfa.t52780131
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Failure Analysis: Why and for Whom?
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure Analysis and After
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure Analysis Terms and Definitions
Microelectronics Failure Analysis: Desk Reference (Seventh Edition)
The Failure Analysis Process: An Overview
Failure Analysis and Prevention
Failure Analysis Methodology
Failure Analysis of Engineering Structures Methodology and Case Histories
Techniques of Failure Analysis
Understanding How Components Fail (Third Edition)
Component Failure Causes and Suggested Analysis Methods
Systems Failure Analysis
Glossary of Terms—Failure Analysis and Prevention
Failure Analysis and Prevention (2021 Edition)
Explosive Sabotage
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure Analysis of Powder Metal Steel Components
Failure Analysis of Heat Treated Steel Components